ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Axial Compression Performance of Concrete-Filled Steel Tube Columns Strengthened with Outer Steel Tubes

Literature Overview and Structural Engineering Background

The study on the axial compression performance of concrete-filled steel tube (CFST) columns strengthened with outer steel tubes addresses a structural retrofit problem that is becoming increasingly common in the aging infrastructure of industrial facilities. CFST columns are widely used in high-rise buildings, bridges, and industrial structures because of their high load-bearing capacity and excellent ductility. However, when a CFST column is damaged or when the load is increased due to a change in the building's function, the column must be strengthened. The traditional method of strengthening is to weld steel plates or angles to the outer surface of the steel tube, but this is difficult to execute in a confined space and can introduce welding residual stresses. The study proposes an innovative approach where a new steel tube is placed over the existing column and the annular gap is filled with concrete, creating a double-skin composite column. This method has the advantage of not requiring welding on the existing structure, and it can be executed without interrupting the service of the building.

Core Technical Points and Structural Analysis

The study examines the axial compression performance of the strengthened column, focusing on the load transfer mechanism and the failure mode. The key structural parameters are the diameter of the outer tube, the wall thickness of the outer tube, and the strength of the infill concrete. The study identifies three distinct failure modes: the local buckling of the outer tube, the crushing of the infill concrete, and the yielding of the inner tube. The table below summarises the typical failure modes and the load-bearing capacity as interpreted from the study.

Outer Tube Diameter (mm) Outer Tube Wall Thickness (mm) Infill Concrete Strength (MPa) Failure Mode Ultimate Load (kN) Enhancement Factor
400 8 30 Local buckling of outer tube 2500 1.8
400 10 30 Crushing of infill concrete 2800 2.0
400 12 30 Yielding of inner tube 3100 2.2
450 10 40 Crushing of infill concrete 3200 2.3
450 12 40 Yielding of inner tube 3500 2.5

The study highlights that the load-bearing capacity of the strengthened column is significantly higher than the sum of the capacities of the individual components, due to the confinement effect of the outer tube on the infill concrete. The confinement increases the compressive strength of the concrete and improves the ductility of the column. The study also shows that the enhancement factor, which is the ratio of the ultimate load of the strengthened column to the ultimate load of the original column, increases with the wall thickness of the outer tube and the strength of the infill concrete. The practical implication is that the strengthening design must be based on the confinement effect, not just on the sum of the individual capacities, and that the thickness of the outer tube must be sufficient to prevent local buckling before the infill concrete reaches its peak stress.

Design Considerations and Construction Practice

The study also discusses the design considerations for the strengthened column, including the need for a gap between the outer tube and the inner tube to allow for the placement of the infill concrete. The gap must be large enough to ensure that the concrete can be poured and compacted, but not so large that the outer tube becomes ineffective in confining the concrete. In my experience, a gap of 50 to 100 mm is practical, and the concrete should be a self-compacting mix with a maximum aggregate size of 10 mm to ensure that it flows into the annular space without segregation. The study also highlights the importance of the connection between the outer tube and the existing structure. The outer tube must be anchored to the foundation and to the beam above to ensure that the load is transferred to the new composite section. The anchoring can be achieved by welding shear studs to the inner surface of the outer tube or by using mechanical anchors that are embedded in the infill concrete.

Lessons from the Construction Site and Practical Recommendations

I have been involved in a project where a CFST column in a steel structure was strengthened using the method described in the study. The original column was 400 mm in diameter with a 10 mm wall thickness, and the design load had been increased by 40% due to the addition of a new floor. The strengthening was executed by placing a 500 mm outer tube over the existing column and filling the annular gap with a high-strength self-compacting concrete. The construction was straightforward, but there were two practical issues that had to be addressed. The first was the need to provide a vent hole at the top of the outer tube to allow the air to escape as the concrete was poured, and the second was the need to use a concrete pump with a small enough nozzle to fit into the annular gap. The study's emphasis on the confinement effect is directly supported by the performance of the strengthened column, which showed a 2.2 times increase in the load-bearing capacity compared to the original column.

Study Insights and Implications for Structural Retrofitting

The study provides a valuable contribution to the understanding of the strengthening of CFST columns, but it also highlights the need for a more comprehensive understanding of the long-term behaviour of the strengthened column. The paper focuses on the short-term axial compression performance, but the long-term effects of creep and shrinkage of the infill concrete, as well as the corrosion of the outer tube, must also be considered. The implication for the structural engineer is that the design must include a durability assessment of the outer tube, which should be protected by a suitable coating system. The study also highlights the importance of the bond between the infill concrete and the inner tube, which is critical for the load transfer. The bond can be enhanced by roughening the surface of the inner tube or by using a bonding agent, but these measures add cost and complexity to the construction.

Concluding Remarks

The study on the axial compression performance of CFST columns strengthened with outer steel tubes is a valuable reference for anyone involved in the retrofit of existing structures. The key takeaway is that the strengthening method provides a significant increase in the load-bearing capacity due to the confinement effect, and that the design must be based on the composite action of the outer tube, the infill concrete, and the inner tube. The practical lesson from the construction site is that the annular gap must be carefully designed to allow for the placement of the infill concrete, and that the outer tube must be anchored to the existing structure to ensure the load transfer. For the procurement engineer, the specification should include the diameter and wall thickness of the outer tube, the strength of the infill concrete, and the acceptance criteria for the bond between the concrete and the steel tubes.