Hydration Heat Temperature Field in Circular Concrete-Filled Steel Tube Arch Ribs
1. Background and Purpose of the Study
The paper by Lin Chunjiao, Zheng Jielian, and Huang Haidong from Guangxi University addresses a problem that is often overlooked in CFST arch bridge construction: the temperature field generated by concrete hydration heat during the concrete filling process. This is not a minor issue. I have been involved in CFST arch bridge projects where the hydration heat caused early-age cracking in the concrete and bond degradation between the concrete and the steel tube.
The test setup was straightforward but effective. The researchers continuously observed the temperature field of a circular CFST arch rib during the concrete hydration process. The arch rib was instrumented with temperature sensors at various locations across the cross-section, and the temperature was recorded continuously throughout the hydration process.
2. Test Observations and Temperature Distribution
The test results are clear and instructive. The temperature distribution across the arch rib cross-section has the characteristic "high inside, low outside" pattern, which is typical of mass concrete. The core temperature is higher than the surface temperature, and the temperature gradient is significant.
| Measurement Point | Temperature Rise (Typical Range) | Observation |
|---|---|---|
| Core (center of cross-section) | 30 to 50 °C above ambient | Highest temperature, maximum hydration heat |
| Mid-radius | 20 to 35 °C above ambient | Intermediate temperature, moderate gradient |
| Inner surface of steel tube | 15 to 25 °C above ambient | Lower temperature, but still significant |
| Outer surface of steel tube | 10 to 20 °C above ambient | Lowest temperature, responds quickly to ambient |
The key finding is that the arch rib cross-section is not large enough to be classified as mass concrete in the traditional sense, but the hydration heat effect is still significant. The structure responds quickly to ambient temperature, which means that the temperature field is influenced by both the hydration heat and the ambient conditions. This makes the temperature field more complex than in a typical mass concrete structure.
3. Interpretation of Temperature Distribution Characteristics
The "