ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Experimental Study on Large-Span Rectangular Concrete-Filled Steel Tube Trusses with Cantilevers

Literature Overview and Core Findings

This paper by Yang Chun and colleagues from South China University of Technology and Foshan University presents an experimental study on large-span rectangular concrete-filled steel tube (CFST) trusses with cantilevers. The study compares two large-scale specimens: one with concrete-filled rectangular steel tube members and one with hollow rectangular steel tube members.

The key findings are:

  1. The CFST truss specimen exhibits increased stiffness, reduced deformation, and improved ultimate load capacity compared to the hollow steel tube truss.
  2. Filling the steel tubes with concrete effectively prevents local buckling of the tube walls, and the failure of the CFST specimen is controlled by material strength.
  3. In both the hollow steel tube truss and the CFST truss, the web members and chord members at the direct welded connections experience significant member-end moments, which cannot be ignored in the design of the connections.

Technical Interpretation and Engineering Significance

The CFST Truss Concept

Rectangular CFST trusses are an efficient structural form for large-span applications. The concrete filling increases the stiffness and strength of the steel tube members, allowing them to resist higher axial forces and bending moments. The concrete also prevents local buckling of the tube walls, which is a common failure mode in hollow steel tube members.

The truss configuration with cantilevers is particularly useful for applications such as stadium roofs, airport terminals, and bridge structures, where the truss needs to extend beyond the supports to provide a canopy or a viewing platform.

Comparison of CFST and Hollow Steel Tube Trusses

The comparison between the CFST and hollow steel tube trusses is the core of the study. The key differences are:

  1. Stiffness: The CFST truss has higher stiffness because the concrete filling increases the cross-sectional area and the moment of inertia of the members.
  2. Deformation: The CFST truss exhibits reduced deformation under load because of the higher stiffness.
  3. Ultimate Load Capacity: The CFST truss has a higher ultimate load capacity because the concrete filling increases the compressive strength and prevents local buckling.
  4. Failure Mode: The CFST truss fails by material strength, while the hollow steel tube truss may fail by local buckling.

The Importance of Connection Design

The paper's finding that the web members and chord members at the direct welded connections experience significant member-end moments is particularly important. In a truss, the connections are typically assumed to be pinned, with the web members carrying only axial forces. However, in reality, the connections have some rotational stiffness, which induces bending moments in the members.

The member-end moments at the connections can be significant, especially in large-span trusses where the members are relatively slender. These moments must be considered in the design of the connections and the members, as they can cause premature failure.

Practical Engineering Insights and Lessons Learned

Design Considerations

  1. Connection Design: The connections in a CFST truss must be designed to resist the member-end moments in addition to the axial forces. This requires careful analysis of the connection stiffness and the distribution of moments.
  2. Concrete Filling Benefits: The concrete filling provides several benefits, including increased stiffness, reduced deformation, and improved ultimate load capacity. However, it also increases the weight of the structure, which must be considered in the design.
  3. Local Buckling Prevention: The concrete filling effectively prevents local buckling of the tube walls, which is a significant advantage for large-span structures where the members are slender.

Construction Considerations

  1. Concrete Placement: The concrete must be placed in the rectangular steel tube members, which can be challenging due to the geometry. The concrete must be placed in a way that ensures complete filling without voids.
  2. Connection Fabrication: The direct welded connections between the web members and chord members require careful fabrication to ensure adequate weld quality and to minimize the stress concentrations.
  3. Cantilever Construction: The cantilevered portion of the truss requires careful construction sequencing to ensure that the structure is stable during erection.

Quality Control and Inspection

  1. Weld Quality: The welds at the connections must be inspected for quality, as they are critical to the performance of the structure. Non-destructive testing, such as ultrasonic testing or radiography, should be used to verify the weld quality.
  2. Concrete Filling Quality: The concrete filling must be inspected to ensure that it is complete and free of voids. This can be done by ultrasonic testing or by drilling small holes to inspect the concrete.

Concluding Reflections

This experimental study provides valuable data on the behavior of large-span rectangular CFST trusses with cantilevers. The comparison between the CFST and hollow steel tube trusses confirms the benefits of concrete filling, including increased stiffness, reduced deformation, and improved ultimate load capacity. The finding that the member-end moments at the connections are significant and cannot be ignored in the design is particularly important for practical design. For engineers involved in the design and construction of large-span trusses, this paper reinforces the importance of proper connection design, concrete filling quality, and consideration of the member-end moments in the analysis. The study also highlights the need for careful attention to the construction sequencing and quality control to ensure the performance of the structure.