ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Temperature Field of Concrete-Filled Steel Tube Members Under Solar Radiation: A Practical Perspective

1. Literature Overview and Core Findings

The paper by Chen Baochun and Liu Zhenyu from Fuzhou University addresses a topic that is often overlooked in design: the temperature field in concrete-filled steel tube (CFST) members due to solar radiation. This is a critical issue for bridges and other outdoor structures, where the daily temperature cycle can induce significant thermal stresses. The authors conducted field tests on CFST members under natural sunlight, measuring the temperature distribution across the cross-section. The results show that the temperature field is non-uniform, with the temperature at the center point being more influenced by the east-west direction (solar radiation direction). The temperature change at points closer to the center lags behind the ambient air temperature. The paper also found that horizontal members experience larger temperature variations than vertical members, and that the temperature difference across the section can be represented by a cubic polynomial.

2. Technical Interpretation and Thermal Behavior

2.1 Non-Uniform Temperature Distribution

The finding that the temperature field is non-uniform is the most important result. In design, we often assume a uniform temperature change for simplicity. This paper shows that this assumption is not valid for CFST members exposed to sunlight. The solar radiation heats the surface of the steel tube, but the heat transfer to the concrete core is slow due to the low thermal conductivity of concrete. This creates a temperature gradient across the section. The surface of the steel tube can be much hotter than the concrete core. This differential temperature causes thermal stresses, which can lead to cracking of the concrete or yielding of the steel tube.

Location Temperature Behavior Practical Implication
Center point More influenced by east-west solar direction The center temperature follows the sun's path, not just the ambient air.
Radial points Temperature change lags behind ambient air The lag increases closer to the center.
Horizontal members Larger temperature variation than vertical members Horizontal members receive more direct solar radiation.
Sun-facing side Large temperature change This side heats up rapidly during the day.
Shaded side Small temperature change This side is protected from direct radiation.

2.2 The Cubic Polynomial Model

The paper proposes that the radial temperature distribution can be represented by a cubic polynomial. This is a practical finding because it allows engineers to calculate the temperature gradient and the resulting thermal stresses without a complex finite element analysis. The cubic polynomial is a good fit for the measured data, but the coefficients must be determined for the specific conditions. The paper found that for vertical members, the maximum temperature difference in the morning is similar to the maximum temperature difference in the afternoon. This suggests a symmetric thermal behavior, which is useful for design.

3. Engineering Practice and Lessons Learned

3.1 Thermal Stresses in Bridge Structures

For a bridge engineer, this paper is a wake-up call. The temperature gradient in a CFST member can cause significant stresses, especially in a bridge deck where the members are exposed to direct sunlight. I have seen cases where CFST arch bridges have developed cracks in the concrete due to thermal gradients. The cracks are not necessarily structural, but they can lead to corrosion of the steel tube and reduce the service life of the structure. The paper provides the data needed to calculate these gradients and to design for them.

3.2 The Difference Between Horizontal and Vertical Members

The finding that horizontal members have larger temperature variations than vertical members is intuitive but important. A horizontal member, such as a bridge girder, receives direct solar radiation on its top surface for most of the day. A vertical member, such as a column, receives radiation on its east face in the morning and its west face in the afternoon. The horizontal member has a more continuous and intense heat input, leading to a larger temperature gradient. This means that horizontal members are more susceptible to thermal stress damage.

4. Study Insights and Reflection

This paper is a good example of the importance of field testing. The authors did not just rely on theoretical models; they went out and measured the actual temperature distribution in CFST members under real sunlight. This is the kind of data that is essential for validating design assumptions. The results show that the temperature field is complex and non-uniform, and that simple uniform temperature assumptions can be significantly in error.

For those of us in the steel pipe industry, this paper highlights the importance of understanding the thermal properties of the composite section. The steel tube has a high thermal conductivity, while the concrete core has a low thermal conductivity. This mismatch creates the temperature gradient. The gradient is not just a design issue; it can also affect the bond between the steel and concrete. If the steel tube expands more than the concrete, it can separate from the concrete, reducing the composite action. This is a long-term durability concern.

The cubic polynomial model is a useful tool, but it is based on a specific set of conditions. The coefficients may need to be adjusted for different geographic locations, seasons, or surface finishes. A dark-painted steel tube will absorb more solar radiation than a light-painted one, leading to a larger temperature gradient. This is a detail that is often overlooked in design, but it can have a significant impact on the thermal behavior.

In conclusion, this paper provides valuable data on the temperature field of CFST members under solar radiation. It shows that the temperature distribution is non-uniform and that the gradient can be significant. This information is essential for designing CFST structures that are durable and safe. The key lesson is that we cannot ignore thermal effects in outdoor structures. We must design for the actual temperature gradients, not just the average temperature.