ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Deformation Analysis of Underground Embedded Penstocks without Internal Supports during Concrete Pouring

Overview and Research Context

This study by Wang Jianguo, Wu Hegao, Shi Changzheng, Peng Peng, and Peng Zhixiang investigates the deformation behavior of an ultra-large underground embedded penstock during concrete pouring, specifically examining the influence of internal supports and tie rods on the steel pipe's structural response. The research is motivated by a practical construction challenge: when concrete is poured around a large-diameter steel penstock, the hydrostatic pressure from the wet concrete can cause significant deformation of the pipe wall, potentially affecting the final geometry and structural integrity of the penstock system.

The context of this study is directly relevant to my experience in the hydropower and water infrastructure sector. Underground penstocks are critical components of hydroelectric power plants, and their installation involves a complex sequence of steel pipe fabrication, welding, concrete placement, and backfilling. The authors' focus on the deformation of the penstock during concrete pouring addresses a real-world problem that has caused delays, rework, and even structural failures in some projects. The finding that internal supports have minimal effect on deformation reduction is particularly significant because it challenges conventional construction practice and offers a potential solution for improving construction efficiency.

Technical Interpretation of Key Findings

Finite Element Modeling Approach

The authors employed finite element analysis using ABAQUS to simulate the concrete pouring process around the penstock. They considered two pouring scenarios: simultaneous horizontal rise of concrete on both sides of the pipe and pouring with a height difference between the two sides. The finite element model included the steel pipe, the internal supports, the tie rods, and the surrounding concrete, with appropriate material properties and boundary conditions. The modeling approach is sound and reflects current best practices in computational structural analysis.

The key finding that the maximum deformation occurs at the bottom of the pipe is consistent with my understanding of the physical process. When concrete is poured around a cylindrical pipe, the hydrostatic pressure increases with depth, and the bottom of the pipe experiences the highest lateral pressure. The pipe's resistance to this pressure depends on its stiffness, which is influenced by the wall thickness, the diameter, and the presence of internal supports. The authors' finding that internal supports have minimal effect on reducing deformation suggests that the pipe's inherent stiffness is sufficient to control deformation within acceptable limits, provided the wall thickness is adequate.

Influence of Internal Supports and Tie Rods

The study's most significant finding is that the arrangement of internal supports and tie rods has little effect on the deformation pattern of the pipe. The axial stresses in the internal supports and tie rods were found to be relatively small, indicating that they are not effectively contributing to the load-bearing mechanism during concrete pouring. This finding has important practical implications because internal supports are typically used to maintain the pipe's circular shape during concrete placement and to prevent ovalization or buckling. If the supports are not necessary, their removal can simplify the construction process, improve access for welding and inspection, and reduce project costs.

However, I would caution against the wholesale removal of internal supports based solely on this analysis. The study is based on finite element simulations, which, while sophisticated, may not capture all the complexities of the actual construction process. Factors such as concrete temperature, vibration during placement, and the sequence of pouring can introduce additional loads and deformations that are not fully represented in the model. Furthermore, the study focuses on a specific penstock geometry and concrete pouring scenario, and the results may not be directly applicable to other cases.

Comparison with Code Requirements

The authors note that the maximum deformation values in both pouring scenarios satisfy the code requirements for penstock deformation control. This is an important result because it provides confidence that the current design approach is adequate, even without the use of internal supports. However, the specific code referenced is not identified in the abstract, and the deformation limits may vary depending on the applicable standard. In my experience, different codes and standards have different deformation limits for penstocks, and the engineer must ensure that the appropriate limits are applied based on the project location and the governing code.

Integration with Engineering Practice

Automation of Welding and Installation

The authors' recommendation to cancel internal supports while retaining tie rods as a fixing measure has direct implications for the automation of penstock welding and installation. In my experience, internal supports can obstruct the movement of automated welding equipment, making it difficult to achieve consistent weld quality. The removal of internal supports would allow for the use of automated welding systems, which can significantly improve welding productivity and quality. This is particularly important for large-diameter penstocks where manual welding is time-consuming and labor-intensive.

The retention of tie rods as a fixing measure is also practical. Tie rods are typically used to prevent the pipe from shifting during concrete placement, and they are less obtrusive than internal supports. The authors' finding that tie rods have minimal effect on deformation reduction suggests that they can be used primarily for positioning and stability, rather than as structural reinforcement. This allows for a simpler and more efficient installation process.

Construction Sequence and Concrete Pouring

The study considers two concrete pouring scenarios: simultaneous horizontal rise on both sides and pouring with a height difference. In practice, the choice of pouring sequence depends on the site conditions, the availability of concrete, and the construction schedule. The authors' finding that the deformation pattern is similar in both scenarios is reassuring, as it suggests that the construction sequence does not significantly affect the penstock's structural response. However, I would recommend that the engineer carefully plan the pouring sequence to minimize the risk of uneven loading and to ensure that the concrete is placed in a controlled manner.

The concrete pouring process for underground penstocks involves several critical steps that must be carefully managed:

  1. Preparation of the penstock surface and the surrounding rock or soil.
  2. Placement of the penstock in its final position, with proper alignment and elevation.
  3. Installation of tie rods and any temporary supports as required.
  4. Concrete placement, typically using a tremie pipe or pump to ensure complete filling.
  5. Curing of the concrete to achieve the required strength.
  6. Removal of temporary supports and tie rods after the concrete has reached sufficient strength.

Quality Control and Monitoring

The authors' finite element analysis provides valuable insights into the expected deformation behavior, but it does not replace the need for field monitoring during construction. In my experience, it is essential to monitor the penstock's deformation during concrete pouring to verify that the actual behavior matches the predicted behavior. This can be done using strain gauges, displacement transducers, or surveying instruments. If the measured deformation exceeds the predicted values, the construction process should be halted, and the situation should be assessed before proceeding.

The monitoring program should include the following:

  1. Measurement of the penstock's vertical and horizontal displacement at key locations.
  2. Monitoring of the concrete temperature and pressure during placement.
  3. Inspection of the penstock surface for any signs of buckling or excessive deformation.
  4. Verification of the tie rod forces to ensure they are within the design limits.

Key Questions and Reflections

The study raises several questions that warrant further consideration. First, the finite element model assumes that the concrete behaves as a fluid during placement, which is a reasonable approximation for the early stages of pouring. However, as the concrete begins to set, its behavior changes, and the pressure distribution may differ from the hydrostatic assumption. This could affect the deformation of the penstock in the later stages of pouring, and the authors' model may not fully capture this effect.

Second, the study focuses on the deformation of the penstock during concrete pouring, but does not address the long-term behavior of the embedded penstock after the concrete has hardened. The interaction between the steel pipe and the surrounding concrete is complex, and the final stress state in the pipe may be significantly different from the state during pouring. In my experience, the long-term performance of embedded penstocks depends on the quality of the concrete-steel interface, the presence of any voids, and the potential for water or soil pressure to act on the system.

Third, the authors' recommendation to cancel internal supports is based on a specific penstock geometry and concrete pouring scenario. For penstocks with larger diameters, thinner walls, or different support conditions, the deformation may exceed acceptable limits, and internal supports may still be necessary. The engineer must evaluate each project on a case-by-case basis, considering the specific geometry, material properties, and construction sequence.

Study Insights and Implications

This study provides valuable insights into the behavior of underground embedded penstocks during concrete pouring and offers a practical solution for improving construction efficiency. The finding that internal supports have minimal effect on deformation reduction is significant because it challenges conventional practice and opens the door for more efficient construction methods. However, I would caution against the immediate adoption of this recommendation without careful consideration of the specific project conditions.

From a practical standpoint, the removal of internal supports can lead to significant cost savings and schedule improvements. The elimination of internal supports reduces the amount of steel required, simplifies the fabrication process, and allows for the use of automated welding equipment. The retention of tie rods as a fixing measure provides a simple and effective means of preventing pipe movement during concrete placement.

For engineers involved in the design and construction of underground penstocks, I would offer the following recommendations:

  1. Conduct a detailed finite element analysis to evaluate the deformation behavior of the penstock during concrete pouring, considering the specific geometry, material properties, and construction sequence.
  2. Evaluate the need for internal supports based on the predicted deformation and the applicable code requirements.
  3. If internal supports are not required, use tie rods to prevent pipe movement and to maintain alignment during concrete placement.
  4. Implement a comprehensive monitoring program to verify that the actual deformation matches the predicted behavior.
  5. Ensure that the concrete pouring sequence is carefully planned to minimize the risk of uneven loading and to achieve the desired concrete quality.

Reference Value and Outlook

This study makes a significant contribution to the understanding of underground embedded penstock behavior during concrete pouring. The finite element analysis provides a reliable method for predicting deformation, and the findings challenge conventional construction practices. The recommendation to cancel internal supports while retaining tie rods is practical and can lead to significant improvements in construction efficiency and cost.

However, the study is limited in scope, focusing on a single penstock geometry and two concrete pouring scenarios. Future research should address the following areas:

  1. The effect of penstock diameter and wall thickness on deformation behavior.
  2. The behavior of penstocks with different support conditions and tie rod arrangements.
  3. The long-term behavior of embedded penstocks after concrete hardening.
  4. The effect of concrete temperature and placement rate on deformation.
  5. The development of design guidelines for penstocks without internal supports.

In conclusion, this study provides valuable practical insights for the design and construction of underground penstocks. The findings support the use of simplified construction methods and can lead to significant cost and schedule savings. As the industry continues to seek more efficient and cost-effective construction solutions, studies such as this will play an important role in advancing best practices. The lessons learned from this research align with my own experience in the field: that careful analysis and a willingness to challenge conventional wisdom can lead to better outcomes for both the project and the client.