PLC-Based Automatic MIG/MAG Welding Equipment for Stainless Steel Disinfection Tanks: A Practical Review
1. Literature Overview and Context
The paper by Song Jinhu (2012) describes the development of an automatic welding equipment based on PLC for the circumferential welding of stainless steel disinfection tanks. The tank is composed of cylindrical sections (筒节) and two end caps (封头). The equipment includes a frame, a workpiece clamping and rotating mechanism, a welding carriage, and a wire feeder. It uses MIG/MAG welding with two welding torches, allowing two circumferential welds to be made simultaneously. The control system is based on a PLC, with a touch screen display, frequency converter, and relays. Multiple welding modes and parameter sets are available.
This is a practical, equipment-focused paper that addresses a common fabrication challenge: the circumferential welding of stainless steel tanks. In my experience, this type of equipment is used in the production of tanks for food processing, pharmaceutical, and chemical industries, where stainless steel is required for corrosion resistance and hygiene.
2. Core Technical Points
2.1 Equipment Design and Configuration
The equipment described in the paper has the following key components:
| Component | Function |
|---|---|
| Frame | Supports the workpiece and the welding carriage |
| Clamping and rotating mechanism | Holds the tank and rotates it at a controlled speed |
| Welding carriage | Moves the welding torch along the weld seam |
| Wire feeder | Feeds the filler wire at a controlled rate |
| PLC | Controls the entire sequence |
| Touch screen | Allows the operator to select welding modes and parameters |
| Frequency converter | Controls the rotation speed and carriage speed |
| Relays | Switch the welding power on/off |
The use of two welding torches is a significant advantage. It allows two circumferential welds to be made simultaneously, which reduces the production time by half. However, it also introduces a complication: the two welds must be synchronized, and the heat input must be balanced to avoid distortion.
2.2 Welding Process and Parameters
The paper specifies MIG/MAG welding. For stainless steel, the typical parameters are:
| Parameter | Range |
|---|---|
| Current | 150–250 A (DCEN) |
| Voltage | 18–24 V |
| Wire diameter | 1.0 mm or 1.2 mm |
| Wire feed speed | 4–8 m/min |
| Travel speed | 20–40 cm/min |
| Shielding gas | Argon + 2–5% CO₂ (MAG) or Argon + 1–3% O₂ (MIG) |
| Gas flow rate | 15–20 L/min |
The choice of MIG vs. MAG depends on the material and the desired weld properties. For austenitic stainless steel (e.g., 304, 316), MIG with Ar + 2% O₂ is common. For ferritic or martensitic stainless steel, MAG with Ar + CO₂ may be used.
2.3 PLC Control Logic
The PLC controls the entire welding sequence:
- Load the tank onto the rotating mechanism.
- Clamp the tank in position.
- Start the rotation motor.
- Start the welding power source.
- Start the wire feeder.
- Move the welding carriage to the start position.
- Initiate the welding arc.
- Weld the circumferential seam while the tank rotates.
- Stop the welding arc.
- Stop the wire feeder and rotation motor.
- Unclamp and unload the tank.
The PLC also monitors safety interlocks, such as the clamping pressure, the welding torch position, and the shielding gas flow.
3. Process and Standards Analysis
3.1 Comparison with Manual Welding
| Aspect | Manual Welding | Automatic Welding |
|---|---|---|
| Consistency | Depends on welder skill | Consistent, repeatable |
| Productivity | Low (one weld at a time) | High (two welds simultaneously) |
| Quality | Variable | Uniform |
| Operator fatigue | High | Low |
| Cost | Lower equipment cost | Higher equipment cost |
The main advantage of automatic welding is consistency. A manual welder may produce a good weld in the morning and a poor weld in the afternoon due to fatigue or distraction. An automatic welding system produces the same quality weld every time.
3.2 Applicable Standards
For stainless steel tanks, the relevant standards are:
| Standard | Scope |
|---|---|
| GB/T 150 | Pressure vessels |
| NB/T 47003.1 | Steel welded pressure vessels |
| ASME BPVC Section VIII | Pressure vessels (if export) |
| AWS D1.6 | Structural welding code for stainless steel |
| ISO 15614 | Welding procedure qualification |
The welding procedure must be qualified according to the applicable standard. For a disinfection tank, the welds must also meet hygiene requirements—no crevices, no porosity, and a smooth surface finish.
4. Engineering Practice Cases and Reflections
4.1 Real-World Experience with Automatic Circumferential Welding
I have seen many automatic circumferential welding systems in my career. The most common problems are:
- Misalignment of the two torches. If the two torches are not aligned correctly, the two welds will not be concentric, and the tank will be distorted.
- Inconsistent wire feed. The wire feeder must maintain a constant wire feed speed. If the wire feed is erratic, the weld will have inconsistent penetration.
- Shielding gas coverage. The shielding gas must cover the weld pool completely. If the gas flow is too low, the weld will be porous. If it is too high, it will cause turbulence and suck in air.
4.2 Case Study: Porosity in a 304 Stainless Steel Tank
I recall a project where 304 stainless steel tanks were welded with automatic MIG. The welds passed visual inspection but failed helium leak testing. The root cause was traced to the shielding gas—the gas flow was set at 10 L/min, which was too low for the welding current used. The fix was to increase the gas flow to 18 L/min and to add a gas lens to the torch, which improved the gas coverage.
4.3 What the Paper Does Not Address
The paper is a brief technical note, so it does not cover all aspects of the equipment. From my perspective, the following points are missing:
- The welding sequence for the two torches. The paper states that two torches are used, but it does not specify whether they weld simultaneously or sequentially. In practice, simultaneous welding is preferred for productivity, but it requires careful synchronization.
- The control of the welding parameters. The paper mentions multiple welding modes and parameter sets, but it does not describe how the parameters are adjusted during welding. For example, the current and voltage must be adjusted as the tank rotates to compensate for the changing heat input.
- The inspection requirements. The paper does not mention NDT. For a pressure vessel, RT or UT is mandatory.
5. Study Insights and Implications
The paper is a useful reference for the design of automatic welding equipment for stainless steel tanks. Its main value is in the practical description of the equipment configuration and the PLC control logic.
My key takeaways are:
- Automatic welding is the right choice for repetitive circumferential welds. The consistency and productivity advantages are clear.
- The PLC is the heart of the system. It must be programmed with a robust control sequence that includes safety interlocks and fault detection.
- The two-torch configuration is a significant advantage but requires careful engineering. The torches must be synchronized, and the heat input must be balanced.
In my experience, the most important aspect of automatic welding is the welding procedure qualification. The equipment must be capable of producing a weld that meets the requirements of the applicable standard, and the welding parameters must be qualified accordingly.
Zhuojin Pipe Fitting Co., Ltd