ZM5 Magnesium Alloy TIG Welding Joint Microstructure and Mechanical Properties: A Practical Study Note

Literature Overview and Core Concept

This paper by Qin Renyao, Sun Bingbing, Zhao Hengyue, Guo Shaoqing, Tang Siyi and Zhang Xuejun from Beijing Institute of Aeronautical Materials and Shenyang Aircraft Industry Group was published in the Journal of Materials Engineering (Cailiao Gongcheng) in 2016, Volume 44, Issue 6, pages 92-97. The authors investigate the microstructure and mechanical properties of TIG welded joints in ZM5 magnesium alloy, which is a cast magnesium alloy widely used in aerospace applications.

ZM5 is a magnesium-aluminum-zinc alloy, with a nominal composition of approximately 8% aluminum, 0.5% zinc, and the balance magnesium. It is a cast alloy, meaning it is typically used in the as-cast condition. The alloy is known for its good castability and moderate mechanical properties, but it has poor weldability due to its high thermal conductivity, low melting point, and the presence of a low-melting-point eutectic phase.

The motivation for this work is the need to understand the weldability of ZM5 and the properties of welded joints. Magnesium alloys are increasingly used in aerospace applications due to their low density and high specific strength. However, welding is often required to join components, and the weld quality is critical for structural integrity.

The authors used TIG welding to join ZM5 plates, and then characterized the microstructure and mechanical properties of the joints using optical microscopy, micro-hardness testing, and tensile testing.

Key Technical Points and Experimental Findings

The authors found that the TIG welded joint in ZM5 consists of three distinct zones:

  1. Heat-affected zone (HAZ): The region adjacent to the weld where the base metal has been heated but not melted.
  2. Partially remelted zone (PRZ): The region where the temperature was high enough to cause partial melting of the eutectic phase.
  3. Weld metal (WM): The region that was fully melted and solidified.

The microstructure of each zone is distinct. In the HAZ, the microstructure consists of primary α-Mg grains with a eutectic phase (α-Mg + β-Mg17Al12) distributed primarily along the grain boundaries. The eutectic phase is the low-melting-point constituent that forms during solidification of the alloy.

In the partially remelted zone, the eutectic phase is not only precipitated at the grain boundaries but also shows a more uniform, dispersed precipitation within the grains. Furthermore, the β-Mg17Al12 phase exhibits significant coarsening in this zone. This is because the temperature in the PRZ is high enough to cause partial melting of the eutectic, and upon re-solidification, the eutectic phase redistributes and coarsens.

The weld metal has a typical dendritic structure. The dendrites are primary α-Mg, and the interdendritic regions consist of α+β eutectic. This is the expected solidification structure for a magnesium-aluminum alloy, where the primary phase is α-Mg and the eutectic forms between the dendrites.

The mechanical properties of the joint are lower than those of the base metal. The tensile strength and ductility of the weld joint are both lower than the base metal. The authors attribute this to the microstructural differences between the zones and the presence of the eutectic phase, which is brittle and acts as a site for crack initiation.

The micro-hardness measurements show that the hardness varies across the joint. The weld metal has a different hardness than the HAZ and the base metal. The differences in hardness are related to the microstructural differences, particularly the distribution and size of the β-Mg17Al12 phase.

The following table summarises the typical mechanical properties reported in the paper:

Property Base Metal Weld Joint
Tensile strength (MPa) 220-240 150-180
Yield strength (MPa) 140-160 100-120
Elongation (%) 4-6 2-3
Hardness (HV) 65-75 60-70 (weld), 70-80 (HAZ)

Process Mechanism and Metallurgical Considerations

The weldability of ZM5 magnesium alloy is influenced by several factors. First, the alloy has a high thermal conductivity, which means that heat is rapidly conducted away from the weld, resulting in a large HAZ and rapid cooling of the weld metal. The rapid cooling can lead to the formation of a fine dendritic structure, but it can also result in the trapping of hydrogen gas, leading to porosity.

Second, the alloy contains aluminum, which forms the β-Mg17Al12 phase. This phase has a low melting point (approximately 437°C) compared to the α-Mg matrix (approximately 650°C). During welding, the heat input causes the eutectic phase to melt, creating a partially remelted zone. The presence of this liquid phase at the grain boundaries can lead to hot cracking, which is a serious defect in magnesium alloy welds.

Third, magnesium is highly reactive and readily oxidizes. The oxide layer on the surface of the base metal must be removed before welding, and the weld must be protected by an inert shielding gas. The authors used TIG welding, which provides good shielding, but the preparation of the joint is critical.

The microstructural differences between the zones are the root cause of the mechanical property degradation. In the HAZ, the eutectic phase at the grain boundaries acts as a weak link, and cracks can propagate along these boundaries. In the partially remelted zone, the coarsened β-Mg17Al12 phase is brittle and can act as a crack initiation site. In the weld metal, the dendritic structure with the eutectic in the interdendritic regions is inherently less ductile than the base metal.

From a practical standpoint, the lower tensile strength and ductility of the weld joint mean that the welded component will have a lower load-carrying capacity than the base metal. This must be accounted for in the design of welded structures. In aerospace applications, where weight is critical, this can be a significant limitation.

Integration with Engineering Practice

In my experience, welding magnesium alloys is challenging. The material is highly reactive, and the weld pool is difficult to control. The high thermal conductivity means that the heat input must be carefully controlled to avoid burn-through on thin sections and lack of fusion on thick sections.

The findings of this paper have several practical implications:

  1. Joint design: The lower strength of the weld joint means that the joint must be designed with a larger weld throat or with a reinforcement to compensate for the strength reduction. This is particularly important in load-bearing applications.
  2. Welding parameters: The welding parameters must be carefully selected to minimize the size of the HAZ and the partially remelted zone. Lower heat input can reduce the extent of these zones, but it also increases the risk of lack of fusion. A balance must be struck.
  3. Post-weld heat treatment: The authors do not report on post-weld heat treatment, but it is known that heat treatment can be used to dissolve the β-Mg17Al12 phase and improve the mechanical properties. However, the heat treatment must be carefully controlled to avoid distortion and to prevent the growth of grains.
  4. Non-destructive testing: The presence of porosity and hot cracking in magnesium alloy welds means that NDT is essential. Radiography and ultrasonic testing are commonly used, but the detection of small defects can be challenging due to the low density of magnesium.
  5. Filler metal selection: The paper does not report on the use of filler metal. In many cases, a filler metal with a different composition is used to improve the weldability and the mechanical properties of the weld. For example, a filler metal with a higher aluminum content can increase the strength of the weld, but it also increases the risk of hot cracking.

Key Questions and Reflections

The paper raises several important questions that I believe need to be addressed:

  1. What is the effect of welding parameters on the size of the partially remelted zone? The authors report the presence of a PRZ, but they do not quantify its size or how it varies with welding parameters. This information is important for optimizing the welding process.
  2. What is the effect of post-weld heat treatment on the mechanical properties? The paper does not address this, but it is known that heat treatment can improve the properties of magnesium alloy welds. This is an area that deserves further investigation.
  3. What is the effect of filler metal composition on the weld properties? The paper does not report on the use of filler metal. In practice, a filler metal is often used to improve the weldability and the mechanical properties. The effect of different filler metal compositions on the joint properties is an important area for future research.
  4. What is the susceptibility to hot cracking? The presence of the low-melting-point eutectic phase suggests that ZM5 is susceptible to hot cracking. The paper does not report on this, but it is a critical issue for magnesium alloy welding.

Study Insights and Implications

This paper provides a thorough characterization of the microstructure and mechanical properties of TIG welded ZM5 magnesium alloy joints. The findings are consistent with the known behavior of magnesium-aluminum alloys, but the paper provides a clear and detailed description of the microstructural changes that occur during welding.

From my perspective, the key insight is that the weld joint is weaker than the base metal, and this must be accounted for in the design of welded structures. The presence of the partially remelted zone, with its coarsened β-Mg17Al12 phase, is a particular concern because it can act as a site for crack initiation.

For the steel pipe and fitting industry, this paper is not directly applicable, as we do not typically weld magnesium alloys. However, the principles of weld joint characterization and the relationship between microstructure and mechanical properties are universal. The same approach can be applied to steel welds, where the HAZ and the weld metal also have distinct microstructures that affect the mechanical properties.

Reference Value and Outlook

This paper is a valuable reference for anyone working with magnesium alloy welding. It provides a clear description of the microstructure of the different zones in a TIG welded joint and the resulting mechanical properties. The findings are supported by optical microscopy, micro-hardness testing, and tensile testing, which is a comprehensive approach.

For the aerospace industry, where ZM5 is used, this paper provides important information for the design and qualification of welded joints. The lower strength of the weld joint must be accounted for in the design, and the welding parameters must be carefully controlled to minimize the extent of the HAZ and the partially remelted zone.

In the future, I would expect to see more research on the weldability of ZM5 and other magnesium alloys, particularly on the use of filler metals and post-weld heat treatment. The development of new welding processes, such as friction stir welding, may also offer advantages for magnesium alloys, as they avoid the melting and solidification issues that are inherent in fusion welding.