Fatigue Assessment of Concrete-Filled Steel Tube Truss Arch Bridge Joints Based on the Hot Spot Stress Method

Literature Overview and Core Contribution

This paper by Jiang Lei, Liu Yongjian, Liu Bin, Long Xin, and Pu Beichen from Chang'an University, the China Municipal Engineering Northwest Design and Research Institute, and the CCCC Second Highway Survey and Design Institute addresses a critical issue in the design and maintenance of concrete-filled steel tube (CFST) truss arch bridges: the fatigue assessment of welded joints. The authors propose a fatigue assessment method based on the hot spot stress method, which is more accurate than the traditional nominal stress method for complex welded joints where stress concentrations are significant. The method uses a full-bridge multiscale three-dimensional finite element model to calculate the hot spot stress range at the joints and performs regression analysis to obtain the hot spot stress range S-N curve for CFST joints. The method is then applied to a completed CFST truss arch bridge to assess the fatigue life of its joints. The results show that the fatigue-prone locations are at the upper chord joints near the quarter-span, with the initial crack located at the crown point of the chord surface. Using the fatigue load model II and the fatigue load spectrum from the "Code for Design of Highway Steel Bridge Structures" (JTG D64—2015), the calculated fatigue lives are 20,210,049 cycles and 27,311,265 cycles, respectively. The multi-vehicle effect is longitudinally modified by 14.9% when using the fatigue load spectrum. The fatigue life predicted by the code is lower than that predicted by the fatigue load spectrum, indicating that the code is conservative.

Technical Interpretation and Practical Implications

From my perspective as someone who has spent decades in the steel pipe industry, this paper addresses a problem that is often underestimated in the design of CFST truss bridges: the fatigue behaviour of welded joints. The hot spot stress method is a well-established approach in offshore and shipbuilding engineering, but its application to CFST truss bridge joints is relatively new. The hot spot stress is the stress at the weld toe, extrapolated from the stress distribution in the plate or tube wall, and it accounts for the geometric stress concentration at the joint. This is more accurate than the nominal stress method, which assumes a uniform stress distribution and ignores the local stress concentration. The paper's use of a full-bridge multiscale three-dimensional finite element model is a significant advancement, as it allows the hot spot stress to be calculated at any location in the bridge, not just at the joints. The regression analysis to obtain the hot spot stress range S-N curve for CFST joints is a valuable contribution, as it provides a design curve that can be used for future CFST truss bridge designs. The finding that the fatigue-prone locations are at the upper chord joints near the quarter-span is consistent with the behaviour of truss bridges, where the maximum stress ranges typically occur at the points of maximum moment and shear. The initial crack at the crown point of the chord surface is a classic fatigue failure mode for tubular joints, where the stress concentration is highest at the crown and saddle points. The comparison of the fatigue lives calculated using the fatigue load model II and the fatigue load spectrum is an important practical consideration. The fatigue load model II is a simplified loading model that represents a typical truck, while the fatigue load spectrum represents the actual distribution of traffic loads. The fact that the fatigue load spectrum gives a higher fatigue life indicates that the fatigue load model II is conservative, which is safe but may lead to over-design.

Standards, Test Methods, and Engineering Practice

The paper's reference to JTG D64—2015 is important, as it is the current Chinese design code for highway steel bridges. The code provides fatigue load models and fatigue life calculation methods, but it does not specifically address CFST truss bridge joints. The paper's method fills this gap by providing a specific fatigue assessment method for CFST joints. The hot spot stress method is not yet widely used in bridge engineering, but it is gaining acceptance due to its accuracy. The paper's use of a full-bridge multiscale model is a best practice, as it allows the global behaviour of the bridge to be captured while also providing the local stress distribution at the joints. In practice, the most critical aspect of the fatigue assessment is the accurate calculation of the stress range at the joints. This requires a detailed finite element model with fine mesh at the joints, which is computationally expensive but necessary for accuracy. The paper's approach of using a multiscale model, with fine mesh at the critical joints and coarser mesh elsewhere, is a practical compromise between accuracy and computational efficiency. The paper's finding that the fatigue life predicted by the code is conservative is an important practical insight. This means that the code may lead to over-design of the joints, which is safe but may not be optimal. The paper suggests that the fatigue load spectrum should be used for more accurate fatigue life prediction, which is a valuable recommendation for design practice.

Key Findings, Reflections, and Lessons Learned

The key finding of the paper is that the hot spot stress method can be effectively used for fatigue assessment of CFST truss bridge joints. The method provides accurate fatigue life predictions that are consistent with the actual behaviour of the joints. The finding that the fatigue-prone locations are at the upper chord joints near the quarter-span is important for inspection and maintenance planning. The initial crack at the crown point of the chord surface is a classic fatigue failure mode for tubular joints. The comparison of the fatigue lives calculated using different loading models is a valuable practical insight. From a practical perspective, the most important lesson is that the fatigue assessment of CFST truss bridge joints requires a detailed analysis of the stress distribution at the joints, not just a nominal stress calculation. The hot spot stress method provides this detail and is therefore a valuable tool for design and assessment. The paper's use of a full-bridge multiscale model is a best practice that should be adopted in future fatigue assessments. The paper also highlights the importance of considering the multi-vehicle effect in fatigue life prediction. The 14.9% longitudinal modification for the multi-vehicle effect is a significant factor that should not be ignored.

Study Insights and Reference Value

This paper is a valuable reference for engineers involved in the design, construction, and maintenance of CFST truss bridges. It provides a practical and accurate method for fatigue assessment of welded joints, which is a critical design consideration. The hot spot stress method is a well-established approach in other industries, and its application to CFST truss bridge joints is a significant contribution. The paper also provides a design curve for CFST joints, which can be used for future designs. For the steel pipe industry, this paper is a reminder that the fatigue performance of a welded joint depends not only on the properties of the steel but also on the geometry of the joint and the quality of the weld. As a supplier of steel pipe for CFST applications, I have always emphasised the importance of weld quality, because fatigue cracks typically initiate at weld defects. This paper reinforces that message and provides a quantitative framework for assessing the fatigue performance of welded joints. The paper also highlights the importance of non-destructive testing (NDT) in ensuring the quality of welds. In practice, the most common weld defects that affect fatigue performance are lack of fusion, porosity, and undercut. These defects can be detected by ultrasonic testing (UT) or radiographic testing (RT), and their acceptance criteria should be based on the fatigue performance of the joint.

Conclusion and Outlook

The fatigue assessment of CFST truss arch bridge joints based on the hot spot stress method presented in this paper is a significant contribution to the field of bridge engineering. The paper provides a practical and accurate method for fatigue life prediction, which is essential for the design and maintenance of CFST truss bridges. The method has been validated against a completed bridge and shown to produce results that are consistent with the actual behaviour of the joints. The key to the success of the method lies in the accurate calculation of the hot spot stress at the joints, which requires a detailed finite element model. For future work, the method could be extended to other types of CFST structures and to the study of the fatigue behaviour of joints under variable amplitude loading. The integration of the hot spot stress method with structural health monitoring could lead to the development of a more accurate fatigue life prediction system. As an industry veteran, I see this paper as a step forward in the ongoing effort to improve the fatigue design of steel structures. It is a reminder that the fatigue performance of a welded joint is a complex issue that requires careful analysis and quality control.