Mechanical Properties of Buried Continuous Steel Pipe Under Reverse Fault Displacement
Literature Overview and Core Problem
This paper by Zhao Xu, Cui Jianyang, Zhong Zilan and Du Xiuli, published in Journal of Beijing University of Technology (2022, Vol. 48, No. 7, pp. 729-738), investigates the mechanical properties of buried continuous steel pipe under reverse fault displacement. The authors use finite element software to establish a three-dimensional nonlinear pipe-soil interaction numerical model, analyse the influence mechanism of reverse fault displacement on the buried steel pipe, and identify three typical failure modes: tensile failure, local buckling and excessive cross-section deformation. The paper also determines the critical reverse fault displacement for each failure mode under different fault dip angles, internal pressures and diameter-to-thickness ratios.
This paper is directly relevant to the design of buried steel pipelines that cross active faults. I have supplied line pipe for pipelines that cross fault zones, and the design of these crossings is one of the most challenging aspects of pipeline engineering. The pipeline must be able to accommodate the fault displacement without rupturing, which requires a combination of proper material selection, appropriate wall thickness and careful route design.
The paper's key findings are:
- When the reverse fault dip angle is 75°, the fault displacement required to cause local buckling is the smallest, making this the most unfavourable dip angle for local buckling.
- Larger internal pressure effectively suppresses excessive cross-section deformation, and as the internal pressure increases, the controlling failure mode changes from local buckling to tensile failure.
- Increasing the diameter-to-thickness ratio significantly improves the deformation capacity of the pipe.
Technical Points and Numerical Model Analysis
The paper's numerical model is well constructed and the parametric study is comprehensive. Let me break down the key technical points.
Numerical Model
The authors use a three-dimensional nonlinear finite element model that includes the pipe, the soil and the interface between them. The pipe is modelled using shell elements, the soil is modelled using solid elements, and the pipe-soil interaction is modelled using contact elements that allow for separation and sliding. The model is validated against experimental data from the literature, which gives confidence in the results.
The model incorporates the following key parameters:
| Parameter | Range Studied | Significance |
|---|---|---|
| Fault dip angle | 60°, 75°, 90° | Determines the direction and magnitude of the fault displacement applied to the pipe |
| Internal pressure | Varied | Affects the stress state and the failure mode |
| Diameter-to-thickness ratio (D/t) | Varied | Affects the local buckling resistance and the deformation capacity |
Failure Modes
The paper identifies three typical failure modes:
- Tensile failure. This occurs when the axial strain in the pipe exceeds the tensile strain capacity of the pipe material. The pipe ruptures at the location of maximum axial strain, which is typically at the point where the pipe crosses the fault.
- Local buckling. This occurs when the compressive strain in the pipe wall exceeds the critical buckling strain. The pipe wall buckles locally, forming a wrinkle or a fold. This is a common failure mode for pipes in compression, and it can occur at the point where the pipe is compressed by the fault displacement.
- Excessive cross-section deformation. This occurs when the cross-section of the pipe is deformed beyond an acceptable limit. This is not a rupture, but a significant ovalisation or flattening of the pipe cross-section, which can reduce the flow capacity or prevent the passage of pigs.
The paper's finding that the failure mode depends on the internal pressure and the D/t ratio is important. At low internal pressure, local buckling is the controlling failure mode. At high internal pressure, the pipe is more resistant to buckling, and tensile failure becomes the controlling mode. This is because the internal pressure creates a hoop stress that stiffens the pipe wall against buckling.
Critical Fault Displacement
The paper determines the critical fault displacement for each failure mode. The critical fault displacement is the amount of fault movement that causes the pipe to reach the limit state for a given failure mode. This is a key parameter for design, because the designer needs to know how much fault displacement the pipe can accommodate.
The paper's finding that the 75° fault dip angle is the most unfavourable for local buckling is significant. This means that a pipeline crossing a reverse fault with a dip angle of 75° is more vulnerable to local buckling than a pipeline crossing a fault with a dip angle of 60° or 90°. The designer should pay particular attention to this case.
Integration with Engineering Practice
This paper has direct practical applications in the design of buried pipelines crossing active faults.
- Route selection. The paper's finding that the fault dip angle affects the critical fault displacement is important for route selection. When a pipeline must cross an active fault, the route should be chosen to minimise the vulnerability of the pipe. If the fault dip angle is 75°, the pipe is more vulnerable to local buckling, and the designer should consider measures to mitigate this, such as increasing the wall thickness or using a higher strength material.
- Wall thickness selection. The paper's finding that the D/t ratio affects the deformation capacity is important for wall thickness selection. A lower D/t ratio (thicker wall) improves the local buckling resistance but may not improve the tensile capacity. The designer must balance the requirements for buckling
Zhuojin Pipe Fitting Co., Ltd