Experimental Study on Interfacial Bond Performance of Concrete-Filled Steel Tube at Constant High Temperature: Study Notes
1. Literature Overview and Key Findings
This paper by Chen Jun, Xue Yuanyuan, Tan Qinghua and Wu Jinliang, published in China Civil Engineering Journal (2018, Vol. 51, No. 3), investigates the interfacial bond behaviour of concrete-filled steel tube (CFST) members under constant high temperatures. The authors conducted push-out slip tests on CFST specimens at temperatures ranging from 20°C to 900°C, with the main parameters being constant temperature, length-to-diameter ratio, and diameter-to-thickness ratio. The results show that temperature has a significant effect on the average bond strength, which first decreases, then increases, and then decreases again as the temperature rises, with a maximum reduction of up to 90%. The average bond strength decreases with increasing length-to-diameter ratio, with a maximum reduction of 50%, while the diameter-to-thickness ratio has a small effect, with a reduction of less than 10%.
2. Technical Interpretation and Material Behaviour at High Temperature
The bond between the steel tube and the concrete core is the foundation for their combined action. At high temperature, the steel expands more than the concrete, which can either increase or decrease the interfacial pressure depending on the temperature range. The non-monotonic behaviour observed — decrease, then increase, then decrease — reflects the competing effects of thermal expansion, steel strength degradation, and concrete spalling or cracking. At lower temperatures, the steel expands and may push against the concrete, increasing the bond. At higher temperatures, the steel loses strength and the concrete may degrade, leading to a loss of bond. The maximum reduction of 90% is alarming; it means that at some temperature, the bond is almost completely lost. This has serious implications for fire resistance design of CFST columns. The length-to-diameter ratio effect is also important: a longer column has a larger interface area, but the bond stress distribution is non-uniform, and the average bond strength decreases. This is consistent with the classic behaviour of bonded interfaces, where the bond stress is highest at the loaded end and decreases along the length.
| Parameter | Effect on Average Bond Strength |
|---|---|
| Temperature (20°C to 900°C) | Decrease → increase → decrease, max reduction 90% |
| Length-to-diameter ratio | Increases → decreases, max reduction 50% |
| Diameter-to-thickness ratio | Small effect, reduction < 10% |
3. Engineering Practice and Fire Safety Implications
In the steel pipe industry, we often supply tubes for CFST columns in buildings that must meet fire resistance requirements. The bond strength is critical for the transfer of load between the steel and concrete, especially at elevated temperatures. If the bond is lost, the steel tube may buckle independently, and the column may fail prematurely. The paper's finding that the bond strength can drop by 90% at high temperatures is a wake-up call. In practice, we need to ensure that the concrete is properly filled and that the interface is clean. Surface preparation of the tube interior is important, but at high temperatures, the bond is governed more by the thermal expansion mismatch and material degradation than by surface roughness. The length-to-diameter ratio effect means that for long columns, the bond is less effective, so additional mechanical connectors, such as shear studs or internal ribs, may be needed to ensure load transfer. This is a common practice in high-rise buildings, where CFST columns are used extensively.
4. Critical Assessment and Recommendations
The paper provides valuable experimental data, but the test specimens were small and the number of parameters was limited. The push-out test is a standard method for measuring bond strength, but it does not fully represent the actual stress state in a real column, where the load is applied axially and the bond stress distribution is more complex. The temperature range of 20°C to 900°C covers typical fire conditions, but the heating rate and the duration of exposure are not specified, which makes it difficult to compare with real fire scenarios. For design purposes, I would recommend using a conservative bond strength value, and for high fire resistance requirements, additional mechanical anchorage should be provided. The paper also does not discuss the effect of concrete type, such as high-strength concrete or lightweight concrete, which could have a significant influence on the bond behaviour. This is a gap that future research should address. Overall, the study is a useful contribution to the understanding of CFST behaviour at high temperature, but it should be supplemented with more realistic fire tests and numerical modelling.