Temperature Distribution in Rectangular Concrete-Filled Steel Tube Sections in Severe Cold Regions
Literature Overview and Context
This paper by Tian Zhijuan, Liu Yongjian, Ma Yinping and Liu Jiang from Chang'an University presents an experimental study of the temperature distribution in rectangular concrete-filled steel tube (CFST) sections in severe cold regions. The study was conducted in Xining, which is representative of severe cold regions in China, and involved field testing of a horizontal rectangular CFST member with longitudinal stiffeners. The authors also developed a finite element thermodynamic analysis model using ABAQUS, considering solar radiation, wind speed, and ambient temperature.
For a veteran who has worked on bridges and structures in cold regions, this is a topic of immediate practical importance. The temperature distribution in a CFST section is not uniform. The steel tube is directly exposed to the environment, so it responds quickly to changes in ambient temperature and solar radiation. The concrete core is insulated by the steel tube, so it responds more slowly. This creates a temperature gradient across the section, which can cause thermal stresses and can affect the structural behavior.
Interpretation of Technical Points
The paper reports several key findings:
- The measured temperatures at the steel tube and the concrete core agree well with the finite element calculations. This validates the finite element model.
- The temperature field in the rectangular CFST section under solar radiation is non-uniform. There is a significant temperature gradient across the section.
- The steel tube temperature is directly affected by the ambient temperature. The temperature change in the steel tube lags slightly behind the ambient temperature change, and the temperature extremes are significantly greater than the ambient temperature extremes.
- The concrete core temperature is indirectly affected by the ambient temperature. The temperature change in the concrete core lags significantly behind the ambient temperature change, and the temperature extremes are smaller than the steel tube temperature extremes.
- The longitudinal stiffeners inside the tube increase the contact area between the steel and the concrete, reducing the lag in the concrete temperature change and reducing the temperature gradient across the section.
These findings have important implications for the design and construction of CFST structures in cold regions.
Practical Implications for Design and Construction
The temperature gradient across the CFST section can cause thermal stresses that are significant enough to affect the structural behavior. In a bridge, for example, the temperature gradient can cause the section to bow, which can affect the alignment and the stress distribution.
The finding that the steel tube temperature extremes are significantly greater than the ambient temperature extremes is important. This means that the steel tube can experience temperatures that are higher than the maximum ambient temperature and lower than the minimum ambient temperature. This can affect the material properties of the steel and can cause the concrete to expand or contract more than expected.
The finding that the longitudinal stiffeners reduce the temperature gradient is also important. This suggests that adding stiffeners can be an effective way to reduce the thermal stresses in a CFST section. However, the stiffeners also increase the cost and the fabrication complexity.
In my experience, the temperature gradient in a CFST section is often not considered in the design. The design is usually based on a uniform temperature assumption, which can be unconservative. The temperature gradient should be considered, especially in cold regions where the temperature range is large.
Standards and Design Practice
The relevant standards for the design of CFST structures include the Chinese GB 50936 and the international standards such as AISC 360 and Eurocode 4. However, these standards do not provide specific guidance on the temperature distribution in CFST sections. The design engineer must rely on the research literature and on engineering judgment.
In practice, I recommend that the temperature gradient be considered in the design of CFST structures in cold regions. The temperature gradient can be estimated using the finite element method or using simplified formulas. The design should consider both the maximum and minimum temperature gradients, and the resulting thermal stresses should be combined with the other loads.
Lessons Learned and Reflections
The most important lesson from this paper is that the temperature distribution in a CFST section is not uniform, and the non-uniformity can have a significant effect on the structural behavior. This is particularly important in cold regions where the temperature range is large.
I recall a project where a CFST bridge was designed based on a uniform temperature assumption. During the first winter, the bridge experienced significant movement, which was attributed to the temperature gradient. The movement was not large enough to cause a failure, but it was large enough to cause concern and to require additional monitoring.
Another lesson is that the longitudinal stiffeners can be an effective way to reduce the temperature gradient. However, the stiffeners should be designed carefully to avoid stress concentrations and to ensure that they do not cause other problems.
Summary
This paper provides a valuable experimental and numerical study of the temperature distribution in rectangular CFST sections in severe cold regions. The findings are clear and well-supported. The temperature field is non-uniform, with a significant gradient across the section. The steel tube responds quickly to environmental changes, while the concrete core responds more slowly. The longitudinal stiffeners reduce the temperature gradient. For engineers involved in the design and construction of CFST structures in cold regions, this paper is an important reference. The key takeaway is that the temperature gradient should be considered in the design, and that stiffeners can be an effective way to reduce it.
Zhuojin Pipe Fitting Co., Ltd