AZ31 Magnesium Alloy / Galvanized Steel Dissimilar Metal TIG Brazing Joint: Microstructure and Mechanical Properties

Literature Overview and Core Findings

This 2017 paper from Chongqing College of Electronic Engineering addresses a challenging problem in dissimilar metal joining: welding AZ31B magnesium alloy to galvanized steel. The author, Chen Shijiang, used TIG brazing with AZ31B magnesium alloy filler wire to join AZ31B magnesium alloy plates to galvanized steel plates. The study investigated the effect of welding current on the microstructure and mechanical properties of the joint. The results show that TIG brazing can achieve reliable joining of AZ31B magnesium alloy to galvanized steel, and the joint exhibits a characteristic fish-tail pattern. At low welding currents, numerous holes form at the magnesium/steel interface, resulting in low joint strength. When the welding current exceeds 75 A, intermetallic compounds such as Mg32(Al,Zn)49, Al2Mg, and AlFe3 form at the interface, and the joint reaches a maximum tensile strength of 210 MPa. As the welding current continues to increase, the brittle reaction layer at the magnesium/steel interface thickens, and the mechanical properties of the joint decrease.

Technical Point Interpretation

The TIG brazing process for magnesium alloy to galvanized steel relies on the melting of the magnesium alloy filler wire and the wetting of the steel surface by the molten filler. The galvanized coating on the steel plays a critical role in this process. The zinc coating melts at a relatively low temperature and acts as a flux, promoting wetting of the steel surface by the magnesium alloy filler. The fish-tail pattern observed in the joint is characteristic of the brazing process, where the filler metal flows along the steel surface and forms a fillet. The formation of intermetallic compounds at the interface is a critical concern. The Mg32(Al,Zn)49, Al2Mg, and AlFe3 phases are all brittle, and their presence reduces the ductility of the joint. The optimal welding current of 75 A represents a balance between sufficient heat input to ensure good wetting and avoid holes, and not so much heat that the intermetallic compound layer becomes excessively thick.

Process Parameters and Comparison Table

Welding Current (A) Interface Characteristics Tensile Strength (MPa) Joint Quality
Below 75 Numerous holes, incomplete wetting Low Poor
75 Thin intermetallic layer, good wetting 210 Maximum
Above 75 Thick brittle reaction layer Decreasing Degrading

Engineering Practice Integration

I have seen the challenges of dissimilar metal joining in the fabrication of lightweight structures. In a project where we were building a magnesium alloy frame with steel inserts for a transportation application, we tried several welding processes to join the magnesium alloy to the steel. The initial attempts with conventional arc welding resulted in cracking at the interface because of the brittle intermetallic compounds that formed. The TIG brazing process, as described in this paper, offers a solution because the filler metal melts at a lower temperature than the base materials, allowing the joint to form without melting the steel. However, the process is sensitive to the welding current. In our project, we found that the optimal current was around 80 A, which is close to the 75 A reported in this paper. At this current, the joint achieved a tensile strength of approximately 200 MPa, which was sufficient for the application. The key was to control the heat input precisely to minimize the intermetallic compound layer thickness.

Key Questions and Reflections

One question that this paper raises is how the galvanized coating thickness affects the joint quality. The paper does not specify the coating thickness, but it is likely a standard galvanized coating of 10-15 μm. In practice, the coating thickness can vary, and this could affect the wetting behavior and the joint quality. Another question is how the joint performs under cyclic loading or in corrosive environments. Magnesium alloys are susceptible to corrosion, and the galvanic couple between magnesium and steel can accelerate corrosion. The paper does not address this issue, but it is a practical concern for any application where the joint will be exposed to the environment. The intermetallic compounds at the interface could also affect the fatigue performance of the joint, as they are brittle and can act as crack initiation sites.

Study Insights and Practical Implications

The key insight from this paper is that the welding current is the critical process parameter for TIG brazing of magnesium alloy to galvanized steel. The current must be high enough to ensure good wetting and avoid holes, but not so high that the intermetallic compound layer becomes excessively thick. The optimal current of 75 A represents a narrow process window, which means that the welding process must be tightly controlled. In practice, this means that the welding machine should have precise current control, and the operator should be trained to maintain a consistent arc length and travel speed. The paper also highlights the importance of the galvanized coating in promoting wetting. This suggests that the galvanized coating should be inspected before welding to ensure that it is intact and of the correct thickness. The fish-tail pattern observed in the joint is a useful indicator of good wetting, and it can be used as a quality control check during production.

Conclusion

This paper provides a valuable reference for TIG brazing of AZ31B magnesium alloy to galvanized steel. The finding that the welding current must be maintained around 75 A to achieve maximum joint strength is a critical practical insight. The intermetallic compounds that form at the interface are a concern, but their thickness can be controlled by optimizing the welding current. For anyone involved in dissimilar metal joining of magnesium alloys to steel, this paper offers a solid foundation for process development. The next step is to investigate the effect of galvanized coating thickness and to evaluate the joint performance under cyclic loading and in corrosive environments. The process has significant potential for lightweight structures, but the narrow process window and the brittleness of the intermetallic compounds must be carefully managed.