ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Marine Steel Structure Steel Pipe Rolling and Lengthening Technology

Literature Overview and Core Findings

This study by Li Tongyue and colleagues at Offshore Oil Engineering (Qingdao) Co., Ltd. addresses the practical challenges of manufacturing large-diameter steel pipes for marine structures. As offshore platforms proliferate, the demand for steel pipes in columns, braces, and joint tubes has increased. Due to limitations in wall thickness and diameter, these pipes are typically manufactured by rolling steel plates and welding the longitudinal seam. The study summarizes the process flow and methods for rolling and lengthening welded steel pipes, providing a reference for quality control in marine steel structure construction.

The key technical points are the process sequence and the quality control measures for each step. The rolling process involves forming the plate into a cylindrical shape, followed by welding the longitudinal seam. The lengthening process involves welding multiple pipe sections together to achieve the required length. The study emphasizes the importance of controlling the rolling parameters, the weld quality, and the dimensional accuracy throughout the process.

Technical Parameter Analysis and Practical Implications

Process Step Key Parameters Quality Control Measures
Plate preparation Plate thickness, width, edge preparation Verify dimensions, edge quality
Rolling Roller position, bending radius, number of passes Check roundness, diameter, ovality
Longitudinal welding Welding process, parameters, filler material 100% NDT, weld profile inspection
Pipe lengthening Fit-up, welding sequence, tack welding Check alignment, weld quality
Final inspection Dimensional checks, NDT, hydrostatic test Verify compliance with specifications

From a manufacturing perspective, the rolling process is the most critical step. The plate must be rolled to the correct diameter with minimal ovality. In my experience, the ovality of the rolled pipe is a common problem, especially for thin-walled pipes. The ovality can be controlled by using a three-roll or four-roll bending machine and by adjusting the roller positions during the rolling process. The number of passes is also important. Too few passes can result in a non-uniform curvature, while too many passes can cause work hardening of the plate.

The longitudinal weld is the next critical step. For marine structures, the weld quality must be excellent because the pipes are subjected to cyclic loading from waves and wind. The welding process should be selected based on the plate thickness and material. For thick plates, submerged arc welding (SAW) is typically used because of its high deposition rate and good weld quality. For thinner plates, gas metal arc welding (GMAW) or flux-cored arc welding (FCAW) may be more appropriate.

Engineering Practice and Delivery Considerations

The lengthening process is where many problems occur in practice. When welding two pipe sections together, the fit-up must be precise to avoid misalignment. Misalignment creates a stress concentration at the weld, which can lead to fatigue failure. The welding sequence is also important. A proper welding sequence can minimize the residual stresses and distortion. In my experience, the use of a rotating jig or a positioner can significantly improve the weld quality and reduce the distortion.

The quality control for the lengthening welds should include 100% ultrasonic testing or radiographic testing. The weld should also be inspected for surface defects using magnetic particle or dye penetrant testing. The hydrostatic test is the final verification of the pipe's integrity. The test pressure should be calculated based on the pipe's design pressure and the material properties.

From a delivery perspective, the pipes must be protected from corrosion during transport and storage. The marine environment is highly corrosive, and the pipes should be coated or wrapped before shipment. The marking on the pipes should be clear and durable, indicating the pipe grade, diameter, wall thickness, and heat number. The documentation should include the material certificates, the weld procedures, and the NDT results.

Study Insights and Reflections

This study provides a practical overview of the rolling and lengthening process for marine steel pipes. The key takeaway is that the process is well-established but requires careful quality control at each step. The rolling process is the most critical because it determines the dimensional accuracy of the pipe. The lengthening process is also important because the weld quality determines the pipe's integrity under cyclic loading.

The study is limited by the lack of specific process parameters and quality control criteria. In practice, the process parameters must be determined based on the specific material and the pipe dimensions. The quality control criteria should be based on the applicable standards, such as API 5L for line pipe or DNV-ST-F101 for subsea pipelines.

From a delivery perspective, the pipes should be delivered with the necessary end preparation for the subsequent welding operations. The ends should be beveled to the correct angle and the bevel should be clean and free of defects. The pipe ends should be protected with end caps to prevent damage during transport.