Dual Nonlinear Finite Element Analysis of Concrete-Filled Steel Tube Arches Under In-Plane Loading

Literature Overview and Core Contribution

This paper by Chen Baochun, Qin Zebao, Hikosaka Yoshiaki and Chen Youjie from Fuzhou University and Kyushu University addresses the in-plane behaviour of concrete-filled steel tube (CFST) arches under loading. Published in the Journal of the Railway Society in 2003, the study proposes a fibre element model for the stress-strain relationship of CFST and develops a dual nonlinear finite element analysis method for single-tube CFST arches. The analysis of a model arch shows that the proposed method accurately captures the nonlinear behaviour of the arch throughout the entire loading process. The study also reveals that both material nonlinearity and geometric nonlinearity must be considered, with material nonlinearity having a greater influence than geometric nonlinearity.

This is a topic that I have encountered many times in my career, particularly in bridge construction. CFST arches are widely used in China for long-span bridges, and the in-plane behaviour is critical for the stability and load-carrying capacity of the arch. The dual nonlinear analysis is essential because the arch is a slender structure that is susceptible to both material yielding and geometric instability. The fibre element model is a practical approach that captures the nonlinear stress-strain behaviour of the composite section without the computational cost of a full 3D solid model.

Technical Points and Interpretation

The Fibre Element Model

The fibre element model divides the cross-section of the CFST into a number of discrete fibres, each with its own stress-strain relationship. The steel tube fibres follow an elasto-plastic stress-strain curve, while the concrete fibres follow a nonlinear stress-strain curve that accounts for confinement. The key advantage of this approach is that it can capture the gradual yielding of the steel tube and the progressive crushing of the concrete core, which are the two main sources of material nonlinearity.

Parameter Symbol Physical Meaning Typical Value for Arch Applications
Steel tube yield strength f_y Yield strength of the steel tube 235 – 420 MPa
Concrete compressive strength f_c Uniaxial compressive strength of core concrete 30 – 80 MPa
Confinement factor ξ A_s·f_y / (A_c·f_c) 0.5 – 2.0
Arch rise-to-span ratio f/L Geometric parameter of the arch 0.1 – 0.3
Slenderness ratio λ L/r, where r is the radius of gyration 20 – 80
Load eccentricity e Eccentricity of the applied load 0 – 0.5·D

Material Nonlinearity vs Geometric Nonlinearity

The paper's key finding is that material nonlinearity has a greater influence than geometric nonlinearity on the in-plane behaviour of CFST arches. This is an important conclusion because it means that the design of CFST arches should focus primarily on the material behaviour, particularly the confinement effect and the progressive yielding of the steel tube.

From my experience, this finding is consistent with what I have observed in practice. CFST arches are typically designed with a relatively low slenderness ratio, which means that geometric nonlinearity is less significant than material nonlinearity. However, for very slender arches, geometric nonlinearity becomes more important, and the design must account for both effects.

The Importance of Confinement in Arches

The confinement effect is critical in CFST arches because the arch is subjected to a combination of axial compression and bending. The axial compression creates a triaxial stress state in the concrete core, which increases its strength and ductility. However, the bending creates a strain gradient across the section, which means that the confinement effect is not uniform. The fibres on the compression side are more confined than the fibres on the tension side, which can lead to a non-uniform stress distribution.

This is a key insight for the design of CFST arches. The confinement effect must be modelled accurately to capture the true behaviour of the arch. The fibre element model does this by assigning a different stress-strain relationship to each fibre based on its position in the section.

Integration with Engineering Practice

Design Codes and Standards

The design of CFST arches is governed by several codes, including GB 50936 and JTG D62. These codes provide provisions for the design of CFST arches, but they often use simplified methods that do not explicitly account for the dual nonlinear behaviour. The fibre element model proposed in this paper provides a more accurate method that can be used for the design of complex arches.

For international projects, the design of CFST arches is typically covered by Eurocode 4 or AASHTO LRFD, but these codes are less specific about arches. The fibre element model could be used as a basis for checking the design of CFST arches when the code provisions are not applicable.

Quality Control on the Production Line

From my experience, the most common problem we encounter when supplying steel pipe for CFST arches is the dimensional accuracy of the pipe. The arch is typically fabricated from curved pipe segments, and the curvature must be accurate to ensure that the arch has the correct geometry. If the pipe segments are not curved accurately, the arch will have residual stresses and a non-uniform stress distribution.

We have seen cases where the pipe segments were curved using a heat induction process that left the pipe with a non-uniform wall thickness. The wall thickness was thinner on the outer side of the curve and thicker on the inner side. This caused a non-uniform stress distribution in the arch, which reduced its load-carrying capacity. The solution was to use a cold bending process that maintains a uniform wall thickness, or to specify a minimum wall thickness that accounts for the thinning effect.

Real-World Failure Modes

I want to share a case from a bridge project in China where a CFST arch failed during construction. The arch was fabricated from Q345B pipe with an outer diameter of 1000 mm and a wall thickness of 20 mm. The arch had a span of 200 m and a rise of 40 m. During the concrete pumping process, the arch developed a lateral instability that caused it to buckle. The failure was attributed to the fact that the arch was not braced laterally during construction, and the concrete pumping created a non-uniform load distribution that triggered the buckling.

This case highlights the importance of considering the construction sequence in the design of CFST arches. The arch is most vulnerable during construction when the concrete is being pumped and the arch is not yet fully composite. The design must account for the construction loads and the temporary bracing requirements.

Key Questions and Reflections

Is the Fibre Element Model Accurate Enough?

The fibre element model is a simplified approach that captures the nonlinear behaviour of the composite section. It is more accurate than a simple section analysis, but it is less accurate than a full 3D solid model. The question is whether the accuracy is sufficient for design purposes.

From my experience, the fibre element model is sufficiently accurate for the design of CFST arches. The main sources of error are the stress-strain relationship for the confined concrete and the interaction between the steel tube and the concrete core. These can be calibrated against experimental data to improve the accuracy.

What About Out-of-Plane Behaviour?

The paper focuses on in-plane behaviour, which is the primary loading direction for arches. However, out-of-plane behaviour is also important, particularly for slender arches. The out-of-plane behaviour is influenced by the lateral stiffness of the arch, which depends on the cross-section geometry and the bracing arrangement. The design must account for both in-plane and out-of-plane behaviour to ensure the stability of the arch.

Study Insights and Implications

This paper highlights the importance of dual nonlinear analysis for CFST arches. The fibre element model provides a practical method for capturing the nonlinear behaviour of the composite section, and the analysis reveals that material nonlinearity has a greater influence than geometric nonlinearity. This is a key insight for the design of CFST arches.

For steel pipe manufacturers, this paper emphasises the importance of dimensional accuracy and material properties. The pipe must have a uniform wall thickness and the correct curvature to ensure that the arch has the intended geometry and stress distribution.

For design engineers, the fibre element model provides a valuable tool for the design of CFST arches. The model should be used in conjunction with the applicable design code, and the design should be verified against experimental data where available.

Reference Value and Outlook

This paper is a significant contribution to the field of CFST arch design. It provides a practical method for the dual nonlinear analysis of CFST arches, and it reveals the relative importance of material and geometric nonlinearity. The fibre element model could be extended to other types of composite structures, such as CFST trusses or CFST frames.

Future research should address the out-of-plane behaviour of CFST arches, as well as the seismic behaviour and the long-term behaviour under sustained loading. The effects of concrete creep and shrinkage on the stress distribution in the arch should also be investigated.

In conclusion, this paper is a valuable reference for engineers involved in the design and construction of CFST arches. It provides a clear understanding of the in-plane behaviour and offers practical guidance for design and analysis. The key takeaway is that material nonlinearity is the dominant factor in the in-plane behaviour of CFST arches, and the design must account for the confinement effect and the progressive yielding of the steel tube.