ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Square Hollow Sandwich Steel Tube Concrete Members Under Compression-Torsion: Experimental Study and Design Implications

Overview of the Study

This paper, published in Progress in Steel Building Structures in 2021, is authored by Liao Xu, Li Jiren, and Wang Qingli from the School of Civil Engineering at Liaoning University of Science and Technology. The study focuses on square hollow sandwich steel tube concrete members, which consist of an outer steel tube, an inner steel tube, and concrete in between. This is a relatively new structural system that combines the advantages of concrete-filled steel tubes with the weight savings of a hollow section. The authors conducted static tests on 12 specimens under combined compression and torsion, with the cross-section size and axial compression ratio as the main parameters. They also developed a finite element model to study the effects of material strength and slenderness ratio on the bearing capacity. The study is funded by the Liaoning Provincial Department of Education and the Liaoning Provincial "Rising Talent" program. This is a fundamental study that addresses the basic behaviour of a structural system that is not yet widely used in practice, but has the potential for applications in towers, masts, and other structures where torsional loading is significant.

Key Technical Points and Failure Modes

The authors studied the behaviour of square hollow sandwich steel tube concrete members under combined compression and torsion. The axial compression ratio (n) is defined as the ratio of the applied axial load to the axial load capacity of the member. The test results show that the failure mode changes significantly with the axial compression ratio.

Axial Compression Ratio (n) Failure Mode Torsional Capacity
n ≤ 0.5 Ductile failure with gradual strength degradation Decreases with increasing n
n = 0.6 Brittle failure with rapid strength degradation Reduced to 70% of pure torsion capacity

For axial compression ratios up to 0.5, the torsional capacity decreases as the axial compression ratio increases, but the failure is still ductile, with a gradual degradation of strength after the peak load. However, when the axial compression ratio reaches 0.6, the behaviour changes dramatically. The torsional capacity drops to 70% of the pure torsion capacity, and the member enters a plastic stage followed by a rapid loss of strength. The ductility is poor, and the failure mode is completely different. This is a critical finding because it defines the limit of the axial compression ratio for practical design. I have seen similar behaviour in concrete-filled steel tube columns under combined compression and bending, where high axial loads lead to brittle failure, but the torsional case is less well studied. This paper provides valuable data on this phenomenon.

Parametric Study and Finite Element Analysis

The authors also developed a finite element model to study the effects of material strength and slenderness ratio on the bearing capacity. The results show that the outer steel tube strength has a significant influence on the torsional capacity, while the concrete strength has a smaller influence. This is intuitive because the outer steel tube is the primary load-bearing element in torsion, and the concrete provides confinement and additional strength. The torsional stiffness decreases significantly with increasing slenderness ratio, but the bearing capacity is not significantly affected. This is an interesting finding because it suggests that the torsional stiffness is more sensitive to slenderness than the torsional strength. In practical terms, this means that a slender member may have adequate strength but insufficient stiffness, which could lead to excessive deformations under service loads.

Parameter Effect on Torsional Capacity Effect on Torsional Stiffness
Outer steel tube strength Significant increase Not studied
Concrete strength Small increase Not studied
Slenderness ratio Not significant Significant decrease

Practical Implications for Design and Fabrication

The square hollow sandwich steel tube concrete member is a complex structural system that requires careful fabrication. The inner steel tube must be properly positioned and supported during concrete placement, and the concrete must be compacted in the annular space between the two tubes. From my experience in the steel pipe industry, this is a challenging fabrication process, especially for long members. The inner tube can easily be displaced during concrete placement, leading to eccentricity and reduced performance. I would recommend that the inner tube be supported by spacers or a temporary frame during concrete placement, and that the concrete be placed in layers with vibration to ensure full compaction. The paper does not address the fabrication issues, but they are critical to the performance of the member.

Standards and Code Gaps

There are currently no specific design codes for hollow sandwich steel tube concrete members. The design is usually based on the general principles for concrete-filled steel tubes, but the hollow core introduces additional complexities. The torsional behaviour is particularly difficult to predict because it involves the interaction between the outer tube, the inner tube, and the concrete. This paper provides valuable experimental data that can be used to develop design formulas, but more research is needed. I would recommend that the authors extend their study to include a wider range of parameters, such as different cross-section shapes, different steel tube thicknesses, and different concrete strengths. They should also consider the effect of the inner tube on the confinement of the concrete, which is a key factor in the performance of the member.

Study Insights and Reflections

This paper is a good example of the importance of experimental testing in the development of new structural systems. The authors conducted a well-designed experimental program that provides valuable data on the behaviour of square hollow sandwich steel tube concrete members under combined compression and torsion. The finite element model is a useful supplement, but it should be validated against the experimental results. I would like to see a comparison between the finite element predictions and the experimental results for the 12 specimens. That would give me much more confidence in the conclusions. The paper also highlights the importance of the axial compression ratio in determining the failure mode, which is a critical design consideration. I would recommend this paper to engineers who are involved in the design of towers, masts, and other structures where torsional loading is significant.

Conclusion

The square hollow sandwich steel tube concrete member is a promising structural system with potential applications in towers, masts, and other structures. This paper provides valuable experimental data on the behaviour of these members under combined compression and torsion, and it identifies the axial compression ratio as the key parameter that determines the failure mode. The finite element analysis provides additional insights into the effects of material strength and slenderness ratio. The practical implications for design and fabrication are significant, but more research is needed to develop design formulas and to address the fabrication challenges. I would recommend this paper to researchers and engineers who are working on the development of this structural system.