Seismic Performance of High-Strength Concrete Columns with Concrete-Filled Steel Tube Cores: Lessons from 38 Specimens

This paper by Zhao Guofan and colleagues at Dalian University of Technology is a classic from 1996, but it remains highly relevant today. The authors tested 38 high-strength concrete columns, each with a concrete-filled steel tube (CFST) core, under axial compression and cyclic lateral loading. The goal was to evaluate the seismic performance of these columns and to recommend design parameters for the minimum volumetric stirrup ratio, the minimum steel tube area ratio, and the maximum axial compression ratio. This is a topic that I have dealt with directly in the supply of steel tubes for high-rise buildings in seismic zones.

The Test Program and Failure Modes

The 38 specimens were designed to investigate the effects of several parameters: the axial compression ratio, the volumetric stirrup ratio, the steel tube area ratio, and the concrete strength. The columns had a square cross-section with a CFST core in the center. The steel tube was a small-diameter seamless or ERW tube, typically 60 mm to 100 mm in diameter, filled with high-strength concrete. The outer concrete was high-strength concrete reinforced with longitudinal bars and transverse stirrups.

The failure modes observed were typical of high-strength concrete columns: the outer concrete spalled, the longitudinal bars buckled, and the stirrups yielded. However, the CFST core remained intact and continued to carry load even after the outer concrete had spalled. This is the key benefit of the CFST core—it provides a ductile load path that prevents the column from failing in a brittle manner.

The authors found that the CFST core significantly improved the ductility of the column. The displacement ductility ratio, which is the ratio of the ultimate displacement to the yield displacement, was increased by 20% to 40% compared to a conventional high-strength concrete column without a CFST core. This is a substantial improvement and is critical for seismic design.

Key Design Parameters

The authors proposed three design parameters. The first is the minimum volumetric stirrup ratio. This is the ratio of the volume of transverse stirrups to the volume of the concrete core. The authors recommended a minimum value of 0.8% for high-strength concrete columns with a CFST core. This is lower than the minimum required for conventional high-strength concrete columns, which is typically 1.2% to 1.5%. The CFST core provides additional confinement, so the stirrups can be reduced.

The second parameter is the minimum steel tube area ratio. This is the ratio of the cross-sectional area of the steel tube to the total cross-sectional area of the column. The authors recommended a minimum value of 1.5%. This ensures that the CFST core can carry a sufficient portion of the axial load even if the outer concrete is damaged.

The third parameter is the maximum axial compression ratio. This is the ratio of the axial load to the axial capacity of the column. The authors recommended a maximum value of 0.75 for high-strength concrete columns with a CFST core. This is higher than the typical limit of 0.65 for conventional high-strength concrete columns, which means that the CFST core allows the column to carry a higher axial load without sacrificing ductility.

Manufacturing and Quality Control Implications

From a manufacturing perspective, the CFST core is a small-diameter steel tube filled with high-strength concrete. The tube is typically seamless or ERW, with a wall thickness of 3 mm to 6 mm. The tube is fabricated, filled with concrete, and then placed in the column formwork. The outer concrete is then cast around the CFST core.

The critical quality issue is the bond between the steel tube and the outer concrete. If the bond is poor, the outer concrete can separate from the CFST core, and the column will behave as two independent components. The authors found that the bond was adequate in their tests, but this was under laboratory conditions. On site, the bond can be compromised by the use of release agents, by dust or debris on the tube surface, or by poor concrete placement.

Another quality issue is the welding of the steel tube. The tube must be welded with a full-penetration weld if it is used as a load-bearing element. I have seen CFST cores that were fabricated with a simple tack weld at the end, which failed during the concrete filling. The tube must also be filled with concrete completely, without voids. This requires a careful filling procedure, with vibration or the use of self-consolidating concrete.

My Takeaway

This paper is a landmark study that demonstrates the benefits of a CFST core in high-strength concrete columns. The practical lesson is that a CFST core can replace a significant amount of transverse reinforcement, allowing for a more economical column design. The recommended parameters—a minimum stirrup ratio of 0.8%, a minimum steel tube area ratio of 1.5%, and a maximum axial compression ratio of 0.75—are reasonable and have been incorporated into many design codes. From a supply chain perspective, the CFST core is a relatively simple product to fabricate, but the quality control must be rigorous. The bond between the tube and the outer concrete is critical, and the tube must be clean and free of defects. I have seen columns with CFST cores perform well in seismic events, and I have also seen columns where the bond was compromised and the outer concrete spalled prematurely. The difference is in the quality of the fabrication and the concrete placement.