ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Composite Stainless Steel Tube High-Strength Recycled Block Concrete Short Columns: Axial Compression Behavior and Practical Considerations

Overview of the Study

Wang Weihua and colleagues from Huaqiao University and the Xiamen Engineering Technology Research Center for Fire Resistance and Comprehensive Disaster Prevention conducted axial compression tests on 16 composite stainless steel tube high-strength recycled block concrete short columns. The composite section consists of a square stainless steel outer tube and a circular carbon steel inner tube, with high-strength concrete containing recycled concrete blocks filling the space. The study examined the effects of recycled block replacement ratio, confinement effect coefficient, and new-to-old concrete strength ratio on the axial compression performance.

This is a sophisticated study that combines multiple innovations: stainless steel for corrosion resistance, a composite section for improved confinement, and recycled concrete blocks for sustainability. From a pipe industry perspective, this is particularly interesting because it involves dissimilar metal welding and the interaction between two different steel types.

Technical Interpretation: The Composite Section and Its Benefits

The composite section — a square stainless steel outer tube with a circular carbon steel inner tube — addresses a fundamental limitation of square steel tube concrete columns. Square tubes provide less confinement than round tubes because the flat sides are less effective at restraining the concrete. By placing a circular tube inside, the inner tube provides better confinement to the core concrete, while the outer tube provides the overall section capacity.

The stainless steel outer tube provides corrosion resistance, which reduces the need for painting and fire protection. This is a significant practical advantage. In aggressive environments, such as coastal or industrial areas, stainless steel can eliminate the need for periodic maintenance. The carbon steel inner tube provides strength at a lower cost than stainless steel.

Parameter Square Stainless Outer Tube Circular Carbon Inner Tube
Material Stainless steel (e.g., 304 or 316) Carbon steel (e.g., Q345)
Primary function Corrosion resistance, section capacity Confinement, core strength
Manufacturing Cold-formed and welded Seamless or welded
Corrosion resistance Excellent Requires coating
Cost Higher Lower

The study found that the composite section has good deformation capacity and residual strength. After the peak load, the load-displacement curve showed a brief decline and then remained nearly horizontal or slightly rising. All specimens retained at least 63% of the peak load as residual strength. This is an excellent performance characteristic for seismic applications, where the column must maintain capacity after yielding.

Stainless Steel in Construction: Corrosion and Welding

Stainless steel is an excellent material for corrosion resistance, but it presents manufacturing challenges. The welding of stainless steel requires careful control of heat input and filler material. Overheating can cause sensitisation, where chromium carbides precipitate at grain boundaries, reducing corrosion resistance. The heat-affected zone (HAZ) of stainless steel welds is particularly susceptible to this.

From a pipe manufacturing perspective, stainless steel tubes are typically produced by cold forming and welding, or by extrusion for seamless tubes. The weld seam in stainless steel tubes must be inspected for defects and for sensitisation. The study does not specifically address the welding of the composite section, but this is a critical manufacturing issue.

The thermal expansion mismatch between stainless steel and carbon steel is another concern. Stainless steel has a higher coefficient of thermal expansion than carbon steel. In a composite section, this mismatch can create thermal stresses when the column is subjected to temperature changes. The study mentions that the composite section has good fire resistance, which suggests that the thermal mismatch is not a major issue, but it should be considered in design.

Recycled Concrete Blocks: Performance Implications

The use of recycled concrete blocks as a partial replacement for natural aggregate is a sustainability innovation. The study found that the axial compression capacity decreases as the recycled block replacement ratio increases, with a maximum reduction of 6.8% at a 20% replacement ratio. This is a modest reduction, which is encouraging.

The recycled concrete blocks have different properties than natural aggregate. They may have lower strength, higher porosity, and different shrinkage characteristics. The bond between the recycled concrete blocks and the cement paste may be weaker than for natural aggregate. However, the study found that the failure process and failure mode of the composite stainless steel tube recycled block concrete columns were similar to those of ordinary composite stainless steel tube concrete columns. This suggests that the recycled blocks do not fundamentally change the failure mechanism.

The study also found that the inner circular steel tube exhibited two failure modes: barrel-shaped (concrete crushing) and shear-type (tube shear failure). The barrel-shaped failure is typical of well-confined concrete, while the shear-type failure suggests that the inner tube may be subjected to high shear forces. This is an important finding for design, as the inner tube must be designed to resist both axial and shear loads.

Design Approach and Lessons Learned

The study proposed a simplified method for calculating the confinement effect of the steel tubes on the core concrete. The method assumes that the circular section's capacity is multiplied by a reduction factor. The study compared four calculation methods and found that this simplified method provides good agreement with test results.

From a practical perspective, the design of composite stainless steel tube columns requires careful consideration of:

  1. Material selection: The stainless steel grade must be selected based on the corrosion environment. For marine environments, 316 stainless steel is preferred. For less aggressive environments, 304 may be sufficient.
  2. Welding quality: The welds between the stainless steel outer tube and the carbon steel inner tube must be inspected for defects and sensitisation. Dissimilar metal welding requires careful selection of filler material.
  3. Thermal expansion: The thermal expansion mismatch between stainless steel and carbon steel must be considered in design, particularly for columns subjected to temperature changes.
  4. Recycled block replacement: The replacement ratio should be limited to 20% to avoid significant capacity reduction.

Concluding Reflection

This study demonstrates the feasibility of composite stainless steel tube columns with recycled concrete blocks. The combination of stainless steel for corrosion resistance, a composite section for improved confinement, and recycled concrete blocks for sustainability is a promising innovation. From a pipe industry perspective, the key takeaway is that the manufacturing of the composite section requires careful control of welding and material selection. The stainless steel outer tube must be welded with proper heat input control to avoid sensitisation, and the dissimilar metal weld between the stainless steel and carbon steel tubes requires appropriate filler material. The recycled concrete blocks can be used at up to 20% replacement without significant capacity reduction. The proposed design method, which applies a reduction factor to the circular section's capacity, is practical and provides good agreement with test results. I would recommend that designers specify the stainless steel grade, the welding procedure, and the recycled block replacement ratio in the project specifications, and that the manufacturing process be verified through inspection and testing. The sustainability benefits of this composite section are significant, and the modest capacity reduction is a reasonable trade-off.