Effect of Filler Material on Microstructure and Properties of Magnesium Alloy TIG Welded Joints

Literature Overview and Background

This paper from the China Academy of Engineering Physics (Ningbo Branch) investigates the effect of filler wire composition on the microstructure and mechanical properties of TIG welded AZ31B magnesium alloy. The authors used two different filler wires, AZ31 and AZ61, to weld 10 mm thick AZ31B plates. The welded joints were analyzed using optical microscopy, scanning electron microscopy, X-ray diffraction, and mechanical testing. The results showed that both filler wires produced joints with good appearance and no obvious defects, but the AZ31 filler wire produced better joint appearance. The AZ61 filler wire produced Al12Mg17 phase at the grain boundaries, while the AZ31 filler wire did not. The hardness distribution differed between the two joints, and the AZ61 filler wire produced joints with 20% higher strength than the AZ31 filler wire.

This paper is highly relevant to the welding of magnesium alloys, which are increasingly used in aerospace, automotive, and electronics applications due to their low density and high specific strength. However, magnesium alloys are notoriously difficult to weld due to their high thermal conductivity, low melting point, and high reactivity with oxygen and nitrogen. The selection of filler wire is one of the most critical decisions in magnesium alloy welding, as it directly affects the microstructure and mechanical properties of the joint.

Microstructural Analysis and Phase Formation

The microstructural analysis revealed a significant difference between the two filler wires. The AZ61 filler wire, which contains 6% aluminum, produced a weld metal with Al12Mg17 phase precipitated at the grain boundaries. The AZ31 filler wire, which contains 3% aluminum, did not produce this phase. This is a critical finding because Al12Mg17 is a brittle intermetallic phase that can reduce the ductility and toughness of the weld metal.

The formation of Al12Mg17 phase can be explained by the phase diagram of the Mg-Al system. The maximum solubility of aluminum in magnesium is approximately 12.7% at the eutectic temperature of 437°C. When the aluminum content exceeds this solubility limit, the Al12Mg17 phase precipitates. In the AZ61 filler wire, the aluminum content is 6%, which is below the maximum solubility but high enough to cause precipitation during the non-equilibrium cooling of the weld. The AZ31 filler wire, with only 3% aluminum, does not reach the precipitation threshold.

The presence of Al12Mg17 at the grain boundaries has two effects. First, it increases the strength of the weld metal through precipitation hardening. This explains why the AZ61 filler wire produced joints with 20% higher strength than the AZ31 filler wire. Second, it reduces the ductility and toughness of the weld metal, as the brittle intermetallic phase can act as a crack initiation site. This trade-off between strength and ductility is a classic dilemma in materials engineering.

Mechanical Properties and Hardness Distribution

The mechanical testing revealed a significant difference in the hardness distribution between the two joints. With the AZ31 filler wire, the highest hardness was found in the base metal, while with the AZ61 filler wire, the highest hardness was found in the weld metal. This is consistent with the microstructural analysis: the AZ61 filler wire produces a weld metal with Al12Mg17 precipitates, which increases the hardness of the weld metal.

The hardness distribution is important because it affects the overall mechanical behavior of the joint. In a welded joint, the hardness profile determines the location of the weakest point, which is where failure is most likely to occur. With the AZ31 filler wire, the weakest point is in the weld metal, while with the AZ61 filler wire, the weakest point is in the heat-affected zone (HAZ). This difference in hardness distribution can have a significant impact on the fatigue performance and fracture behavior of the joint.

The tensile strength results showed that the AZ61 filler wire produced joints with 20% higher strength than the AZ31 filler wire. This is a significant improvement, but it comes at the cost of reduced ductility. The AZ61 filler wire also produced a joint with better appearance, which suggests that the higher aluminum content improves the weldability of the alloy.

Selection Criteria for Filler Wire

Based on this study and my experience, the selection of filler wire for magnesium alloy welding should consider the following factors:

  1. Base metal composition: The filler wire should be compatible with the base metal. For AZ31B base metal, both AZ31 and AZ61 filler wires can be used, but the choice depends on the application requirements.
  2. Strength requirements: If high strength is required, AZ61 filler wire is preferred, as it produces 20% higher strength. However, this comes at the cost of reduced ductility.
  3. Ductility and toughness requirements: If the joint will be subjected to impact loading or cyclic loading, AZ31 filler wire may be preferred, as it produces a more ductile weld metal without brittle intermetallic phases.
  4. Corrosion resistance: The presence of Al12Mg17 phase can affect the corrosion resistance of the weld metal. In corrosive environments, AZ31 filler wire may be preferred, as it produces a more uniform microstructure.
  5. Weldability: The AZ61 filler wire produced better joint appearance, which suggests that it has better weldability. This may be due to the higher aluminum content, which improves the fluidity of the weld pool.

Summary and Study Insights

This paper provides a valuable comparison of two filler wires for TIG welding of AZ31B magnesium alloy. The key technical points are the formation of Al12Mg17 phase with the AZ61 filler wire, the resulting increase in strength and hardness, and the trade-off between strength and ductility. For engineers working with magnesium alloys, this paper provides important guidance on filler wire selection. The lessons I draw from this work are clear: the choice of filler wire is not a simple decision, but one that must consider the specific requirements of the application. If strength is the primary concern, AZ61 filler wire is the better choice. If ductility and toughness are more important, AZ31 filler wire should be used. In practice, I would recommend conducting welding procedure qualification tests with both filler wires and selecting the one that best meets the application requirements. The 20% strength increase provided by the AZ61 filler wire is significant, but it must be weighed against the potential reduction in ductility and the increased risk of brittle fracture in service.