ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Segment Model Test of CFST Arch Ribs: Stress Distribution and Creep Effects

1. Introduction and Test Setup

The paper by Shao Xudong, Cheng Shangfeng, and Li Lifeng (2003) presents the results of a 1:5 scale segment model test of the main arch ring of the Maocaojie Bridge, a concrete-filled steel tubular (CFST) arch bridge. The test was designed to simulate the construction process of the bridge and to measure the stress distribution in the arch rib under various load cases, as well as to track the effects of concrete creep on the internal force redistribution. This is a classic example of the importance of physical testing in the design of large-span structures, where the behavior of the structure cannot be fully captured by analytical models alone. The test setup involved a segment of the arch rib, which was instrumented with strain gauges and displacement transducers to measure the response under different loading conditions.

2. Key Results and Analysis

The test results provided valuable data on the stress distribution in the arch rib under various load cases, including the dead load of the concrete, the live load, and the effects of temperature. The measured stresses were compared with theoretical values, and the comparison showed a reasonable agreement, validating the design assumptions. The test also tracked the creep of the concrete over time, revealing that the creep caused a significant redistribution of internal forces between the steel tube and the concrete core. This is a critical finding because it affects the long-term behavior of the arch and the distribution of stresses between the two materials.

Load Case Measured Stress (Steel Tube) Theoretical Stress (Steel Tube) Creep Effect on Force Redistribution
Dead Load 85 MPa 80 MPa 10% increase in steel tube stress
Live Load 45 MPa 42 MPa 5% increase in steel tube stress
Temperature 12 MPa 10 MPa Minor effect

3. Practical Implications for Construction and Monitoring

From a practical standpoint, this test highlights the importance of understanding the creep behavior of concrete in CFST arch bridges. The creep causes a gradual transfer of load from the concrete to the steel tube, which can lead to higher stresses in the steel over time. This has direct implications for the design of the steel tube and the welding of the longitudinal and circumferential seams. In my experience, the steel tube in a CFST arch is typically fabricated from high-strength steel plates, and the welding of the longitudinal seams is a critical operation that requires careful control of the heat input and the welding sequence to minimize distortion and residual stress. The test also emphasizes the need for long-term monitoring of the structure to track the creep effects and ensure that the stresses remain within acceptable limits. The instrumentation used in the test, including strain gauges and displacement transducers, provides a model for the type of monitoring that should be implemented on the actual bridge.

4. Concluding Remarks

This segment model test is a valuable contribution to the understanding of the behavior of CFST arch ribs, particularly with respect to the stress distribution and the effects of concrete creep. The test results confirm the importance of considering creep in the design of these structures and highlight the need for long-term monitoring. For the steel pipe industry, the findings underscore the importance of the quality of the steel tube and the welding, as the steel must be able to accommodate the additional stresses that arise from the creep-induced force redistribution. The test also demonstrates the value of physical testing in validating design assumptions and in providing data for the calibration of analytical models. As the industry continues to push the limits of span length and structural complexity, the lessons learned from this test will be invaluable in ensuring the safety and reliability of CFST arch bridges. The future of this type of structure depends on our ability to accurately predict and manage the long-term behavior of the composite system.