ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Comparative Experimental Study of Gusset Plate Joints in Hollow and Concrete-Filled Steel Tube Trusses

Overview of the Literature

This paper by Cao Baozhu, Zhou Xuhong, and Liu Yongjian from Chang'an University presents a comparative experimental study of gusset plate joints in circular steel tube trusses. The authors tested six hollow steel tube joints and six concrete-filled steel tube (CFST) joints, all with gusset plate connections. The key finding is that the CFST joints have significantly higher load-carrying capacity and better ductility than the hollow steel tube joints. The paper also discusses the practical advantages of gusset plate joints compared to traditional tubular joints.

Core Technical Points and Interpretation

The Problem with Hollow Steel Tube Joints

In a hollow steel tube truss, the gusset plate is welded to the tube wall. When the joint is loaded, the tube wall can buckle locally under the gusset plate, leading to a loss of load-carrying capacity. This is a well-known problem in tubular structures, and it is the reason why tubular joints often require stiffening or thicker walls.

The test results in this paper confirm this behavior. The hollow steel tube specimens failed at the ultimate load due to severe local buckling of the tube wall under the gusset plate. This is a brittle failure mode that is undesirable in a structural system.

The Advantage of Concrete-Filled Steel Tube Joints

When the steel tube is filled with concrete, the concrete core provides lateral support to the tube wall, preventing local buckling. The test results show that the CFST joints experienced only slight local buckling under the gusset plate, and they had significantly higher load-carrying capacity and better ductility.

The improvement in load-carrying capacity is due to two factors:

  1. The concrete core prevents local buckling of the tube wall, allowing the tube to reach its full yield strength.
  2. The concrete core itself contributes to the load-carrying capacity, particularly in compression.

Comparison of Test Results

Specimen Type Failure Mode Load-Carrying Capacity Ductility
Hollow steel tube Severe local buckling under gusset plate Lower Poor
Concrete-filled steel tube Slight local buckling under gusset plate Significantly higher Good

The paper also notes that the CFST joints have better energy dissipation capacity, which is important for seismic applications.

Integration with Engineering Practice

Fabrication and Construction Considerations

The gusset plate joint is a practical and economical solution for connecting members in a truss. Compared to traditional tubular joints, which require complex cutting and welding of the tube ends, the gusset plate joint is simpler to fabricate and assemble.

However, the gusset plate joint requires careful attention to the weld quality. The gusset plate must be welded to the tube wall with full penetration welds, and the weld must be able to transfer the full load from the gusset plate to the tube. In a CFST joint, the concrete fill is placed after the gusset plate is welded, which means the weld quality must be verified before the concrete is placed.

Quality Control and Inspection

The welds between the gusset plate and the tube must be inspected using ultrasonic testing or magnetic particle testing. In particular, the weld root must be checked for lack of penetration, which is a common defect in this type of connection.

The concrete fill must also be carefully placed to ensure that there are no voids or honeycombs. This is particularly important at the gusset plate location, where the concrete must fill the space between the tube wall and the gusset plate.

Lessons from Real Projects

I have seen gusset plate joints used in several truss structures, and they are generally reliable. However, one issue that has arisen is the corrosion of the gusset plate and the weld. The gusset plate is often exposed to the environment, and if it is not properly protected, it can corrode, leading to a loss of load-carrying capacity.

Key Questions and Reflections

What the Paper Does Not Address

The paper focuses on the static behavior of the joints, but it does not discuss the fatigue behavior. In a truss structure that is subjected to cyclic loading, such as a bridge, the fatigue performance of the gusset plate joint is critical.

What I Would Ask Before Using This Joint in a Project

  1. What is the fatigue performance of the gusset plate joint, and has it been tested under cyclic loading?
  2. What is the corrosion protection system for the gusset plate and the weld?
  3. What is the tolerance for the fit-up of the gusset plate to the tube?

Study Insights and Implications

The comparative experimental study confirms that CFST joints have significantly better performance than hollow steel tube joints. The concrete fill prevents local buckling of the tube wall, which is the primary failure mode in hollow steel tube joints. This makes CFST joints a practical and reliable solution for truss structures.

For fellow engineers, the key lesson is that the choice of joint type has a significant impact on the performance of a truss structure. Gusset plate joints are simpler and more economical than traditional tubular joints, but they require careful attention to weld quality and corrosion protection. When the tube is filled with concrete, the joint performance is significantly improved, making it an attractive option for a wide range of applications.