Fire Resistance of Square CFST Composite Special-Shaped Columns Protected by ALC Boards: A Practical Assessment
Literature Overview
The paper by Zhao Bingzhen, Chen Zhihua and colleagues addresses the fire resistance of square concrete-filled steel tube (CFST) composite special-shaped (SCFRT) columns protected by autoclaved lightweight aerated concrete (ALC) boards. The authors conducted fire resistance tests on a full-scale specimen, and they found that the ALC board protection can meet the fire resistance requirements for a first-grade fire resistance rating. The ALC board temperature lagged significantly behind the furnace temperature, demonstrating its excellent insulation properties. The authors also observed that the concrete infill in the steel tube provides a heat sink effect, and that the cavity between the limbs of the special-shaped column provides additional insulation. The test data provide a detailed temperature distribution across the cross-section, which can be used for finite element analysis.
Background and Motivation
The fire resistance of CFST columns is a well-studied topic, but the fire resistance of special-shaped CFST columns, such as the SCFRT column, is not. The SCFRT column is a composite column that consists of multiple square steel tubes connected by steel plates or stiffeners, forming a cross-shaped or L-shaped cross-section. This type of column is used in buildings where the column must be flush with the wall, to avoid the protrusion of a conventional circular or square column. The fire protection of these columns is a challenge because the geometry is complex, and the traditional fire protection methods, such as fire-resistant coatings or concrete encasement, are either not effective or not economical.
The use of ALC boards is an attractive option because they are lightweight, easy to install, and have excellent fire-resistant properties. ALC is a precast concrete product that is autoclaved to create a cellular structure with high porosity. The porosity provides excellent thermal insulation, which is why the temperature of the ALC board lags so far behind the furnace temperature. The boards can be cut to size and attached to the column using mechanical fasteners or adhesive.
Test Observations and Fire Behaviour
The test results show that the ALC board protection is effective in maintaining the temperature of the steel tube below the critical temperature for a significant period. The critical temperature for structural steel is typically around 500°C to 600°C, depending on the load level. The authors report that the steel tube temperature remained below this critical temperature for the duration of the test, which was designed to simulate a first-grade fire resistance rating of 3 hours. The temperature of the ALC board at the outer surface was close to the furnace temperature, but the temperature at the inner surface, adjacent to the steel tube, was much lower. This demonstrates the effectiveness of the ALC board as a thermal barrier.
The authors also observed that the concrete infill in the steel tube has a heat sink effect. The concrete absorbs heat from the steel tube, which slows down the temperature rise of the steel. This is a well-known benefit of CFST columns, and it is one of the reasons why they have better fire resistance than bare steel columns. The concrete also provides structural support to the steel tube, preventing local buckling at elevated temperatures.
The cavity between the limbs of the special-shaped column is another interesting observation. The cavity acts as an air gap, which provides additional insulation. The air in the cavity is stagnant, and it acts as a thermal barrier. This is a beneficial effect, but it also means that the temperature distribution across the cross-section is non-uniform, with the limbs that are exposed to the fire being hotter than the limbs that are shielded by the cavity.
Practical Fire Protection Engineering
From a practical standpoint, the use of ALC boards for fire protection of SCFRT columns is a viable solution, but it requires careful design and installation. The boards must be cut to the exact dimensions of the column, and the joints between the boards must be sealed to prevent the passage of hot gases. The fasteners must be corrosion-resistant and must be able to withstand the elevated temperatures. The installation must be done by trained personnel, because the boards are fragile and can be damaged during handling.
The design of the fire protection must also consider the load level of the column. A column with a high load level will have a lower critical temperature, and it will require more protection. The design should be based on the actual load level and the required fire resistance rating. The use of ALC boards is economical for most applications, but it may not be suitable for very high load levels or for very long fire resistance ratings.
Final Reflections
The paper by Zhao Bingzhen and colleagues is a valuable contribution to the field of fire protection of composite columns. It provides experimental evidence that ALC boards can be used effectively to protect SCFRT columns, and it provides detailed temperature data that can be used for design. For the steel pipe industry, this paper highlights the importance of considering fire resistance in the design of CFST columns. The steel tube is the primary load-bearing element, and its fire resistance is critical to the overall performance of the column. The use of ALC boards is a practical and economical solution, but it requires careful design and installation. The pipe industry should be aware of this solution and should be prepared to provide the steel tubes with the required properties for fire-resistant applications.