ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Axial Compression Bearing Capacity of Steel Tube Coal Gangue Concrete

1. Literature Overview and Background

The paper by Zhao Weiping et al. (2024) addresses an important environmental and structural engineering challenge: the utilization of coal gangue as a coarse aggregate in concrete-filled steel tubes (CFST). Coal gangue is a byproduct of coal mining and washing, and its accumulation poses significant environmental hazards, including land degradation, water pollution, and air quality issues. The study explores the feasibility of using coal gangue as a replacement for natural coarse aggregate in CFST columns, which could provide a sustainable solution while also reducing construction costs.

The study conducted axial compression tests on steel tube coal gangue concrete specimens with a design concrete strength of C40. The key parameters investigated were the coal gangue replacement rate, loading method, and diameter-to-thickness ratio (D/t) of the steel tube. The findings are particularly relevant to regions with abundant coal gangue resources, such as Shanxi, Shaanxi, and Inner Mongolia in China, where disposal costs and environmental regulations are becoming increasingly stringent.

2. Technical Analysis of Failure Modes and Confinement

2.1 Failure Modes

The study identified two distinct failure modes depending on the loading method:

Loading Method Failure Mode Description
Method A Shear-type failure Diagonal shear cracks developed in the core concrete, with the steel tube exhibiting shear deformation.
Method B Barrel-shaped failure Local buckling of the steel tube occurred at mid-height, with the core concrete crushed in the central region.

The shear-type failure (Method A) occurred when the load was applied through the steel tube and the core concrete simultaneously, creating a more uniform stress distribution. The barrel-shaped failure (Method B) occurred when the load was applied primarily to the core concrete, allowing the steel tube to buckle outward.

2.2 Confinement Effect

The steel tube provided effective lateral confinement to the coal gangue concrete, significantly enhancing its compressive strength. The confinement mechanism is similar to that in conventional CFST columns, with the steel tube restraining the lateral expansion of the concrete core and inducing a triaxial stress state that increases the concrete's strength and ductility.

The study found that the confinement effect was more pronounced in Method B loading, where the core concrete compressive strength enhancement was more significant. This is because the steel tube was more effectively engaged in confining the concrete when the load was applied directly to the core.

2.3 Effect of Coal Gangue Replacement Rate

The coal gangue replacement rate was found to be the most significant factor affecting the ultimate bearing capacity. As the replacement rate increased, the ultimate bearing capacity decreased, reflecting the lower strength and stiffness of coal gangue concrete compared to natural aggregate concrete. However, the steel tube confinement effectively compensated for this strength reduction, allowing the steel tube coal gangue concrete to achieve acceptable performance.

3. Practical Considerations for Material Handling and Construction

3.1 Material Preparation and Quality Control

From a practical standpoint, the use of coal gangue as a coarse aggregate requires careful quality control. Coal gangue can vary significantly in composition and properties depending on the source and the degree of weathering. Key considerations include:

  1. Suitability assessment: Coal gangue must be tested for chemical stability, particularly for sulfate content, which can cause expansion and cracking in concrete.
  2. Crushing and grading: The coal gangue must be crushed to the appropriate size and graded to achieve a well-graded aggregate that minimizes voids and maximizes packing density.
  3. Moisture content: Coal gangue typically has a higher moisture content than natural aggregates, which must be accounted for in the mix design to maintain the correct water-cement ratio.

3.2 Steel Tube Fabrication and Welding

The steel tube must be fabricated to the required dimensions with proper welding quality. For CFST columns, the tube is typically manufactured using ERW or SAW processes. The weld quality is critical to ensure that the tube can withstand the hoop stresses induced by the concrete core expansion. In my experience, weld defects such as lack of fusion, porosity, or undercut can lead to premature failure of the tube and loss of confinement.

3.3 Concrete Placement and Curing

The placement of coal gangue concrete into the steel tube presents challenges due to the higher viscosity and lower workability of the mix. Proper vibration is essential to ensure complete filling and to avoid voids or honeycombing. The curing process must also be carefully controlled to prevent shrinkage cracking, which can reduce the bond between the concrete and the steel tube.

4. Engineering Practice and Lessons Learned

4.1 Environmental and Economic Benefits

The use of coal gangue as a coarse aggregate in CFST columns offers significant environmental and economic benefits. In regions where coal gangue is abundant, this approach can reduce the need for natural aggregate extraction, lower construction costs, and mitigate the environmental impact of coal gangue disposal. However, the material must be properly processed and tested to ensure consistent quality.

4.2 Design Implications

The study found that the ultimate bearing capacity of steel tube coal gangue concrete is primarily influenced by the coal gangue replacement rate. Designers must account for the reduced strength of coal gangue concrete when determining the required steel tube dimensions and wall thickness. The confinement provided by the steel tube is effective in compensating for the strength reduction, but the design must be based on the actual material properties, not on assumptions derived from natural aggregate concrete.

4.3 Practical Recommendations

Based on this study and my experience, I recommend the following practical measures:

  1. Conduct comprehensive material testing of coal gangue before use, including chemical composition, aggregate crushing value, and sulfate content.
  2. Use a coal gangue replacement rate of no more than 50% for structural applications, unless additional testing and validation are performed.
  3. Ensure proper concrete placement and vibration to avoid voids, which can significantly reduce the confinement effect.
  4. Consider the use of high-strength steel tubes to compensate for the reduced concrete strength and to maintain the required bearing capacity.

5. Conclusion

This study provides valuable insights into the axial compression behavior of steel tube coal gangue concrete, demonstrating that coal gangue can be effectively used as a coarse aggregate in CFST columns when properly processed and confined. The steel tube provides effective lateral confinement, compensating for the lower strength of coal gangue concrete and ensuring acceptable bearing capacity. The findings highlight the importance of controlling the coal gangue replacement rate and ensuring proper material quality and construction practices. For engineers and contractors, this approach offers a sustainable and cost-effective solution for utilizing coal gangue, but it requires careful material selection, quality control, and design consideration. The practical lessons from this study reinforce the need for a holistic approach that integrates material science, structural design, and construction management to achieve safe and sustainable outcomes.