Concrete-Filled Steel Tube Members with Circumferential Voids under Combined Compression-Bending-Torsion Loading: Hysteretic Behavior and Design Implications

1. Literature Overview and Research Context

The paper by Liao Feiyu et al. (2019) from Fujian Agriculture and Forestry University and Chongqing University presents an experimental and numerical study on concrete-filled steel tube (CFST) members with circumferential voids under combined compression, bending, and torsion loading. The research addresses a critical issue that is often overlooked in both design and construction: the presence of voids or gaps between the steel tube and the core concrete.

The study involves 12 specimens, including 8 with circumferential voids, 2 without voids, and 2 hollow steel tube control specimens. The specimens were subjected to constant axial compression and cyclic bending-torsion coupling. The primary parameters were void ratio, bending-torsion ratio, and axial compression ratio.

2. Test Program and Key Findings

2.1 Specimen Configuration and Test Setup

The test specimens were designed to represent CFST members with circumferential voids at the interface between the steel tube and concrete core. This type of defect can occur due to concrete shrinkage, inadequate compaction, or construction errors. The void ratio was systematically varied to investigate its effect on structural performance.

Specimen Group Void Ratio Bending-Torsion Ratio Axial Compression Ratio
Group 1 (8 specimens) Varied (0-25%) Varied Varied
Group 2 (2 specimens) 0 (no void) Reference Reference
Group 3 (2 specimens) Hollow tube N/A N/A

2.2 Observed Failure Modes and Performance

The test results revealed that the presence of circumferential voids significantly alters the failure mode of CFST members. While sound CFST members typically exhibit ductile failure with concrete crushing and steel tube yielding, the voided specimens showed premature local buckling of the steel tube in the voided regions.

The voids also caused reductions in load-carrying capacity, stiffness, and energy dissipation capacity. The extent of degradation depended on the void ratio, with higher void ratios producing more severe performance reductions.

3. Technical Interpretation: The Mechanism of Void-Induced Degradation

3.1 Loss of Composite Action

The fundamental issue with circumferential voids is the loss of composite action between the steel tube and concrete core. In a sound CFST member, the steel tube provides confinement to the concrete, and the concrete provides internal support to the steel tube, preventing local buckling. When voids are present, this mutual support is lost in the voided regions.

3.2 Stress Redistribution and Local Effects

The presence of voids creates a non-uniform stress distribution around the cross-section. In the voided regions, the steel tube must resist the entire load without the support of the concrete core. This leads to:

3.3 Effect on Hysteretic Behavior

Under cyclic loading, the voids cause pinching in the hysteresis curves due to the loss of stiffness during load reversals. The energy dissipation capacity is reduced because the voided regions cannot contribute to plastic energy dissipation.

4. Engineering Practice and Lessons Learned

4.1 Root Causes of Voids in CFST Members

From my experience in the field, circumferential voids in CFST members are typically caused by one or more of the following factors:

Cause Description Detection Method
Concrete Shrinkage Drying shrinkage of the concrete core creates gaps at the interface Ultrasonic testing
Inadequate Compaction Insufficient vibration or improper placement leaves air pockets Impact-echo testing
Concrete Segregation Poor mix design or placement causes aggregate separation Radiographic testing
Temperature Effects Differential thermal expansion between steel and concrete Strain monitoring
Construction Errors Misalignment or improper concrete pumping Visual inspection after drilling

4.2 Detection and Quality Control

The detection of circumferential voids is a critical quality control issue. Standard methods include:

In my experience, ultrasonic testing is the most practical method for routine inspection of CFST members. However, the interpretation of UT results requires expertise because the steel-concrete interface is inherently complex.

4.3 Remediation and Repair

When voids are detected, the remediation approach depends on the extent and location of the defect:

The grouting procedure is critical. The grout must be injected under pressure to ensure complete filling of the void. The injection ports must be properly positioned to allow the grout to flow through the entire voided region.

5. Study Insights and Practical Recommendations

5.1 Design Implications

The study's finding that voids reduce capacity, stiffness, and energy dissipation has direct implications for design. Engineers should consider the possibility of voids in CFST members and account for their potential effects.

The practical recommendations include:

  1. Design for Void Tolerance: The design should account for a minimum void ratio that can be reliably detected and repaired.
  2. Enhanced Inspection: CFST members should be inspected for voids after concrete placement, using appropriate non-destructive testing methods.
  3. Construction Quality Control: The concrete placement procedure should be optimized to minimize the risk of void formation.
  4. Repair Provisions: The design should include provisions for void repair, including access ports and grouting systems.

5.2 Numerical Modeling and Future Research

The finite element model developed in this study provides a valuable tool for analyzing the effect of voids on CFST members. However, the model should be validated against a broader range of test data before being used for design purposes.

Future research should address:

5.3 Practical Application Guidance

For engineers working with CFST members, the key lesson from this study is that voids are not merely a cosmetic defect. They are a structural deficiency that can significantly compromise the performance of the member, particularly under seismic loading.

The following practical guidance is essential:

  1. Inspection Protocol: Establish a routine inspection protocol for CFST members, including ultrasonic testing after concrete placement and periodic re-inspection.
  2. Acceptance Criteria: Define clear acceptance criteria for void size and location. Voids exceeding the acceptance criteria should be repaired before the member is put into service.
  3. Repair Quality Control: The repair process should be subject to the same quality control as the original construction, including verification of grout filling and bond strength.

The research presented in this study is a valuable contribution to our understanding of the effect of voids on CFST members. It provides both experimental evidence and numerical tools for assessing the performance of voided members. For the practicing engineer, the key takeaway is that void prevention through proper construction practice is far more effective than void detection and repair after the fact.