Development and Manufacture of Large-Diameter Thick-Wall TP347H Stainless Steel Pipe
Literature Overview
This paper by Yin Renjie, Wang Ena, Bian Huachuan, Li Xu and Zhang Tao, published in Steel Pipe (2009, Vol. 38, No. 6, pp. 34-37), documents the successful development of a Φ355.6 mm × 42.8 mm large-diameter thick-wall TP347H stainless steel pipe by Panzhihua Iron and Steel Group Chengdu Steel Vanadium Co., Ltd. The manufacturing route is a combination of centrifugal casting for the hollow billet followed by Pilger rolling for hot forming. The resulting pipe meets all requirements of ASME A312 and shows uniform longitudinal and transverse properties.
TP347H is a niobium-stabilised austenitic stainless steel with a carbon content of 0.04-0.10%, designed for high-temperature service. It is widely used in power plant boilers, heat exchangers and petrochemical furnaces where temperatures can reach 600-800°C. The grade is particularly sensitive to sensitisation, and the stabilisation with niobium is intended to prevent chromium carbide precipitation at grain boundaries.
Manufacturing Route Analysis
The traditional route for large-diameter thick-wall stainless steel pipe is either extrusion or forging followed by machining. Both are expensive and have limitations. Extrusion requires large presses and is not economical for small batch sizes. Forging followed by machining has poor material utilisation and leaves the pipe with a machined surface that may not have the same properties as a hot-formed surface.
The centrifugal casting plus Pilger rolling route offers an alternative that combines the advantages of both processes. Centrifugal casting produces a hollow billet with a fine, uniform microstructure and good density. The Pilger mill then reduces the wall thickness and diameter while imparting the necessary deformation to refine the grain structure and improve mechanical properties.
| Process Step | Key Parameters | Typical Issues |
|---|---|---|
| Centrifugal casting | Mould rotation speed, pouring temperature, cooling rate | Segregation, porosity, non-metallic inclusions |
| Billet preparation | Machining of inner and outer surfaces, defect removal | Surface cracks, inclusions |
| Pilger rolling | Roll pass design, feed rate, reduction ratio, temperature | Wall thickness variation, surface defects, grain growth |
| Heat treatment | Solution annealing temperature, holding time, quench rate | Sensitisation, grain coarsening, distortion |
| Finishing | Straightening, cutting, end preparation, NDT | Residual stress, surface finish |
The paper reports that the centrifugal casting billet has a homogeneous structure and that the Pilger rolling process imparts sufficient deformation to achieve the required mechanical properties. The final pipe shows uniform longitudinal and transverse properties, which is a key requirement for high-temperature service where the pipe may be subjected to biaxial stress states.
Technical Points and Property Evaluation
The key technical challenge in manufacturing TP347H pipe is controlling the grain size and preventing sensitisation. TP347H is a high-carbon grade, and if the solution annealing temperature is too low or the cooling rate is too slow, chromium carbides can precipitate at grain boundaries, leading to intergranular corrosion and reduced creep strength.
| Property | ASME A312 Requirement | Reported Result |
|---|---|---|
| Tensile strength, MPa | ≥515 | Meets requirement |
| Yield strength, MPa | ≥205 | Meets requirement |
| Elongation, % | ≥35 | Meets requirement |
| Hardness, HRB | ≤90 | Meets requirement |
| Grain size | ASTM No. 7 or finer | Meets requirement |
| Intergranular corrosion | Pass per ASTM A262 Practice E | Pass |
The paper does not provide detailed property data, but the statement that all technical indicators meet ASME A312 requirements and that the pipe shows uniform longitudinal and transverse properties is a strong indication of a successful development.
Integration with Engineering Practice
I have seen TP347H pipe used in supercritical boiler superheaters and reheaters, and I have also seen it fail. The most common failure mode in service is creep rupture, which is often associated with grain coarsening or with excessive cold work during forming. The pipe in this paper is manufactured by hot forming, which avoids the cold work issue, but the Pilger rolling process can introduce residual stresses that need to be relieved by heat treatment.
The centrifugal casting route has one advantage that is often overlooked: it produces a pipe with a very clean inner surface. In boiler applications, the inner surface is exposed to steam, and any surface defects can become initiation sites for oxide scale spalling or for corrosion. The centrifugal casting process produces a smooth inner surface that requires minimal machining, which reduces the risk of surface damage.
However, centrifugal casting has a limitation: it produces a pipe with a columnar grain structure in the as-cast condition. This structure must be broken down by hot working. The Pilger mill provides the necessary deformation, but the reduction ratio must be sufficient to achieve full recrystallisation. If the reduction is insufficient, the pipe will retain a banded or columnar structure that has poor transverse properties.
The paper does not provide details on the reduction ratio used, but the statement that the pipe has uniform longitudinal and transverse properties suggests that the reduction was adequate. This is a critical point for the manufacturing team to verify on every heat.
Key Questions and Reflections
One question that the paper does not address is the economics of the centrifugal casting plus Pilger rolling route compared to extrusion. The paper mentions that the route combines the advantages of both processes, but it does not provide a cost comparison. In my experience, centrifugal casting is competitive for small batch sizes and for large diameters where extrusion presses are not available. For large production runs, extrusion may be more economical.
Another question is the weldability of the pipe. TP347H is designed for high-temperature service, and the pipe may need to be welded in the field. The niobium stabilisation helps prevent sensitisation, but the weld heat-affected zone can still be susceptible to cracking if the welding procedure is not properly qualified. The paper does not address this, but it is a critical issue for the end user.
The paper also does not discuss the inspection requirements for the pipe. ASME A312 requires ultrasonic testing or eddy current testing for seamless pipe, and the paper does not state which method was used. For thick-wall pipe, ultrasonic testing is the preferred method, and the acceptance criteria should be agreed with the purchaser.
Study Insights and Implications
This paper is a valuable contribution to the field of stainless steel pipe manufacturing. It demonstrates that the centrifugal casting plus Pilger rolling route is a viable alternative to extrusion for large-diameter thick-wall TP347H pipe. The successful development of this pipe has positive implications for the domestic supply of large-diameter thick-wall stainless steel pipe, which is critical for power plant and petrochemical applications.
For the manufacturing team, the key lesson is that the process must be controlled carefully at every step. The centrifugal casting parameters must be optimised to avoid segregation and porosity, and the Pilger rolling parameters must be set to achieve the required reduction and grain refinement. The heat treatment must be designed to ensure full solution annealing and rapid quenching to avoid sensitisation.
For the end user, the pipe should be inspected to the full requirements of ASME A312, including ultrasonic testing, mechanical property testing and intergranular corrosion testing. The pipe should also be checked for dimensional accuracy, particularly wall thickness variation, which is a common issue in Pilger rolled pipe.
The development of this pipe is a good example of how process innovation can expand the range of products that can be manufactured domestically. It is also a reminder that new manufacturing routes must be validated by thorough testing and that the results must be documented for future reference. The paper provides a useful starting point, but the industry needs more data on the long-term performance of this pipe in service, particularly its creep strength and its resistance to high-temperature corrosion. This is the kind of development that deserves to be followed up with more research and with field trials in actual power plant service. The domestic industry should take pride in this achievement, but it should also continue to refine the process and to build the database of experience that is needed for confident design and specification.
Zhuojin Pipe Fitting Co., Ltd