ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Compression-Bending Performance and Bearing Capacity Calculation of Concrete-Filled Steel Tube Composite Columns

Literature Overview and Study Motivation

This paper by Ke Xiaojun and colleagues from Guangxi University and Northeast Electric Power University investigates the compression-bending performance of concrete-filled steel tube (CFST) composite columns and proposes a new method for calculating their bearing capacity. The motivation for the study is a significant deficiency in the current design code CECS 188:2005, which is used for the design of composite columns. The code does not account for the contribution of the steel tube to the bearing capacity, which means that the full capacity of the composite column is not utilised. This is a conservative but also an uneconomical approach, and it can lead to larger column sections than necessary.

The authors conducted eccentric compression tests on CFST composite columns to study their failure modes and the confinement mechanism. Based on the test results, they developed a theoretical model for the bearing capacity that accounts for the steel tube and its confinement effect. The model was validated against 40 sets of test data, and the results show that it is accurate and reliable. This is a significant contribution to the field, because it provides a rational basis for the design of CFST composite columns that fully utilises the capacity of all the components.

Key Technical Points and Interpretation

Failure Modes and the Boundary Criterion

The test results show that CFST composite columns fail in two distinct modes, depending on the eccentricity of the applied load:

  1. Large eccentricity failure: The failure is initiated by the yielding of the longitudinal reinforcement in the tension zone, followed by the crushing of the concrete in the compression zone. This is a ductile failure mode, and it is similar to the failure of a conventional reinforced concrete column.
  2. Small eccentricity failure: The failure is initiated by the crushing of the concrete in the compression zone, while the reinforcement in the tension zone may not reach its yield strength. This is a more brittle failure mode, and it is similar to the failure of a heavily loaded reinforced concrete column.

The boundary between the two modes is defined by the condition that the tension reinforcement reaches its yield strength at the same time that the concrete in the compression zone reaches its ultimate compressive strain. This is the classic balanced failure condition, and it is used as the basis for the design of the column.

The authors also observed that the cross-section of the column remains plane after deformation, which confirms that the plane-section assumption is valid for the analysis of CFST composite columns. This is an important finding, because it means that the strain distribution across the section can be determined using the standard beam theory, and the internal forces can be calculated by integrating the stress-strain relationships of the individual components.

Confinement Effect of the Steel Tube

One of the most interesting findings of the study is the effect of the eccentricity on the confinement provided by the steel tube. The authors measured the transverse strain of the steel tube, and they found that the transverse strain increases as the eccentricity decreases. This means that the confinement effect is stronger for columns with a smaller eccentricity, which are closer to the axial compression condition. For columns with a large eccentricity, the confinement effect is weaker, because the bending-induced tension on one side of the column reduces the compressive stress in the steel tube.

This finding has important implications for the design of CFST composite columns. For columns that are primarily subjected to axial load, the confinement effect can significantly enhance the bearing capacity, and it should be taken into account. For columns that are subjected to a large bending moment, the confinement effect is less significant, and a simpler design approach may be sufficient.

Proposed Bearing Capacity Calculation Method

The authors propose a new method for calculating the bearing capacity of CFST composite columns under combined compression and bending. The method is based on the following principles:

  1. The cross-section is divided into the concrete core, the steel tube, and the longitudinal reinforcement.
  2. The strain distribution across the section is determined using the plane-section assumption.
  3. The stress in each component is determined using the appropriate stress-strain relationship.
  4. The internal forces are calculated by integrating the stresses over the cross-section.
  5. The bearing capacity is determined by finding the combination of axial load and bending moment that satisfies the equilibrium and the compatibility conditions.

The method accounts for the confinement effect of the steel tube, which is modelled using a confinement factor that depends on the eccentricity and the geometric properties of the section. The method was validated against 40 sets of test data, and the results show that the predicted capacities are in good agreement with the experimental values.

Integration with Manufacturing and Delivery Practice

Steel Tube Fabrication and Quality Requirements

The findings of this paper have direct implications for the fabrication of the steel tube used in CFST composite columns. The confinement effect depends on the ability of the steel tube to resist the transverse expansion of the concrete core, which means that the tube must have sufficient stiffness and strength in the circumferential direction. This requires:

In practice, the steel tube is typically a seamless or ERW pipe, and it is often fabricated with a slight taper or with stiffening rings to enhance the confinement effect. The internal surface of the tube must be clean and free from defects, because any discontinuity can act as a stress raiser and initiate a crack.

Concrete Placement and Compaction

The confinement effect also depends on the quality of the concrete core. If the concrete is not properly compacted, there will be voids or honeycombs between the concrete and the steel tube, and the confinement effect will be reduced. This is particularly important for columns with a small eccentricity, where the confinement effect is the strongest.

In practice, the concrete is placed by pumping from the bottom of the column, and the compaction is achieved by the pressure of the pumped concrete and by the use of vibrators. The placement sequence must be carefully planned to ensure that the concrete fills the entire cross-section without segregation or voids. The use of self-compacting concrete can be advantageous, because it does not require vibration and it can flow around the reinforcement and the steel tube.

Inspection and Testing

The paper's emphasis on the confinement effect highlights the importance of inspecting the quality of the concrete core and the bond between the steel and the concrete. The inspection methods include:

For critical applications, a full-scale test on a prototype column is recommended, to verify the design and the construction quality. The test should include strain gauges on the steel tube and the reinforcement, as well as displacement transducers to measure the lateral deflection and the axial shortening.

Key Questions and Reflections

Why the Current Code is Inadequate

The current design code CECS 188:2005 does not account for the contribution of the steel tube to the bearing capacity of CFST composite columns. This is a conservative approach, but it is also uneconomical, because it does not utilise the full capacity of the composite section. The paper provides a rational basis for improving the design method, and it shows that the steel tube can contribute significantly to the bearing capacity, particularly for columns with a small eccentricity.

From my perspective, the code's approach is understandable from a historical perspective, because the design of CFST composite columns was originally based on the design of conventional reinforced concrete columns. However, the code has not kept pace with the research, and it is now outdated. The industry needs a design method that accounts for the steel tube and its confinement effect, and this paper provides such a method.

The Importance of the Confinement Effect

The confinement effect is a key factor in the performance of CFST composite columns, and it should not be neglected in the design. The paper shows that the confinement effect is stronger for columns with a small eccentricity, which means that the design method should account for the eccentricity when calculating the confinement factor.

In practice, the confinement effect is often neglected in the design, which leads to a conservative but uneconomical design. The paper's method provides a way to account for the confinement effect, and it can lead to more efficient designs.

Validation and Reliability

The proposed method was validated against 40 sets of test data, and the results show that it is accurate and reliable. However, the test data may not cover the full range of parameters that are encountered in practice, such as high-strength concrete, high-strength steel, and large-diameter columns. The method should be further validated with additional test data and with field measurements from real structures.

Study Insights and Implications

This paper is a valuable contribution to the field of CFST composite column design, and it provides a rational basis for improving the current design code. The findings on the failure modes, the confinement effect, and the bearing capacity calculation method are important for the design and the construction of CFST composite columns.

For the industry, the implications are clear:

  1. The design of CFST composite columns should account for the contribution of the steel tube and the confinement effect.
  2. The design method should be based on the actual stress-strain relationships of the components, rather than on simplified assumptions.
  3. The design should be validated with full-scale testing for critical applications.

The paper also raises important questions about the behaviour of CFST composite columns under other loading conditions, such as cyclic loading, seismic loading, and fire. These topics deserve further investigation.

Concluding Remarks

In summary, this paper addresses a significant deficiency in the current design code for CFST composite columns, and it proposes a new method for calculating the bearing capacity that accounts for the steel tube and its confinement effect. The method is based on the actual failure modes and the stress-strain relationships of the components, and it was validated against 40 sets of test data. The findings are directly applicable to the design and the construction of CFST composite columns, and they provide a rational basis for improving the current design code. As an industry, we should embrace these findings and incorporate them into our design and construction practices, while also recognising the need for further research on the behaviour of CFST composite columns under other loading conditions. The steel tube is not just a passive element; it is an active structural component that can significantly enhance the bearing capacity of the composite column.