Field Test on Deformation Characteristics of Existing Foundations Reinforced with Micro Steel Pipe Piles
1. Literature Overview and Research Background
This paper by Kong Gangqiang, Yu Jianghua, Ren Lianwei, Wang Wenming, Hu Da and Li Liuxi from Hohai University, Henan Polytechnic University, Shandong Jianzhu University, and Hunan City University, published in the Journal of Architecture and Civil Engineering in 2022, presents field test results on the deformation characteristics of existing foundations reinforced with micro steel pipe piles. The research was supported by the Fundamental Research Funds for Central Universities.
The study is based on a foundation reinforcement project at the boiler room of Henan Polytechnic University. The research optimises the construction sequence for micro steel pipe pile groups reinforcing existing foundations and validates a simplified beam model for analysing the existing foundation and column.
The study addresses a common challenge in foundation engineering: how to reinforce existing foundations without causing excessive deformation or damage to the existing structure. Micro steel pipe piles are increasingly used for this purpose due to their versatility, relatively low cost, and minimal disturbance to existing structures.
2. Core Technical Points and Findings
2.1 Research Methodology
The research methodology includes:
| Step | Description |
|---|---|
| 1 | Optimisation of construction sequence for micro steel pipe pile groups |
| 2 | Simplification of existing foundation and column as a beam model (fixed at one end, simply supported at the other) |
| 3 | Validation of the beam model |
| 4 | Field test of deformation characteristics during pile installation |
| 5 | Measurement of surface displacement and column angle changes |
| 6 | Comparison of different pile installation sequences |
2.2 Key Findings
The field test results reveal the following important findings:
| Finding | Significance |
|---|---|
| Combined clockwise-counterclockwise pile installation sequence is superior to single counterclockwise sequence | Reduces surface displacement by approximately 50% |
| Surface displacement from combined sequence is approximately 1/6 of column displacement | Indicates minimal disturbance to existing structure |
| Surface displacement from single counterclockwise sequence is approximately 1/4 of column displacement | Higher disturbance compared to combined sequence |
| Piles installed earlier provide a shielding and reinforcing effect on surrounding soil | Reduces disturbance from subsequent pile installation |
| Maximum displacement and stress occur during installation of the 3rd or 4th pile | Critical stage in construction sequence |
2.3 Analysis of Deformation Mechanism
The research provides insights into the mechanism of deformation during micro steel pipe pile installation:
- The installation of piles causes soil disturbance, which can lead to displacement of existing structures.
- Piles installed earlier create a shielding effect, reducing the disturbance caused by subsequent pile installation in the same direction.
- The combined clockwise-counterclockwise sequence reduces the cumulative effect of soil disturbance.
- The maximum displacement and stress occur during installation of the 3rd or 4th pile, indicating that this is the critical stage in the construction sequence.
3. Engineering Practice Integration
3.1 Manufacturing and Material Considerations
From a manufacturing perspective, micro steel pipe piles are typically manufactured from seamless or welded steel pipe with diameters ranging from 100mm to 300mm. The pipe must have sufficient strength and stiffness to withstand the installation forces and to provide the required load-bearing capacity.
In my experience with steel pipe manufacturing for foundation applications, the key quality requirements for micro steel pipe piles include:
| Quality Parameter | Requirement |
|---|---|
| Wall thickness | Uniform, within specified tolerance |
| Yield strength | As specified for the application |
| Weld quality | Full penetration, defect-free |
| Straightness | Within specified tolerance |
| Surface condition | Free from defects, suitable for corrosion protection |
3.2 Construction Practice Considerations
The finding that the combined clockwise-counterclockwise pile installation sequence is superior has direct implications for construction practice. This sequence should be specified in project plans to minimise disturbance to existing structures.
The identification of the 3rd or 4th pile as the critical stage is also valuable for construction management. Monitoring should be intensified during this stage, and contingency plans should be in place in case excessive displacement is detected.
3.3 Site Practice Considerations
On site, the following measures are recommended based on the research findings:
- Use combined clockwise-counterclockwise pile installation sequence.
- Monitor surface displacement and column deformation during pile installation.
- Intensify monitoring during installation of the 3rd and 4th piles.
- Implement contingency plans if excessive displacement is detected.
- Consider the shielding effect of previously installed piles when planning the installation sequence.
4. Key Questions and Reflections
Several questions arise from this research:
- How does the pile installation sequence affect the performance of the completed foundation system?
- What is the long-term behaviour of the reinforced foundation, including consolidation and creep effects?
- How do the findings apply to different soil conditions and different foundation types?
- What is the effect of pile spacing and configuration on the deformation characteristics?
5. Study Insights and Practical Implications
This research provides valuable insights into the construction of micro steel pipe pile groups for foundation reinforcement. The key takeaways for practising engineers are:
- The construction sequence significantly affects the deformation of existing structures during pile installation.
- Combined clockwise-counterclockwise installation is superior to single-direction installation.
- The critical stage in construction is during installation of the 3rd or 4th pile.
- Previously installed piles provide a shielding effect that reduces disturbance from subsequent installation.
6. Reference Value and Outlook
The research makes a significant contribution to the practice of foundation reinforcement using micro steel pipe piles. The field test data provides valuable information for construction planning and monitoring.
Future research should investigate the long-term behaviour of reinforced foundations and should extend the findings to different soil conditions and foundation types. The development of design guidelines for micro steel pipe pile reinforcement based on these findings would be particularly valuable for practising engineers.
The paper is an important reference for geotechnical engineers, foundation contractors, and construction managers involved in foundation reinforcement projects.
Zhuojin Pipe Fitting Co., Ltd