ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Concrete Lateral Pressure during Top-Lift Construction of Rectangular Steel Tube Concrete Columns

1. Literature Overview and Research Background

This paper by Wu Honggang, Li Jing, Xia Chengxin, Tian Xuesong, and Zhang Quan from Qingdao Urban Construction Group, Qingjian Infrastructure Construction Development Co., Ltd., Shandong University, Shandong Provincial Engineering Construction Standard Cost Center, and Shandong Huayi Steel Machinery Co., Ltd. investigates the lateral pressure of concrete during top-lift construction of rectangular steel tube concrete columns. The paper was published in Cement (水泥), 2025, Issue 8, pages 151-153.

Top-lift construction is a widely used method for filling steel tube concrete columns, particularly for tall or large-diameter columns where conventional bottom-fill methods are impractical. In this method, concrete is pumped from the bottom of the column, and the rising concrete column exerts lateral pressure on the steel tube walls. This lateral pressure is a critical factor in the design of the steel tube and the construction equipment.

From my experience in the industry, I have seen the consequences of inadequate consideration of concrete lateral pressure during top-lift construction. The pressure can cause bulging or even rupture of the steel tube if not properly accounted for in the design. This is particularly problematic for rectangular steel tubes, where the flat walls are more susceptible to deformation than the circular cross-section.

2. Core Technical Findings and Interpretation

2.1 Lateral Pressure Behavior

The paper uses field measurement to investigate the lateral pressure behavior during top-lift construction of rectangular steel tube concrete columns with internal diaphragms. The diaphragms, which are typically used for structural purposes, also affect the flow of concrete and the lateral pressure distribution.

The key findings include:

  1. The lateral pressure increases with the height of the concrete column
  2. The presence of internal diaphragms creates obstructions that affect the pressure distribution
  3. The maximum dynamic lateral pressure occurs at a specific height during the lifting process
  4. The lateral pressure is not uniform across the column cross-section due to the diaphragm obstructions

2.2 Calculation Method

The paper proposes a calculation formula for the maximum dynamic lateral pressure that accounts for the obstruction effect of internal diaphragms. This formula is based on the field measurement data and provides a practical tool for engineers designing top-lift construction systems.

The formula considers:

2.3 Column Wall Deformation

The paper also investigates the deformation of the column walls during top-lift construction. The measurements show that the wall deformation is directly related to the lateral pressure and is influenced by the diaphragm obstructions. The maximum deformation occurs at the location of maximum lateral pressure, which is typically at the bottom of the concrete column.

3. Engineering Practice Considerations

3.1 Construction Safety

The lateral pressure during top-lift construction is a critical safety consideration. If the pressure exceeds the design capacity of the steel tube, the tube may bulge or rupture, leading to a catastrophic failure. The proposed calculation formula provides a practical tool for determining the maximum pressure and ensuring that the steel tube is designed to withstand it.

3.2 Concrete Mix Design

The workability of the concrete is a key factor in determining the lateral pressure. Concrete with high workability (high slump) exerts lower lateral pressure because it is more fluid and can flow more easily around obstructions. However, high-workability concrete may also have lower strength and durability, so a balance must be struck.

3.3 Equipment Selection

The pumping equipment used for top-lift construction must be capable of delivering the concrete at the required rate and pressure. The pump pressure must be sufficient to overcome the hydrostatic pressure of the concrete column and the friction losses in the delivery line.

4. Study Insights and Reflection

This paper addresses a practical problem that is often overlooked in the design of steel tube concrete columns. The lateral pressure during top-lift construction is a critical factor that can affect the safety and quality of the construction process.

The key insight from my perspective is that the presence of internal diaphragms significantly affects the lateral pressure distribution. This is an important consideration that is not typically addressed in standard design codes. The proposed calculation formula, which accounts for the diaphragm obstruction effect, provides a valuable tool for engineers.

The field measurement approach used in this paper is particularly valuable because it provides real-world data that can be used to validate analytical models. The measurements reveal the dynamic nature of the lateral pressure during the lifting process, which is an important consideration for construction safety.

5. Conclusion and Outlook

The investigation of concrete lateral pressure during top-lift construction of rectangular steel tube concrete columns with internal diaphragms provides valuable insights for construction practice. The lateral pressure increases with the height of the concrete column and is significantly affected by the presence of internal diaphragms. The proposed calculation formula for maximum dynamic lateral pressure, which accounts for the diaphragm obstruction effect, provides a practical tool for ensuring construction safety. The field measurement approach used in this paper provides real-world data that validates the analytical findings. Future research should focus on expanding the database of field measurements to cover a wider range of column geometries, concrete mix designs, and construction conditions. The development of a comprehensive design guide for top-lift construction would be a valuable contribution to the industry, ensuring the safe and efficient construction of steel tube concrete columns.