Flexural Performance of Tapered High-Strength Hollow Sandwich Thin-Walled Steel Tube Concrete Members

1. Literature Overview and Test Program

The paper by Wang Xiantie et al. (2022) investigates the flexural performance of a novel structural member: a tapered high-strength hollow sandwich thin-walled steel tube concrete member. This member consists of an outer tapered steel tube, an inner steel tube, and a concrete core between them, with a hollow center. The use of high-strength materials (Q690D steel and C120 concrete) and thin-walled sections makes this member lightweight and efficient, but also introduces challenges related to local buckling and confinement.

The study conducted pure bending tests on 10 specimens in 5 groups, with the following parameters:

Parameter Range Investigated
Inner steel tube diameter-to-thickness ratio (D/t) 35 to 100
Outer steel tube diameter-to-thickness ratio (D/t) 50 to 120
Hollow ratio 0.72 to 0.85
Longitudinal stiffeners With and without

The test program was designed to evaluate the effects of these parameters on the flexural behavior, including failure modes, moment-deflection relationships, bearing capacity, stiffness, and strain development.

2. Technical Analysis of Flexural Behavior

2.1 Failure Modes and Deformation Characteristics

The study found that the specimens exhibited a ductile flexural failure mode. The outer steel tube in the tensile zone yielded first, followed by the concrete in the compressive zone, and finally the inner steel tube. The neutral axis shifted upward as the load increased, consistent with the plane section assumption.

The tapered geometry of the outer steel tube introduced additional complexity. The taper creates a varying cross-section along the member length, which affects the stress distribution and the location of the maximum moment. The study found that the tapered members exhibited a more gradual stiffness degradation compared to prismatic members, reflecting the gradual yielding of the outer tube along the taper.

2.2 Effects of Key Parameters

The study identified the following parametric effects:

Parameter Effect on Flexural Performance
Hollow ratio Increasing hollow ratio decreased the ultimate flexural capacity and stiffness.
Inner steel tube D/t Increasing inner steel tube D/t decreased the ultimate flexural capacity and stiffness.
Outer steel tube D/t Increasing outer steel tube D/t decreased the ultimate flexural capacity and stiffness.
Longitudinal stiffeners Adding stiffeners increased the ultimate flexural capacity by 7.29% to 20.18%.

The longitudinal stiffeners were particularly effective in enhancing the flexural capacity. The stiffeners delayed the local buckling of the outer steel tube, allowing the member to sustain higher loads before failure. The improvement was more significant for members with larger hollow ratios and thinner steel tubes, where local buckling was more critical.

2.3 Applicability of Existing Standards

The study evaluated the applicability of existing standards for calculating the flexural capacity and stiffness of the tapered high-strength hollow sandwich thin-walled steel tube concrete members. The key findings are summarized in the following table:

Standard Applicability for Capacity Applicability for Stiffness
T/CEC 185—2018 Conservative for members within the parameter limits; unsafe for members exceeding the limits. Accurate for hollow ratios less than 0.82.
EC 4 Unsafe for members exceeding the parameter limits. Accurate for hollow ratios less than 0.82.

The results indicate that the existing standards are not fully applicable to the tapered high-strength hollow sandwich thin-walled members, particularly for members with high hollow ratios and thin-walled sections. This highlights the need for further research and the development of specific design guidelines for these innovative members.

3. Standards Applicability and Practical Guidance

3.1 Design Implications

The findings of this study have significant implications for the design of tapered high-strength hollow sandwich thin-walled steel tube concrete members. Designers must carefully evaluate the applicability of existing standards and consider the specific parameters of the member, particularly the hollow ratio and the D/t ratios of the steel tubes.

Key design considerations include:

  1. Parameter limits: The study identified specific limits for the hollow ratio and D/t ratios beyond which the existing standards are not applicable. Designers should ensure that these limits are not exceeded.
  2. Longitudinal stiffeners: The use of longitudinal stiffeners is recommended for members with high hollow ratios and thin-walled sections to enhance the flexural capacity and prevent local buckling.
  3. High-strength materials: The use of Q690D steel and C120 concrete requires careful consideration of the material properties and the interaction between the steel and concrete.

3.2 Fabrication and Welding Challenges

The fabrication of tapered high-strength hollow sandwich thin-walled steel tube concrete members presents significant challenges:

  1. Tapered tube fabrication: The outer steel tube must be fabricated with a precise taper, which requires specialized rolling and welding processes. The weld quality is critical to ensure the structural integrity of the tube.
  2. Thin-walled sections: The thin-walled sections are more susceptible to local buckling and weld distortion. Careful welding procedures and distortion control measures are essential.
  3. High-strength steel welding: Q690D steel requires specific welding procedures to avoid hydrogen-induced cracking and to maintain the mechanical properties of the heat-affected zone.

3.3 Lessons from the Field

In my experience, the most critical issue with high-strength steel members is the welding quality. Q690D steel has a high carbon equivalent, which increases the risk of hydrogen-induced cracking. Preheating, interpass temperature control, and proper consumable selection are essential to avoid weld defects.

In one project, inadequate preheating led to hydrogen-induced cracking in the weld of a high-strength steel member, resulting in premature failure during testing. The lesson is clear: welding procedures for high-strength steel must be carefully developed and qualified, and the welds must be thoroughly inspected.

4. Conclusion

This study provides valuable insights into the flexural performance of tapered high-strength hollow sandwich thin-walled steel tube concrete members. The findings demonstrate that these members exhibit ductile flexural behavior, with the outer steel tube yielding first and the neutral axis shifting upward as the load increases. The hollow ratio and the D/t ratios of the steel tubes significantly affect the flexural capacity and stiffness, and the use of longitudinal stiffeners can enhance the capacity by 7.29% to 20.18%. The study also highlights the limitations of existing standards for these innovative members, particularly for members with high hollow ratios and thin-walled sections. For engineers involved in the design of lightweight and efficient structural members, the key takeaway is that the design must be based on a thorough understanding of the specific parameters and the applicability of existing standards. The fabrication and welding of these members require rigorous quality control, particularly for high-strength steel and thin-walled sections. The lessons from the field reinforce the importance of proper welding procedures, distortion control, and comprehensive inspection to ensure the structural integrity and performance of these innovative members.