Axial Compression Bearing Capacity of Double-Skin Concrete-Filled Steel Tubes Based on Unified Theory
1. Introduction: The Concept of Double-Skin CFST
The paper by Zhang Yufen et al. addresses a topic that is relatively new to many engineers: double-skin concrete-filled steel tubes (CFST). In a double-skin CFST, there are two steel tubes, an inner and an outer tube, with concrete filled between them. This creates a composite section with an inner void, which reduces the self-weight of the member while maintaining high bearing capacity.
The authors applied the unified theory of concrete-filled steel tubes to the calculation of the axial compression bearing capacity of double-skin CFST members. They proposed an equivalent confinement coefficient and derived formulas for the axial compression strength of both solid double-skin CFST and hollow double-skin CFST short columns.
2. The Unified Theory Approach
2.1 Background of the Unified Theory
The unified theory of CFST was developed by Professor Zhong Shantong and his colleagues. The theory treats the CFST member as a unified composite material with a single stress-strain relationship, rather than treating the steel tube and concrete core as separate materials. This approach simplifies the design calculation while maintaining accuracy.
The key parameter in the unified theory is the confinement coefficient, which represents the degree of confinement provided by the steel tube to the concrete core. The confinement coefficient depends on the steel ratio, the yield strength of the steel, and the compressive strength of the concrete.
2.2 Extension to Double-Skin CFST
The authors extended the unified theory to double-skin CFST by introducing an equivalent confinement coefficient. This coefficient accounts for the confinement provided by both the inner and outer steel tubes.
| Parameter | Single-Skin CFST | Double-Skin CFST |
|---|---|---|
| Steel tubes | One | Two (inner and outer) |
| Concrete | Solid core | Annular section |
| Confinement | Outer tube only | Inner and outer tubes |
| Equivalent confinement coefficient | Standard | Modified to account for both tubes |
2.3 Verification with Test Data
The authors compared their formula results with existing test data from the literature. The comparison showed good agreement, indicating that the unified theory can be used to calculate the axial compression bearing capacity of double-skin CFST members within certain ranges of steel ratio and hollow ratio.
3. Practical Implications for Pipe Manufacturing
3.1 Manufacturing Double-Skin CFST Members
The manufacturing of double-skin CFST members presents unique challenges for the pipe industry. The inner and outer tubes must be concentric, and the concrete must be placed in the annular space between them.
| Challenge | Practical Solution |
|---|---|
| Concentricity of inner and outer tubes | Use spacers or centering devices |
| Concrete placement in annular space | Use self-compacting concrete; pump from bottom |
| Inspection of concrete filling | Use ultrasonic testing; drill inspection holes |
| Connection of inner and outer tubes | Weld end plates or use structural connections |
3.2 Pipe Selection for Double-Skin CFST
The selection of pipe for double-skin CFST members requires careful consideration of the inner and outer tube dimensions. The outer tube provides the primary confinement, while the inner tube provides additional confinement and contributes to the axial load-carrying capacity.
| Outer Tube Diameter (mm) | Inner Tube Diameter (mm) | Wall Thickness (mm) | Typical Application |
|---|---|---|---|
| 219 | 89 | 6-8 | Columns with moderate load |
| 273 | 108 | 8-10 | Columns with high load |
| 325 | 140 | 10-12 | Large columns |
| 406 | 168 | 12-16 | Very large columns |
3.3 Welding Considerations
The welding of double-skin CFST members requires careful attention to the connections between the inner and outer tubes. The inner tube must be connected to the outer tube at the ends to ensure composite action. This connection is typically made by welding end plates or by using structural connections.
In my experience, the welding of the inner tube to the end plates is critical. The weld must be full penetration to ensure proper load transfer. The welding sequence must be controlled to minimise distortion of the inner tube.
4. Key Takeaways and Study Insights
The paper by Zhang Yufen et al. provides a theoretical method for calculating the axial compression bearing capacity of double-skin CFST members. The key findings are:
- The unified theory of CFST can be extended to double-skin CFST members by introducing an equivalent confinement coefficient.
- The equivalent confinement coefficient accounts for the confinement provided by both the inner and outer steel tubes.
- The formula results agree well with existing test data within certain ranges of steel ratio and hollow ratio.
- The method provides a new theoretical approach for the design of double-skin CFST members.
For those of us in the pipe industry, the practical implications are clear. Double-skin CFST members offer advantages in terms of reduced self-weight and high bearing capacity, but they require careful manufacturing and quality control. The concentricity of the inner and outer tubes, the quality of the concrete filling, and the welding of the connections are all critical factors.
The next time you receive an inquiry for pipe intended for double-skin CFST applications, remember that you are not just supplying two concentric tubes; you are supplying the components of a composite structural member whose performance depends on the interaction between the two tubes and the concrete between them. Pay attention to the details, and the member will perform as designed.
Zhuojin Pipe Fitting Co., Ltd