Dual TIG Arc Additive Manufacturing of Steel Stainless Steel Gradient

Core idea from the paper

The 2025 paper on dual TIG arc additive manufacturing of low carbon steel to stainless steel gradient material is directly relevant to bimetal pipe, valve bodies, and corrosion resistant overlays. The authors show that composition can be made to change almost linearly along height, and microstructure changes from martensite and ferrite at the bottom to martensite, then martensite and austenite, then ferrite and austenite at the top. That is exactly what happens when two dissimilar alloys are melted together in a controlled way. The question for a factory is not whether it can be done, but whether it can be done repeatably and inspected economically.

Microstructure zones and practical risk

Zone Microstructure Main risk
Bottom Martensite and ferrite Cracking if carbon and dilution are uncontrolled
Middle Martensite Toughness loss and need for post heat
Upper middle Martensite and austenite Local hardness drop and corrosion mismatch
Top Ferrite and austenite Good corrosion but possible sensitization if thermal cycles are wrong

The tensile strengths of 1224 MPa horizontal and 1106 MPa vertical with 11 and 12.5 percent elongation are impressive, but they are not a pressure equipment acceptance criterion. I would ask where the fracture happened, whether the interface had carbon migration, and whether intermetallic or sigma phase formed during long thermal cycles. In pipe fittings, a gradient from carbon steel to stainless can reduce the need for a heavy transition flange, but it also creates a zone where galvanic corrosion, hydrogen induced cracking, or PWHT embrittlement can hide.

How I would qualify and deliver such a part

First, I would define the service envelope: pressure, temperature, corrosion medium, cyclic load, and allowable PWHT. Then I would run a PDCA cycle with coupon geometry that matches wall thickness and cooling rate. FMEA would rank lack of fusion, dilution spikes, intermetallic formation, and residual stress cracking. For NDE, I would use phased array UT for planar defects, hardness traverse, corrosion coupon test, and possibly metallography from witness plates. If the part is for sour service, HIC and SSC testing cannot be skipped just because the top surface looks stainless.

The paper shows promise for functionally graded components, but the industrial value depends on controlling the gradient like a weld procedure, not like a laboratory recipe. If the factory can prove the transition zone, it can save weight, cost, and field welding, but it must sell the result with data that an inspector or owner will trust.