Seismic Mitigation of Semi-Floating System Concrete-Filled Steel Tube Arch Bridges Using Viscous Dampers
Bridge System and Seismic Concern
Peng Yihua, He Xuhui, Jing Haiquan and Yan Lei from Central South University have studied the use of viscous dampers to mitigate the seismic response of a semi-floating system concrete-filled steel tube (CFST) arch bridge. This is a topic that is directly relevant to the construction of long-span arch bridges, which are becoming more common in China and elsewhere. The semi-floating system is a popular choice for the main girder of a half-through CFST arch bridge because it allows the girder to move longitudinally during an earthquake, which reduces the seismic forces. However, this movement can be large, and it can cause damage to the expansion joints and the bearings. The viscous damper is a device that can control this movement by dissipating energy. The authors used a 252 m span half-through CFST arch bridge as a case study and performed nonlinear time-history analysis to study the effect of the damper parameters.
Damper Parameter Study and Results
The authors compared the seismic response of the bridge with and without viscous dampers. The key parameters of the damper are the damping coefficient and the velocity exponent. The authors studied the effect of these parameters on the seismic response of the main girder and the arch ribs. The following table summarises the key findings.
| Response Quantity | Without Damper | With Damper | Change |
|---|---|---|---|
| Main girder longitudinal displacement | Large | Significantly reduced | Significant reduction |
| Arch crown longitudinal displacement | Baseline | Increased | Increase |
| Arch rib axial force at key locations | Baseline | Varies by location | Mixed effect |
| Arch rib shear force at key locations | Baseline | Varies by location | Mixed effect |
| Arch rib bending moment at key locations | Baseline | Varies by location | Mixed effect |
| Local bending moment at damper location | Baseline | Significantly increased | Significant increase |
The most important finding is that the viscous damper significantly reduces the longitudinal displacement of the main girder, which is the primary purpose of the damper. However, this comes at a cost: the longitudinal displacement at the arch crown increases, and the internal forces at the key locations of the arch ribs are affected in different ways. The local bending moment at the damper location is significantly increased, which means that the connection between the damper and the arch rib must be designed to resist this additional moment.
Design Considerations and Detailing
The authors' study provides a method for selecting the damper parameters. The damping coefficient and the velocity exponent must be chosen to achieve the desired reduction in the main girder displacement without causing an unacceptable increase in the arch rib forces. This is a delicate balance. In my experience, the design of a viscous damper for a bridge is not just a matter of selecting a device from a catalogue. It requires a detailed analysis of the bridge's dynamic behaviour and a careful study of the damper's effect on the structure. The connection between the damper and the arch rib is a critical detail. The damper must be connected to the structure in a way that allows it to transmit the damping force without causing a local failure. The authors found that the local bending moment at the damper location is significantly increased, which means that the connection must be stiffened and the local stresses must be checked.
Lessons for Bridge Construction and Maintenance
From a construction perspective, the installation of viscous dampers on a CFST arch bridge requires careful planning. The dampers are typically installed after the main girder is erected and before the bridge is opened to traffic. The alignment of the damper is critical, and the connection must be made with high-quality welds or bolted connections. In my experience, the most common problem with viscous dampers is leakage. The damper is a hydraulic device, and the seals can fail over time. This is why the maintenance plan must include regular inspection of the dampers and the connections. The authors' study does not cover the long-term performance of the dampers, but this is a practical concern that must be addressed in the design.
Summary and Reflections
This paper is a valuable contribution to the seismic design of CFST arch bridges. The authors have shown that viscous dampers can effectively reduce the longitudinal displacement of the main girder in a semi-floating system, but they have also shown that this comes with a cost: the arch rib forces are affected, and the local bending moment at the damper location is increased. The design of the damper parameters and the connection details is a delicate balance that requires a detailed analysis. For the practising engineer, the lesson is clear: viscous dampers are a useful tool, but they are not a simple solution. They must be designed and detailed with care, and the long-term maintenance must be planned. I have seen bridges with viscous dampers that worked perfectly, and I have seen bridges where the dampers leaked and became ineffective. The difference is in the design, the installation, and the maintenance. This paper gives us the tools to get the design right, and I recommend it to anyone who is involved in the design or construction of a CFST arch bridge.