Axial Compression Capacity of Square Steel Tube Recycled Concrete Short Columns with Inner Steel Sections

Overview of the Study

This paper from Guangzhou University and the Guangdong Provincial Engineering Technology Research Center for Complex Steel Structures investigates the axial compression capacity of square steel tube recycled concrete short columns with inner steel sections. The research team employed the limit analysis method and the twin-shear unified strength theory to develop a theoretical model for predicting the axial compression capacity of these composite columns.

The key innovation is the conversion of the square steel tube section to an equivalent circular steel tube section with equal area and steel ratio, introducing two correction factors: the equivalent constraint reduction factor ψ and the recycled concrete strength reduction factor γu. The analysis considers the effects of the inner diameter-to-thickness ratio, confinement coefficient, steel ratio of the inner steel section, and recycled coarse aggregate replacement rate on the axial compression capacity.

The theoretical predictions were validated against experimental data, showing good agreement. This confirms the validity of the proposed calculation formula, which provides a theoretical basis for the design of such composite columns.

Technical Interpretation of the Composite Column Behaviour

Square steel tube recycled concrete columns with inner steel sections are a relatively new structural system that combines the advantages of steel-concrete composite construction with the sustainability benefits of recycled concrete. The inner steel section provides additional load-carrying capacity and improves the ductility of the column, while the outer steel tube provides confinement to the concrete core.

The twin-shear unified strength theory is a generalised strength criterion that can account for the different tensile and compressive strengths of concrete. By applying this theory, the authors were able to capture the complex stress state in the confined concrete, which is subjected to triaxial compression due to the confinement provided by the outer steel tube and the inner steel section.

The equivalent circular section approach is a practical simplification that allows the use of established formulas for circular steel tube concrete columns. The correction factors ψ and γu account for the differences between square and circular sections and the strength reduction of recycled concrete compared to natural aggregate concrete.

Engineering Practice and Lessons Learned

Recycled concrete has gained increasing attention in recent years due to the growing demand for sustainable construction practices. However, the use of recycled coarse aggregate in structural concrete raises concerns about strength and durability, as the recycled aggregate typically has lower strength and higher porosity than natural aggregate.

The findings of this paper are particularly relevant for the design of composite columns in high-rise buildings and other structures where axial compression is the dominant load. The proposed calculation formula provides a rational basis for incorporating recycled concrete into these structural elements, which can contribute to the sustainability goals of the construction industry.

Parameter Effect on Axial Capacity Practical Implication
Recycled aggregate replacement rate Decreases capacity Higher replacement rate requires larger section or more steel
Steel ratio of inner section Increases capacity More inner steel improves load-carrying capacity
Confinement coefficient Increases capacity Better confinement improves ductility and strength
Inner diameter-to-thickness ratio Decreases capacity Thinner walls reduce confinement effectiveness
Equivalent constraint factor ψ Accounts for section shape Square sections have lower confinement than circular

Standards and Design Considerations

The current standards for steel-concrete composite structures, such as GB 50936 and JGJ 138, do not specifically address the use of recycled concrete in square steel tube columns with inner steel sections. This paper provides a theoretical foundation for extending these standards to cover this new structural system.

The proposed calculation formula can be incorporated into design practice, but it is important to note that the correction factors ψ and γu are based on specific material properties and geometric parameters. For design purposes, these factors should be calibrated against a broader range of experimental data to ensure their applicability across different material and geometric combinations.

In my experience, the use of recycled concrete in structural applications requires careful quality control. The recycled coarse aggregate must be properly processed and tested to ensure consistent properties, and the mix design must be adjusted to account for the higher water absorption of recycled aggregate. The strength reduction factor γu proposed in this paper provides a rational basis for accounting for these effects in design.

Key Questions and Reflections

This paper raises several important questions for further research. First, how does the axial compression capacity of these columns behave under eccentric loading? The paper focuses on axial compression, but in practice, columns are often subjected to combined axial and bending loads, which may result in different failure modes.

Second, what is the long-term behaviour of these columns under sustained loading? Recycled concrete may exhibit different creep and shrinkage behaviour compared to natural aggregate concrete, which could affect the long-term performance of the composite column.

Third, how does the bond between the inner steel section and the surrounding concrete affect the load transfer mechanism? The paper assumes perfect bond, but in practice, the bond may be degraded by factors such as concrete shrinkage or cyclic loading.

Study Insights and Implications

This paper provides a valuable contribution to the field of composite structural engineering. By developing a rational calculation formula for the axial compression capacity of square steel tube recycled concrete columns with inner steel sections, the authors have addressed a significant gap in the existing literature.

For structural engineers, the key takeaway is that recycled concrete can be used in composite columns with appropriate design adjustments. The proposed formula, validated against experimental data, provides a practical tool for design, and the correction factors ψ and γu allow for the differences between square and circular sections and the strength reduction of recycled concrete.

In my own practice, I have seen the growing interest in using recycled concrete in structural applications, driven by both sustainability requirements and cost considerations. This paper provides a solid technical foundation for extending the use of recycled concrete to composite columns, which is a significant step forward.

However, I would caution that the proposed formula should be used with care until it has been validated against a broader range of experimental data. The correction factors are based on a limited set of tests, and their applicability to different material and geometric combinations should be verified before the formula is adopted in design codes.

This paper is a valuable reference for structural engineers and researchers working on composite structures and sustainable construction. The theoretical framework and the validated calculation formula provide a solid basis for further research and practical application.