ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

TIG Welding Rapid Manufacturing of Metal Bodies: Performance Optimization

Introduction and Process Overview

Rapid manufacturing, also known as additive manufacturing or 3D printing, has revolutionized the way we think about producing metal components. While most of the attention has been on laser-based and electron beam-based processes, there is a simpler and more cost-effective approach that uses conventional TIG welding equipment. The paper by Luo Yong, Li Rui, and Zhang Hua from Jiangxi University of Science and Technology and Nanchang University describes a TIG welding-based rapid manufacturing process for producing metal bodies.

The concept is straightforward: a TIG torch is mounted on a positioning system, and metal is deposited layer by layer to build up a three-dimensional component. The process is similar to gas metal arc welding-based additive manufacturing, but uses TIG welding with a separate filler wire feed. The advantages of TIG-based rapid manufacturing include the ability to use a wide range of filler materials, precise control of heat input, and the ability to produce components with good surface quality.

Process Characteristics and Challenges

The authors describe the TIG rapid manufacturing process and its key characteristics:

Layer-by-Layer Deposition

The process builds components by depositing successive layers of weld metal. Each layer is typically 1-3 mm thick, depending on the welding parameters and the wire feed rate. The layers are deposited in a pattern that follows the cross-section of the component being built.

Microstructure Evolution

The microstructure of the deposited metal is complex and varies from layer to layer. Each layer undergoes a thermal cycle that includes rapid heating, melting, and cooling. The heat from subsequent layers can cause tempering or recrystallization of previously deposited layers. This results in a heterogeneous microstructure with varying grain sizes and phases.

Heat Accumulation

As the process continues, heat accumulates in the component. This can cause distortion, residual stresses, and even cracking in some materials. Controlling the heat input and the interpass temperature is critical to producing a sound component.

Surface Quality

The surface quality of the as-deposited component is generally rough, with a characteristic "weld bead" appearance. The surface roughness can be improved by post-process machining, but this adds cost and time.

Temperature Control System

The key contribution of this paper is the development of a temperature control system based on a neural network-PID controller with infrared temperature measurement. This is a significant advance because temperature control is one of the most critical aspects of TIG-based rapid manufacturing.

System Architecture

The temperature control system consists of the following components:

Component Function
Infrared pyrometer Measures the surface temperature of the deposited metal
Neural network controller Learns the relationship between process parameters and temperature
PID controller Provides closed-loop temperature control
TIG power supply Adjusts welding current based on controller output
Wire feeder Adjusts wire feed rate based on controller output

The neural network is trained using data from previous welding runs. It learns the relationship between the welding parameters (current, voltage, travel speed, wire feed rate) and the resulting temperature. The PID controller then uses this information to maintain the temperature within a specified range.

Working Principle

The system works as follows:

  1. The infrared pyrometer measures the surface temperature of the deposited metal.
  2. The measured temperature is compared to the setpoint temperature.
  3. The neural network-PID controller calculates the required adjustment to the welding parameters.
  4. The TIG power supply and wire feeder adjust the current and wire feed rate accordingly.
  5. The process repeats, maintaining the temperature within the desired range.

Benefits of Neural Network-PID Control

The combination of neural network and PID control offers several advantages over conventional PID control alone:

Performance Optimization

The authors also describe a technique called "surface metal wire-free welding heat treatment" that is used in combination with the temperature control system. This technique involves applying a final welding pass without filler wire to provide a controlled heat treatment to the surface of the component.

Effect on Microstructure

The combination of temperature control and surface heat treatment results in a more uniform microstructure. The grain size is more consistent throughout the component, and the presence of any undesirable phases is reduced.

Effect on Mechanical Properties

The authors report that the combination of temperature control and surface heat treatment improves the overall mechanical properties of the metal body. The tensile strength, yield strength, and ductility are all improved compared to components produced without temperature control.

Practical Considerations for Industrial Application

TIG-based rapid manufacturing has several advantages over laser-based processes for certain applications:

Cost

TIG welding equipment is significantly less expensive than laser welding equipment. A basic TIG welding setup can be purchased for a fraction of the cost of a laser welding system.

Material Flexibility

TIG welding can use a wide range of filler materials, including steels, stainless steels, nickel alloys, and titanium alloys. This makes it suitable for a broader range of applications.

Equipment Availability

TIG welding equipment is widely available and well-understood. Maintenance and repair are straightforward, and spare parts are readily available.

However, there are also limitations:

Deposition Rate

The deposition rate of TIG welding is lower than that of laser-based processes. This means that TIG-based rapid manufacturing is slower and more suitable for smaller components or components with simple geometries.

Heat Input

TIG welding typically has a higher heat input than laser welding, which can cause more distortion and residual stresses. This is why temperature control is so critical.

Surface Quality

The surface quality of TIG-deposited components is generally rougher than that of laser-deposited components. This may require additional machining or surface treatment.

Comparison with Other Additive Manufacturing Processes

Feature TIG-Based Laser-Based Electron Beam-Based
Equipment cost Low High Very high
Deposition rate Low Medium High
Material range Wide Wide Limited
Heat input High Medium Low
Surface quality Rough Good Excellent
Distortion High Medium Low

Conclusion

This paper presents a practical approach to TIG-based rapid manufacturing with integrated temperature control. The neural network-PID controller provides adaptive temperature control that improves the consistency and quality of the deposited metal. The surface heat treatment further enhances the mechanical properties. While TIG-based rapid manufacturing has limitations in deposition rate and surface quality, it offers a cost-effective alternative to laser-based processes for many applications. The temperature control system described in this paper is a significant contribution that addresses one of the key challenges in TIG-based rapid manufacturing. For any shop considering this technology, the insights from this paper provide a solid foundation for process development.