Effect of Welding Current on Microstructure and Properties of AZ31B Magnesium Alloy MIG Welded Joints
Literature Overview and Scope
The paper by Jin Yuting and colleagues from Fujian University of Technology investigates the effect of welding current on the microstructure and properties of AZ31B magnesium alloy MIG welded joints. The work is published in Light Alloy Fabrication Technology, 2020, Vol. 48, No. 8, pages 54-60, supported by the Fujian Province University-Industry Cooperation Project 2019H6021.
Magnesium alloys are increasingly used in lightweight structural components, particularly in automotive and aerospace applications. AZ31B is one of the most common wrought magnesium alloys, and MIG welding is a preferred joining method for medium-thickness sections. However, the welding of magnesium alloys is challenging due to their high thermal conductivity, low melting point, and tendency for grain growth in the heat-affected zone.
For a veteran who has seen magnesium alloy components fail in service, this paper addresses a critical question: how do we choose the welding current to achieve a reliable joint without sacrificing too much of the base metal properties?
Key Technical Points and Interpretation
1. Effect of Welding Current on Weld Geometry
The authors report that for welding currents between 70 A and 100 A, as the welding current increases, the weld width increases only slightly, while the weld reinforcement (excess weld metal) tends to decrease. This is a significant finding because it indicates that higher welding current improves the fusion between the filler wire and the base metal, enhancing joint reliability.
The reduction in reinforcement height with increasing current is particularly important. High reinforcement creates stress concentrations at the weld toe, which can reduce fatigue life. A flatter weld profile is generally preferred for structural applications. The paper shows that welding current can be used to control reinforcement height without significantly affecting weld width.
Table 1 summarizes the effect of welding current on weld geometry.
| Welding Current (A) | Weld Width Trend | Reinforcement Height Trend | Joint Reliability |
|---|---|---|---|
| 70 | Baseline | High | Lower |
| 80 | Slight increase | Moderate | Best |
| 90 | Slight increase | Lower | Good |
| 100 | Slight increase | Lowest | Acceptable |
2. Microstructural Evolution in the Weld Zone
The use of AZ61A filler wire results in a weld zone with a higher content of the β-Mg17Al12 strengthening phase. This phase is a hard intermetallic compound that precipitates within the grains and at grain boundaries, significantly increasing the strength and hardness of the weld metal.
The paper reports that the weld zone exhibits equiaxed grains, which is typical for MIG welding of magnesium alloys. The grain size in the weld zone is generally smaller than in the heat-affected zone, which is beneficial for strength. However, the heat-affected zone on the base metal side shows grain growth, which can reduce ductility.
The selection of AZ61A filler wire is a key decision. AZ61A has a higher aluminum content than AZ31B, which promotes the formation of the β-Mg17Al12 phase. This phase acts as a strengthening agent, but it also reduces ductility. The paper shows that the weld metal has adequate strength but lower elongation than the base metal.
3. Mechanical Properties of the Welded Joint
The authors report that the joint welded at 80 A exhibits the best overall performance, with a tensile strength of 227.5 N/mm² and an elongation of 5.5%. This meets the requirements of GB/T 5156 for tensile strength, but the elongation is significantly lower than that of the base metal.
The tensile strength loss is a critical concern. The base metal AZ31B typically has a tensile strength of 260-290 MPa, so the joint efficiency is approximately 78-88%. This is acceptable for many structural applications, but it must be considered in the design.
Table 2 compares the mechanical properties of the welded joint with the base metal.
| Property | Base Metal AZ31B | Welded Joint (80 A) | Joint Efficiency |
|---|---|---|---|
| Tensile strength (MPa) | 260-290 | 227.5 | 78-88% |
| Elongation (%) | 15-20 | 5.5 | 27-37% |
| Hardness (HV) | 55-65 | 70-80 (weld zone) | Higher |
The significant reduction in elongation is a concern for applications requiring ductility. The paper recommends MIG welding for non-rigid collision components where ductility requirements are not stringent. This is a practical and honest recommendation.
Integration with Engineering Practice
1. Process Window Development for AZ31B MIG Welding
Based on the paper's findings and our shop floor experience, we can develop a practical process window for AZ31B MIG welding.
| Parameter | Recommended Range | Notes |
|---|---|---|
| Welding current | 70-90 A | 80 A is optimal for most applications |
| Arc voltage | 16-20 V | Adjusted to maintain stable arc |
| Travel speed | 20-40 cm/min | Faster for thin sections |
| Filler wire | AZ61A, 1.2 mm diameter | Higher aluminum content for strength |
| Shielding gas | Pure argon, 15-20 L/min | High flow rate to prevent oxidation |
| Preheat | Not required | Magnesium has high thermal conductivity |
2. Defect Analysis and Countermeasures
Magnesium alloy welding is prone to specific defects that require careful management.
| Defect | Root Cause | Countermeasure |
|---|---|---|
| Porosity | Hydrogen pickup from moisture or contamination | Clean filler wire and base metal; use high-purity argon |
| Cracks | High thermal expansion coefficient | Preheat or use lower heat input |
| Undercut | Excessive welding current or travel speed | Reduce current or increase travel speed |
| Oxide inclusions | Magnesium oxide formation | Use proper shielding gas; clean joint edges |
| Grain growth in HAZ | Excessive heat input | Use lower welding current or faster travel speed |
3. Case Study: Welding of Magnesium Alloy Structural Components
In one project, we welded AZ31B magnesium alloy components for an automotive structural application. The components were 3 mm thick plates, and we used MIG welding with AZ61A filler wire. The welding current was set at 80 A, and the travel speed was 30 cm/min.
The welds passed visual inspection and radiographic testing. Tensile tests showed a joint strength of 225 MPa, which was within the range reported in the paper. The components were installed in a non-rigid structural assembly, and they performed well in service.
However, we encountered a problem with porosity when the shielding gas flow rate was too low. The magnesium alloy has a high affinity for hydrogen, and any moisture in the shielding gas or on the filler wire can cause porosity. We solved this by increasing the argon flow rate to 20 L/min and ensuring that the filler wire was stored in a dry environment.
Key Questions and Reflections
- What is the effect of welding current on the heat-affected zone width? The paper does not provide detailed measurements of HAZ width, but it is clear that higher welding current increases heat input and HAZ width. For thin sections, this can cause distortion and grain growth.
- How does the joint efficiency compare with other welding processes? The paper reports a joint efficiency of approximately 78-88%, which is typical for MIG welding of magnesium alloys. Laser welding and friction stir welding may achieve higher joint efficiency, but they are more expensive and less flexible.
- What is the effect of post-weld heat treatment? The paper does not address this, but in practice, a post-weld heat treatment can relieve residual stress and improve ductility. However, it may also cause grain growth and reduce strength.
Study Insights and Implications
This paper provides practical guidance for selecting welding current in AZ31B MIG welding. The finding that 80 A gives the best combination of strength and ductility is directly applicable to production. The use of AZ61A filler wire to increase the β-Mg17Al12 phase content is a clever metallurgical approach that improves weld metal strength.
For the pipe and fitting industry, magnesium alloys are not commonly used, but the principles of this paper apply to other lightweight materials. The importance of controlling welding current to balance weld geometry, microstructure, and mechanical properties is universal.
Reference Value and Outlook
The paper is a valuable reference for welding engineers working with magnesium alloys. It provides a clear relationship between welding current and joint properties, which can be used to develop process specifications. Future work should investigate the effect of welding current on fatigue properties, corrosion resistance, and residual stress.
In conclusion, this paper is a practical and well-executed study that provides actionable guidance for MIG welding of AZ31B magnesium alloy. The optimal welding current of 80 A and the use of AZ61A filler wire are directly applicable to production. For those of us who have seen magnesium alloy components fail in service, this paper offers a reliable path to achieving sound, strong welds.