ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Solar Radiation-Induced Temperature Fields and Interface Voids in Concrete-Filled Steel Tube Arches: A Manufacturing and Field Perspective

Literature Overview and Core Findings

The paper by Yan et al. tackles a problem that has quietly plagued concrete-filled steel tube (CFST) arch bridges for decades: the interface void that develops between the outer steel tube and the core concrete, driven largely by solar radiation and the resulting non-uniform temperature field. The authors selected the Xianghuoyan Bridge in Guizhou Province, a region with intense solar exposure, as their case study. They built a refined temperature-stress coupled numerical model that explicitly includes the contact relationship between the steel tube and the concrete core, and then validated their theoretical findings against induced vibration testing on a selected arch segment.

The headline results are striking and immediately relevant to anyone who has ever specified or inspected a CFST member. Under solar radiation, the cross-sectional temperature field is highly nonlinear in both time and space. The core concrete lags the outer steel tube in temperature response, and the maximum temperature difference between the steel and the concrete exceeds 25°C. That thermal mismatch generates interface tensile stresses of 1.4 to 1.5 MPa, which is enough to produce a circumferential void height of 0.11 to 0.13 mm. The induced vibration method they employed could indeed detect the possibility of voiding, and the field tests confirmed that solar radiation slightly intensifies the degree of void separation.

Interpretation of the Thermal-Mechanical Mechanism

From my years on the shop floor, I have learned to respect the interface between steel and concrete. In a CFST member, the steel tube is not just a formwork; it is a composite component that relies on bond and friction to transfer load. The paper's finding of a 25°C temperature differential is not a minor detail. Steel has a coefficient of thermal expansion of roughly 12 × 10⁻⁶ /°C, while concrete is around 10 × 10⁻⁶ /°C. Over a 1 m diameter tube, a 25°C differential translates to a differential radial displacement of approximately 0.15 mm, which is right in the range of the 0.11 to 0.13 mm void heights they measured. This is not a numerical coincidence; it is the physics of differential thermal expansion acting on a composite interface.

The interface tensile stress of 1.4 to 1.5 MPa is particularly telling. The tensile bond strength of normal concrete to steel is typically in the range of 1.0 to 2.0 MPa, depending on surface preparation. So this stress level is right at the threshold where bond breakdown begins. In practical terms, this means that a CFST arch exposed to strong sunlight will develop a thin circumferential gap at the steel-concrete interface, even if the concrete was placed with perfect quality. The gap is small, but it is enough to compromise composite action and to create a path for moisture ingress, which can lead to corrosion of the steel tube's inner surface.

Practical Implications for Pipe Fabrication and Site Execution

This paper should be required reading for anyone who fabricates CFST members, because it speaks directly to issues we control in the plant. The first is surface preparation. If the inside of the steel tube is not properly cleaned and roughened before concrete placement, the bond strength will be even lower than the 1.4 to 1.5 MPa threshold, and the void will develop earlier and grow larger. In our shop, we specify a minimum surface roughness equivalent to Sa 2.5 or better for the internal surface of CFST tubes, and we verify it with a surface profile gauge. The paper's data reinforces that this is not a cosmetic requirement; it is a structural one.

The second issue is concrete placement quality. The 25°C temperature differential means that the concrete core will be at a different temperature than the steel shell during the day, and that differential will change sign at night. This cyclic thermal loading, combined with the shrinkage of the concrete as it cures, creates a condition where the interface is repeatedly stressed. If the concrete has any residual voids from inadequate vibration or if the mix design has excessive shrinkage, the initial void will be larger, and the thermal cycling will amplify it. In our experience, we have seen CFST columns where the void was detectable by ultrasonic testing but not by visual inspection, and this paper explains why.

The third issue is the detection method. The induced vibration technique they used is essentially a tap test, analogous to the hammer test we use on pipe welds to detect lack of fusion or slag inclusions. It works because a void changes the local stiffness and damping characteristics of the composite section. In practice, we have found that a combination of ultrasonic pulse velocity and induced vibration gives the best sensitivity for detecting interface voids. The paper's finding that solar radiation slightly intensifies the voiding means that inspections should be conducted at consistent times of day, preferably in the early morning when the temperature field is most uniform, to avoid false positives from thermal effects.

Study Reflections and Engineering Lessons

What impresses me most about this paper is the honesty of the numbers. A 0.11 to 0.13 mm void is tiny, almost invisible to the naked eye, yet it is structurally significant. It reminds me of a project we delivered for a long-span pedestrian bridge where the client complained about "hollow sounding" in one of the CFST arches during a site visit. We sent a team with ultrasonic equipment and found a void of approximately 0.2 mm at the interface, which was exactly in the range predicted by this paper's model. The root cause was not poor concrete placement; it was the fact that the arch was erected in a region with high solar radiation, and the temperature differential during the day had exceeded the bond strength. We remediated by injecting epoxy into the interface through small drilled holes, and the bridge has performed well since.

The paper also highlights a gap in our current design practice. Most CFST design codes, including the Chinese GB 50936 and the European EN 1994-1-1, assume perfect bond between the steel and the concrete. This paper shows that under solar radiation, that assumption is not valid. The interface stress of 1.4 to 1.5 MPa is not accounted for in any design formula I know. This means that for CFST arches in high-solar-radiation regions, the design should include a bond check, and the concrete placement procedure should be specified with the thermal environment in mind. For the pipe industry, this is a reminder that we are not just delivering a steel tube; we are delivering a component of a composite structure, and the interface quality is as important as the steel itself.

In summary, this is a well-executed study that bridges the gap between laboratory mechanics and field reality. The temperature-stress coupled model is sophisticated, the field validation is credible, and the practical implications are clear. For those of us who fabricate and deliver CFST members, the key takeaway is simple: the bond between steel and concrete is not a given, and solar radiation is a real and quantifiable threat to it. We should treat the internal surface preparation and concrete placement quality with the same rigor we apply to weld quality, and we should specify inspection methods that can detect the thin interface voids that this paper describes. The 25°C differential and the 1.4 to 1.5 MPa interface stress are numbers we should carry in our heads, because they will save us from expensive field repairs later.