ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Simplified Creep Calculation Method for Axially Loaded CFST Members

1. What This Paper Is Really About

This is a Southwest Jiaotong University study on the long-term deformation (creep) of concrete-filled steel tube (CFST) members under axial compression. The paper proposes a simplified calculation method based on the age-adjusted effective modulus method and the step-by-step integration method, and compares it with traditional methods. The paper also investigates the effect of different concrete creep prediction models (CEB90 and EC2) and relative humidity values on the accuracy of the long-term deformation calculation.

Creep is a critical issue for CFST members, particularly in bridges and high-rise buildings, because the concrete core creeps under sustained load, causing a gradual transfer of load from the concrete to the steel tube. This load transfer increases the steel stress and decreases the concrete stress over time, and it can also cause additional deformation (deflection in beams, shortening in columns) that must be accounted for in the design.

2. Key Findings and Their Engineering Significance

2.1 The Simplified Method

The paper proposes a simplified method that combines the age-adjusted effective modulus method (AEMM) with the step-by-step integration method. The AEMM is a well-established approach for analysing creep in composite structures — it adjusts the elastic modulus of the concrete to account for the effect of aging and creep, and then uses a step-by-step integration to track the load transfer over time.

The proposed method is shown to be simple and accurate, and it can be used for the long-term deformation analysis of axially loaded CFST members. The comparison with traditional methods shows that the proposed method is more efficient and provides results that are in good agreement with test data.

2.2 Effect of Creep Models and Humidity

The paper investigates the effect of different creep prediction models on the accuracy of the long-term deformation calculation. The CEB90 model and the EC2 model, with a relative humidity range of 90-98%, are found to provide accurate results for CFST members. This is an important finding because the relative humidity inside a sealed steel tube is different from the ambient humidity — the concrete is in a sealed environment, so the humidity is likely to be high (90-98%) regardless of the external conditions.

The paper also compares the proposed method with existing test results, showing good agreement. This validates the method and the choice of creep model.

2.3 Practical Implications

The practical implication of this study is that designers can use the simplified method to calculate the long-term deformation of CFST members, rather than performing a complex finite element analysis or using a more elaborate creep model. The choice of the CEB90 or EC2 model, with a relative humidity of 90-98%, is appropriate for CFST members because of the sealed environment.

3. Practical Implications for Manufacturing and Construction

3.1 Concrete Mix Design

The creep behaviour of the concrete is influenced by the mix design. A lower water-cement ratio, a higher aggregate content, and the use of admixtures (such as superplasticizers) can reduce creep. For CFST members, the concrete is typically self-consolidating, which may have a higher paste content and therefore higher creep. The designer should be aware of this and use an appropriate creep model.

3.2 Steel-Concrete Interface

The load transfer between the steel tube and the concrete core is influenced by the bond at the interface. In a CFST member, the bond is typically good because the concrete shrinks and expands against the steel tube, but the bond can be affected by the surface condition of the steel (e.g., rust, oil, or paint). For a composite action to be fully developed, the steel tube should be clean and free of contaminants.

3.3 Long-Term Deformation in Service

The long-term deformation of a CFST member is not just a theoretical concern — it affects the serviceability of the structure. In a bridge, the creep-induced deflection can cause the deck to sag, which may require additional camber to be built into the structure. In a high-rise building, the creep-induced shortening of the columns can cause differential settlement between columns, which may affect the cladding and the internal partitions.

4. Lessons Learned and Recommendations

4.1 For Designers

Use the simplified method proposed in the paper for the long-term deformation analysis of axially loaded CFST members. Use the CEB90 or EC2 creep model with a relative humidity of 90-98%, which is appropriate for the sealed environment inside the steel tube. For more complex loading conditions (e.g., combined axial and bending), a more detailed analysis may be required.

4.2 For Fabricators

Ensure the steel tube is clean and free of contaminants before concrete filling. The bond between the steel and the concrete is important for the composite action, and any contamination can reduce the bond and affect the long-term behaviour.

4.3 For Site Engineers

Monitor the long-term deformation of CFST members in service. The creep-induced deformation can be significant, and it should be accounted for in the design of the structure. If the deformation exceeds the expected values, investigate the cause — it may be due to a higher-than-expected creep of the concrete, a lower-than-expected bond at the steel-concrete interface, or a different humidity condition than assumed.

5. Closing Thoughts

This is a well-executed study that provides a practical tool for the long-term deformation analysis of CFST members. The simplified method is simple and accurate, and the choice of the CEB90 or EC2 creep model with a high relative humidity is appropriate for the sealed environment. The key takeaway is that designers should not ignore creep in CFST members — it can cause significant long-term deformation and load transfer, and it should be accounted for in the design. The simplified method makes this analysis practical, and the paper provides clear guidance on the choice of creep model and humidity.