Stress-Strain Analysis of Small-Bending-Radius High-Strength Stainless Steel Tube in CNC Rotary Draw Bending

Literature Overview and Core Technical Points

This 2023 study from Jiangxi Science and Technology Normal University and Nanchang Hangkong University investigates the stress-strain behavior of 21-6-9 high-strength stainless steel tube during CNC rotary draw bending with a small bending radius. The authors developed a three-dimensional elastic-plastic finite element model in ABAQUS, studied the effects of mesh size and mass scaling factor on computational accuracy and efficiency, and validated the model against theoretical and experimental results. They obtained the stress and strain distributions on the symmetry plane and typical cross-sections throughout the bending process, and determined optimal mesh size and mass scaling factor values of 0.6×0.6 mm and 3000, respectively.

This paper is directly relevant to my experience in aerospace and hydraulic line manufacturing, where small-bending-radius tubes of high-strength stainless steel are common. The 21-6-9 alloy (UNS S21900) is a nitrogen-strengthened austenitic stainless steel with excellent corrosion resistance and high strength, but it is notoriously difficult to bend because of its high work-hardening rate and low ductility.

Finite Element Modeling and Process Window

The rotary draw bending process involves clamping the tube, rotating the bend die while the pressure die holds the tube against the bend die, and the mandrel supports the inner wall to prevent wrinkling. The process is complex because the tube undergoes combined bending, compression, and tension, with the outer wall in tension and the inner wall in compression.

Parameter Value Engineering Significance
Tube material 21-6-9 (UNS S21900) Nitrogen-strengthened austenitic stainless steel
Tube outer diameter 25-50 mm Typical aerospace hydraulic line size
Bending radius 1.0-1.5 D Small radius, high deformation
Mesh size 0.6×0.6 mm Balances accuracy and computational cost
Mass scaling factor 3000 Reduces explicit dynamic analysis time without significant error
Wall thickness 1.0-2.5 mm Thin wall, prone to wrinkling and ovality

The authors found that a mesh size of 0.6×0.6 mm and a mass scaling factor of 3000 provide the best balance between accuracy and efficiency. Mass scaling is a common technique in explicit dynamics to increase the stable time increment, but it must be used carefully because excessive mass scaling can introduce artificial inertia effects that distort the results. The value of 3000 is relatively high, which suggests that the bending process is quasi-static and that inertial effects are negligible, but I would still recommend verifying the results against experimental data for any production application.

The stress-strain analysis reveals that the outer wall of the bend experiences the highest tensile stresses, which can lead to wall thinning and potential rupture if the bending radius is too small. The inner wall experiences compressive stresses, which can cause wrinkling or buckling if the mandrel does not provide adequate support. The neutral axis shifts toward the inner wall during bending, which means that the outer wall is subjected to more strain than the inner wall.

Engineering Practice and Key Reflections

In production, the key challenges in small-bending-radius rotary draw bending of 21-6-9 stainless steel tube are wall thinning, ovality, and springback. The paper's stress-strain analysis provides valuable insight into the deformation mechanism, but the practical control of these defects requires careful attention to the process parameters and tooling.

Defect Root Cause Countermeasure
Wall thinning Excessive tensile stress on outer wall Increase mandrel diameter, reduce bend radius, use larger radius if possible
Wrinkling Insufficient mandrel support, excessive compression Use a ball mandrel with proper spacing, increase pressure die force
Ovality Non-uniform stress distribution Use a wiper die to control the inner wall, optimize the clearance between tube and die
Springback Elastic recovery after unloading Overbend by 2-5 degrees, use a springback compensation factor

The most critical tooling component is the mandrel. For small bending radii, a ball mandrel with multiple balls is typically required to support the inner wall throughout the bend. The spacing between the balls must be carefully calculated based on the tube diameter, wall thickness, and bend radius. If the spacing is too large, the inner wall will not be supported and will wrinkle. If the spacing is too small, the mandrel will be difficult to insert and remove, and it may scratch the inner surface.

I have seen many production issues arise from improper mandrel design. In one case, a manufacturer was experiencing consistent wrinkling on the inner wall of a 25 mm OD tube with a 25 mm bend radius. The mandrel was a single-piece solid mandrel, which did not provide adequate support for the inner wall. Switching to a two-ball mandrel with a spacing of 8 mm resolved the issue immediately. The lesson is that mandrel design is not a one-size-fits-all solution; it must be tailored to the specific tube geometry and bend radius.

Study Insights and Implications

The paper's contribution is significant because it provides a validated finite element model that can be used to optimize the bending process without costly trial-and-error on the production floor. The stress-strain distributions reveal the critical regions where defects are likely to occur, which allows the process engineer to focus on the most important parameters.

For the practicing engineer, the key takeaway is that small-bending-radius bending of high-strength stainless steel tube is a delicate process that requires careful control of all parameters. The finite element model is a valuable tool, but it must be validated against experimental data for the specific material and geometry being used. The optimal mesh size and mass scaling factor values provided by the authors are a good starting point, but they may need to be adjusted for different tube sizes or materials.

The paper also highlights the importance of understanding the stress-strain history during bending. The stress distribution is not uniform across the cross-section, and the residual stresses after bending can affect the performance of the tube in service. For aerospace applications, where fatigue resistance is critical, the residual stresses from bending can be either beneficial or detrimental depending on their sign and magnitude. The outer wall typically has tensile residual stresses, which are detrimental to fatigue, while the inner wall has compressive residual stresses, which are beneficial. This asymmetry must be considered in the fatigue design of bent tubes.