ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Effect of Additives on Microstructure and Properties of Centrifugal SHS Ceramic Composite Steel Pipes

Literature Overview and Manufacturing Context

This paper by Zhu Yu et al. from Nantong University investigates the role of additives in the centrifugal self-propagating high-temperature synthesis (SHS) process for producing ceramic-lined steel composite pipes. The Al-Fe2O3 thermite system is the basis, with SiO2 and Na2B4O7 added at varying mass fractions. The SHS process is a fascinating manufacturing route that leverages the exothermic reaction between aluminum and iron oxide to generate high temperatures (typically 2000-3000°C) that melt and fuse a ceramic layer onto the inner wall of a rotating steel pipe. The centrifugal force from pipe rotation distributes the molten ceramic uniformly, and as the reaction completes, a dense Al2O3-based ceramic lining forms, metallurgically bonded to the steel substrate. This technology is particularly valuable for producing wear-resistant and corrosion-resistant pipes for mining, power generation, and material handling applications where conventional steel pipes would fail prematurely.

Technical Findings and Microstructural Analysis

The X-ray diffraction (XRD) analysis reveals that the ceramic layer comprises α-Al2O3, FeAl2O4, Al2SiO5, and B2O3 phases. The presence of FeAl2O4 (hercynite) indicates partial reaction between the iron oxide and alumina, while Al2SiO5 (mullite) forms from the reaction of SiO2 with Al2O3, acting as a reinforcing phase. The Na2B4O7 additive serves as a flux, lowering the melting point of the ceramic and promoting densification. Scanning electron microscopy (SEM) shows dense grain packing in the ceramic layer, with energy-dispersive spectroscopy (EDS) confirming the presence of elemental iron, which is a byproduct of the thermite reaction that gets trapped in the ceramic matrix. Optical microscopy reveals excellent bonding between the ceramic layer and the Fe transition layer, with no interfacial gaps — a critical quality indicator for composite pipes. The mechanical property tests demonstrate that the addition of 7% SiO2 and 4% Na2B4O7 yields the optimal performance, with shear strength reaching 22 MPa and crushing strength reaching 430 MPa, representing improvements of 240% and 22.8% respectively over samples without additives.

Process Parameters and Quality Control Considerations

From a manufacturing perspective, the SHS process is highly sensitive to several parameters: the rotational speed of the pipe (which determines centrifugal force and ceramic layer thickness uniformity), the particle size distribution of the thermite powder, the ignition method, and the cooling rate after reaction completion. The additives play a crucial role in controlling the reaction kinetics and the resulting microstructure. SiO2 acts as a diluent, moderating the reaction temperature and preventing excessive porosity, while Na2B4O7 improves the flowability of the molten ceramic, allowing it to spread evenly under centrifugal force. The optimal additive content must be carefully balanced — too much SiO2 reduces the reaction temperature and may leave unreacted material, while insufficient Na2B4O7 leads to porous, poorly bonded ceramic layers. In production, I would emphasize the importance of rigorous raw material quality control, consistent powder blending, and precise control of the centrifugal casting parameters to ensure batch-to-batch consistency.

Defect Analysis and Countermeasures

Common defects in SHS ceramic composite pipes include: (1) porosity in the ceramic layer, caused by gas evolution during the reaction or insufficient centrifugal force; (2) interfacial debonding between the ceramic and steel substrate, resulting from inadequate reaction temperature or contamination at the steel surface; (3) cracking of the ceramic layer due to thermal stress during cooling, particularly if the cooling rate is too rapid; and (4) non-uniform ceramic thickness, caused by variations in powder feed rate or pipe rotation speed. Countermeasures include preheating the steel pipe before ignition to improve bonding, using graded powder particle sizes to achieve better packing density, controlling the cooling rate to minimize thermal gradients, and implementing ultrasonic or X-ray inspection to detect interfacial defects. The shear strength test is a critical quality control measure, as it directly evaluates the bond quality between the ceramic and steel — a value below 15 MPa would indicate inadequate bonding and potential delamination in service.

Engineering Practice and Application Insights

In my experience with wear-resistant piping systems, the primary failure mode is not the ceramic layer itself but the interfacial bond failure that leads to ceramic spalling and subsequent erosion of the steel substrate. The 240% improvement in shear strength achieved with the optimal additive formulation is therefore highly significant for real-world applications. Ceramic composite pipes are particularly valuable in applications such as coal slurry transport, ash handling in power plants, and ore processing in mining operations, where abrasive wear is severe. The economic benefits are substantial — a ceramic composite pipe can last 5-10 times longer than a conventional steel pipe in abrasive service, reducing maintenance costs and downtime. However, the manufacturing process requires specialized equipment and careful process control, which limits its application to high-value, critical service lines. I would recommend this technology for the most demanding wear applications where the higher initial cost is justified by the extended service life and reduced maintenance burden.