ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Seismic Response of Exposed Steel Penstocks in Hydropower Stations: A Practical Review

Literature Overview and Context

This paper by Liu Yuan, Shi Changzheng, Wu Hegao and Cheng Zhenglong addresses a question I have seen cause real trouble on site: what actually happens to an exposed steel penstock when the ground starts shaking. The authors use finite element time-history analysis on a surface steel penstock of a hydropower station, considering two load cases: normal operation with water inside the pipe, and the pipe drained and empty during an earthquake. The work was supported by the China Postdoctoral Science Foundation and published in Water Resources and Power in 2014. For those of us who have walked penstocks, anchored them, welded the supports and then watched the concrete cure, this is not an academic curiosity. It is a safety question.

The paper reports that in the normal operation case, the penstock mainly develops large transverse acceleration and displacement. In the drained case, because there is no internal water mass and because of the vertical restraint arrangement, the pipe not only moves transversely but also develops significant vertical acceleration and displacement, causing the pipe to lift off its sliding supports and jump upward. The conclusion is blunt: earthquake-induced transverse sliding and vertical jumping of the steel pipe will adversely affect safe and stable operation, and both transverse and vertical restraint measures should be adopted.

Interpretation of Technical Points

Let me unpack what this means in the language of the plant floor. A surface penstock is not buried; it sits on saddle supports or ring girders, often with sliding bearings to accommodate thermal expansion. The design philosophy is usually to let the pipe move axially for temperature, but to restrain it transversely. What this paper shows is that in a seismic event, that transverse restraint may not be enough, and the vertical restraint may be insufficient to prevent liftoff.

The key parameters are the acceleration and displacement response. The authors performed time-history analysis, which is the correct approach because a response spectrum analysis would miss the phase relationships that cause the pipe to jump. The important practical finding is that the vertical response is not simply a scaled version of the horizontal response. When the pipe is empty, the vertical stiffness of the support system is often much lower than the transverse stiffness, so the pipe can lift off.

I have seen this exact phenomenon in a different context: a large-diameter surface pipe in a pumping station that had inadequate hold-down clamps. During a moderate seismic event, the pipe lifted and shifted, damaging the sliding bearing and causing a leak at a flanged joint. The repair cost was significant, and the root cause was the same as described in this paper.

Practical Implications for Design and Construction

The recommendation to adopt both transverse and vertical restraint measures is sound, but the implementation details matter. In my experience, the following points are critical:

  1. The vertical restraint should be designed to resist the uplift force, not just the gravity load. The uplift force can be several times the dead weight of the pipe in a strong earthquake.
  2. The transverse restraint should be stiff enough to limit the transverse displacement to a value that the expansion joint or the pipe bending can accommodate.
  3. The connection between the restraint and the pipe must not introduce stress concentrations that could cause fatigue or fracture.

I have seen designs where the restraint was a simple U-bolt around the pipe, which is fine for a small pipe but inadequate for a large-diameter penstock. The correct approach is usually a combination of a saddle support with a hold-down strap or a clamp that is designed to resist the uplift.

Standards and Design Practice

The relevant standards for penstock design are typically the Chinese SL 281 (Design Code for Penstocks of Hydropower Stations) and the international equivalents such as ASME B31.3 or the DNV standards for submarine pipelines. However, seismic design of surface penstocks is often not covered in sufficient detail in these standards. The design engineer must rely on the general seismic provisions of the building code or the specific seismic design code for hydraulic structures.

In practice, I recommend that the seismic design of a surface penstock be treated as a special case, with a dedicated dynamic analysis. The finite element approach used in this paper is appropriate, but the boundary conditions must be modeled correctly. The sliding supports should be modeled as contact elements, not as fixed constraints, because the liftoff phenomenon depends on the ability of the pipe to separate from the support.

Lessons Learned and Reflections

The most important lesson from this paper is that the vertical direction is often the forgotten direction in penstock design. We spend a lot of time on transverse restraint for thermal expansion, and on axial restraint for water hammer, but the vertical uplift under seismic loading is frequently overlooked.

I recall a project where the penstock supports were designed with a transverse restraint but no vertical hold-down. The justification was that the pipe was heavy and would not lift. This paper shows that this assumption is not valid. The pipe can lift, and when it does, it can damage the supports, the expansion joints, and the pipe itself.

The recommendation to adopt both transverse and vertical restraint measures should be taken seriously. In my experience, the additional cost of a hold-down system is small compared to the potential cost of a seismic event.

Summary

This paper provides a clear and well-supported demonstration that exposed steel penstocks can experience significant vertical uplift and transverse sliding during earthquakes, particularly when the pipe is empty. The finite element time-history analysis is the right tool for this problem, and the conclusion that both transverse and vertical restraint measures are necessary is sound and practical. For engineers involved in the design of surface penstocks, this paper should be required reading, and the design should include a dedicated seismic analysis that considers the liftoff phenomenon.