Investigation and Discussion on Several Issues in the Development of Composite or Clad Steel Pipes (Part 1)

Literature Overview and Core Technical Concept

This paper by He Defu and Wang Jingying from Shanghai Jiuli Industry and Trade Development Co., Ltd. and Zhejiang Dechuan Pipe Industry Co., Ltd. provides a comprehensive examination of the development of composite or clad steel pipes, which are essential for applications requiring corrosion resistance in aggressive environments. The paper distinguishes between metallurgical composite pipes, where the corrosion-resistant alloy (CRA) layer is metallurgically bonded to the carbon steel substrate through processes such as roll bonding, explosive bonding, or weld overlay, and mechanical lined pipes, where the CRA layer is mechanically expanded against the carbon steel pipe without a metallurgical bond. The authors discuss the development trends of these two types, highlighting the advantages and limitations of each. The core technical focus is on the quality of the weld joints in these composite pipes, particularly for pipes with internal CRA weld overlay, and the methods to optimize weld quality and ensure the manufacturing and application quality of mechanically lined pipes. The paper also compares the heat treatment standards for composite steel plates and pipes between domestic and international standards, and discusses the inspection methods for bond quality, as well as the material selection criteria for composite pipes.

Technical Interpretation and Manufacturing Process Analysis

The fundamental difference between metallurgical composite pipes and mechanically lined pipes lies in the nature of the bond between the CRA layer and the carbon steel substrate. In metallurgical composite pipes, the bond is achieved through atomic diffusion or fusion, resulting in a bond strength that is typically higher than the yield strength of the weaker material, and the interface is continuous and free of gaps. In mechanically lined pipes, the CRA liner is expanded against the carbon steel pipe, creating a mechanical interference fit, but the bond is not metallurgical, and there is a potential for gaps or delamination under certain loading conditions. The manufacturing process for metallurgical composite pipes includes roll bonding, where the CRA plate and the carbon steel plate are hot-rolled together to achieve diffusion bonding; explosive bonding, where a controlled explosion is used to impact the CRA plate onto the carbon steel substrate; and weld overlay, where the CRA material is deposited onto the inner surface of the carbon steel pipe using welding processes such as submerged arc welding (SAW) or gas tungsten arc welding (GTAW). Each method has its own advantages and limitations in terms of cost, bond quality, and the range of CRA materials that can be used. For mechanically lined pipes, the process typically involves inserting a CRA liner into the carbon steel pipe and then expanding it using a hydraulic or mechanical mandrel to achieve a tight fit. The quality of the mechanical bond depends on the precision of the pipe dimensions, the expansion ratio, and the surface finish of both the liner and the carbon steel pipe.

Manufacturing Method Bond Type Typical Bond Strength Advantages Limitations
Roll bonding Metallurgical > 200 MPa Large area, uniform bond Limited to plate form, requires hot rolling
Explosive bonding Metallurgical > 300 MPa High bond strength, wide material range Limited to plate form, safety concerns
Weld overlay Metallurgical > 400 MPa Applicable to pipe form, flexible Low deposition rate, dilution issues
Mechanical expansion Mechanical Interference fit Low cost, simple process Risk of gaps, limited to low-pressure applications

Weld Quality and Defect Analysis

The paper places significant emphasis on the weld quality of composite pipes, particularly for pipes with internal CRA weld overlay. In my experience, the most critical issue with weld overlay on the inner surface of carbon steel pipes is the dilution of the CRA layer by the carbon steel substrate. Dilution occurs when the welding heat melts a portion of the carbon steel, which then mixes with the deposited CRA material, reducing its corrosion resistance. The degree of dilution depends on the welding process, the welding parameters, and the number of passes. For example, with SAW, the dilution can be as high as 20-30% in the first pass, which is unacceptable for most CRA materials. To achieve the required corrosion resistance, the weld overlay must be applied in multiple passes, with the final pass having a dilution of less than 5%. This requires careful control of the welding parameters, including the welding current, voltage, travel speed, and the composition of the filler metal. In practice, I have seen many cases where insufficient attention to dilution control resulted in premature corrosion failure of the weld overlay, leading to costly repairs or even the replacement of the entire pipe section. Another critical issue is the formation of defects such as lack of fusion, porosity, and cracks in the weld overlay. These defects can serve as initiation sites for corrosion, and they must be detected and repaired before the pipe is put into service. Non-destructive testing methods such as ultrasonic testing (UT) and eddy current testing (ET) are commonly used to detect these defects, but their sensitivity depends on the geometry of the weld overlay and the orientation of the defects.

Standards Comparison and Inspection Methods

The paper compares the heat treatment standards for composite steel plates and pipes between domestic and international standards, highlighting significant differences in the requirements for post-weld heat treatment (PWHT). For example, the ASME Boiler and Pressure Vessel Code (Section VIII) requires PWHT for composite pipes with a carbon steel substrate thickness above a certain value, while the Chinese standard GB 150 may have different requirements. The purpose of PWHT is to relieve residual stresses in the weld and the heat-affected zone, which can reduce the risk of stress corrosion cracking (SCC) and improve the fracture toughness of the material. However, PWHT can also have adverse effects on the CRA layer, such as sensitization in stainless steels, which reduces their corrosion resistance. Therefore, the selection of the PWHT temperature and time must be carefully balanced to achieve the desired stress relief without compromising the corrosion resistance of the CRA layer. The bond quality inspection methods for composite pipes are also discussed, including ultrasonic testing (UT) for the detection of disbonding, and shear testing for the evaluation of bond strength. In my experience, the most reliable method for evaluating bond quality is a combination of UT and destructive testing, where samples are cut from the pipe and tested in shear to determine the bond strength. However, destructive testing is not practical for all pipes, so UT is typically used for 100% inspection, with destructive testing performed on a sampling basis. The acceptance criteria for bond quality vary depending on the application, but a common requirement is that the bond strength should be at least 80% of the yield strength of the weaker material, and the disbonded area should not exceed 5% of the total bond area.

Engineering Practice and Application Considerations

The selection of composite pipes for a given application depends on several factors, including the corrosivity of the transported fluid, the operating pressure and temperature, the design life, and the cost of the pipe. For applications with highly corrosive fluids, such as sour gas containing hydrogen sulfide, metallurgical composite pipes are preferred because the metallurgical bond provides a continuous barrier against corrosion, and the CRA layer can be selected based on its resistance to sulfide stress cracking (SSC) and hydrogen-induced cracking (HIC). For applications with moderately corrosive fluids, mechanically lined pipes may be a more economical choice, but the risk of liner collapse or disbonding under pressure cycling must be carefully evaluated. In my experience, the most common failure mode for mechanically lined pipes is the collapse of the liner due to the formation of a vacuum during pipeline depressurization, or the buckling of the liner due to compressive stresses during bending. These issues can be mitigated by proper design of the liner thickness and the expansion ratio, as well as by the use of special end connections that prevent the ingress of the process fluid into the annulus between the liner and the carbon steel pipe. The paper also discusses the material selection criteria for composite pipes, which involve the compatibility of the CRA material with the process fluid, the mechanical properties of the CRA material, and the weldability of the CRA material to the carbon steel substrate. In practice, the most commonly used CRA materials are austenitic stainless steels (such as 316L and 904L), duplex stainless steels (such as 2205 and 2507), and nickel-based alloys (such as Alloy 825 and Alloy 625). The selection of the CRA material should be based on the results of corrosion testing, such as ASTM G48 for pitting and crevice corrosion, and ASTM G39 for SCC, rather than solely on the nominal composition of the alloy.

Key Questions and Reflections

One of the key questions that this paper raises is the long-term reliability of composite pipes, particularly the behavior of the bond interface under cyclic loading and thermal cycling. For metallurgical composite pipes, the bond interface is typically free of defects, but the difference in the coefficient of thermal expansion between the CRA layer and the carbon steel substrate can generate thermal stresses that may lead to fatigue cracking of the bond interface. For mechanically lined pipes, the bond interface is a mechanical interference fit, and the liner can move relative to the carbon steel pipe under cyclic loading, leading to fretting wear and potential fatigue failure. These issues are not fully addressed in the paper, but they are critical for the long-term performance of composite pipes in service. Another key question is the inspectability of composite pipes during service. The presence of the CRA layer makes it difficult to inspect the carbon steel substrate using conventional UT methods, because the CRA layer can interfere with the propagation of ultrasonic waves. This requires the development of specialized inspection techniques, such as the use of phased array UT or the use of electromagnetic acoustic transducers (EMAT), which can penetrate the CRA layer and detect defects in the carbon steel substrate. In my experience, the lack of reliable in-service inspection methods for composite pipes has been a significant barrier to their widespread adoption, particularly in the oil and gas industry, where pipeline integrity is of paramount importance.

Study Insights and Practical Recommendations

The main takeaway from this paper is that the selection of composite pipes requires a thorough understanding of the manufacturing process, the weld quality, and the inspection methods, as well as the specific requirements of the application. The paper provides a valuable overview of the current state of the art, but it also highlights the need for further research on the long-term behavior of composite pipes, particularly in terms of fatigue, thermal cycling, and in-service inspection. From a manufacturing perspective, the key to producing high-quality composite pipes is the control of the weld overlay process, particularly the dilution of the CRA layer, and the proper application of PWHT to relieve residual stresses without compromising the corrosion resistance of the CRA layer. In practice, I would recommend that engineers specify composite pipes based on the results of corrosion testing, rather than on the nominal composition of the CRA material, and that they require 100% UT inspection of the bond interface, with destructive testing performed on a sampling basis. Additionally, the design of the pipe should account for the potential for liner collapse or disbonding in mechanically lined pipes, and the appropriate end connections should be selected to prevent the ingress of the process fluid into the annulus. The paper also emphasizes the importance of selecting the appropriate CRA material based on the specific corrosivity of the process fluid, and I would add that the selection should also consider the weldability of the CRA material and its compatibility with the carbon steel substrate.

Concluding Remarks

This paper provides a comprehensive and insightful examination of the development of composite or clad steel pipes, covering the fundamental differences between metallurgical and mechanical bonding, the manufacturing processes, the weld quality issues, and the inspection methods. The paper is particularly valuable for its discussion of the heat treatment standards and the bond quality inspection methods, which are critical for ensuring the long-term reliability of composite pipes. However, the paper also highlights the need for further research on the long-term behavior of composite pipes, particularly in terms of fatigue and thermal cycling, as well as the need for improved in-service inspection methods. For engineers involved in the selection, manufacturing, or application of composite pipes, this paper serves as a valuable reference, but it should be used in conjunction with sound engineering judgment and a thorough understanding of the specific requirements of the application. The success of composite pipes depends not only on the quality of the manufacturing process but also on the careful selection of the CRA material and the proper design of the pipe for the intended service conditions. In my experience, the most common cause of failure in composite pipes is not the manufacturing process but the lack of attention to the service conditions, particularly the corrosivity of the process fluid and the potential for liner collapse or disbonding. Therefore, I would encourage fellow engineers to approach the selection of composite pipes with a thorough understanding of the application, and to verify all design assumptions through careful analysis and testing before committing to their use in a project.