ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Hydration Heat Temperature Field in Giant Steel Tube High-Strength Concrete Columns: Analysis and Practical Considerations

Overview of the Study

This paper, published in the Journal of Shenyang Jianzhu University (Natural Science Edition) in 2023, is authored by Wang Qiang and colleagues from Shenyang Jianzhu University, North Testing Technology Co., Ltd., China Railway Investment Construction Group, and China Construction Third Engineering Bureau. The study focuses on the hydration heat temperature field in giant steel tube C70 high-strength concrete columns. The authors conducted experiments to obtain the temperature field development law and to assess the concrete placement quality. They then used the finite element software MIDAS FEA to simulate the temperature field and to study the effects of different concrete thermal parameters. The study is funded by the National Natural Science Foundation of China and the Liaoning Provincial Department of Education. This is a highly practical paper that addresses a real problem in the construction of giant steel tube concrete columns, which are used in high-rise buildings and large-span structures. The hydration heat of high-strength concrete can lead to high temperatures and temperature gradients, which can cause cracking and reduce the durability of the concrete.

Key Technical Points and Temperature Field Analysis

The authors studied the temperature field in a giant steel tube C70 high-strength concrete column. The temperature control indicators in the test specimen did not meet the requirements of the Code for Construction of Mass Concrete (GB 50496-2018), but the concrete placement quality was able to meet the construction quality requirements. This is an important finding because it suggests that the temperature control requirements in the code may be too strict for high-strength concrete in steel tubes. The steel tube provides confinement and reduces the temperature gradient, which may allow for more relaxed temperature control. The authors also found that the model considering the internal steel components matched the test results well, while the theoretical formula for the concrete thermal parameters gave results that differed significantly from the test results. This is a critical finding because it shows that the internal steel components, such as stiffeners and internal rings, have a significant influence on the temperature field and must be considered in the analysis.

Parameter Influence on Temperature Field
Internal steel components Significant; must be considered in the model
Concrete thermal parameters Theoretical formula gives inaccurate results
Hydration reaction rate Higher rate leads to higher peak temperature
Ambient temperature Affects the temperature gradient and cooling rate

Numerical Simulation and Parameter Study

The authors used the finite element software MIDAS FEA to simulate the temperature field and to study the effects of different concrete thermal parameters. The results show that the model considering the internal steel components matches the test results well, while the model using theoretical formula values for the concrete thermal parameters gives results that differ significantly from the test results. This suggests that the internal steel components, such as stiffeners and internal rings, act as heat sinks and reduce the peak temperature. The authors also found that the hydration reaction rate has a significant influence on the temperature field. A lower hydration reaction rate leads to a lower peak temperature and a more uniform temperature distribution, which reduces the risk of cracking. This is an important finding because it suggests that the concrete mix design should be optimized to reduce the hydration reaction rate, for example by using a slower-setting cement or a lower cement content.

Practical Implications for Concrete Mix Design and Construction

From my experience in the steel pipe and pipe fitting industry, the construction of giant steel tube concrete columns is a challenging process that requires careful planning and execution. The concrete must be placed in layers, and each layer must be properly compacted to ensure full contact with the steel tube. The hydration heat can lead to high temperatures, which can cause the concrete to expand and the steel tube to deform. The temperature gradient between the concrete and the steel tube can also cause thermal stresses, which can lead to cracking. The authors found that the temperature control indicators in the test specimen did not meet the requirements of the code, but the concrete placement quality was still acceptable. This suggests that the temperature control requirements in the code may be too strict for high-strength concrete in steel tubes, and that the steel tube provides some protection against the adverse effects of high temperatures.

Standards and Code Gaps

The current code for mass concrete, GB 50496-2018, sets temperature control requirements that are based on the behaviour of plain concrete. For steel tube confined concrete, the steel tube provides confinement and reduces the temperature gradient, which may allow for more relaxed temperature control. The authors suggest that the temperature control indicators for C70 high-strength concrete can be appropriately relaxed. This is a significant finding because it could reduce the cost and complexity of the construction process. However, I would caution that the relaxation should be based on a thorough analysis of the specific conditions, and that the concrete placement quality should be verified by non-destructive testing, such as ultrasonic testing or core sampling.

Study Insights and Reflections

This paper is a good example of how experimental testing and numerical simulation can be combined to solve a practical construction problem. The authors conducted a well-designed experimental program to obtain the temperature field development law, and they used the finite element software to extend the results to a wider range of conditions. The finding that the internal steel components must be considered in the temperature field analysis is particularly important, and it is a lesson that applies to all steel tube concrete structures. I would recommend this paper to engineers who are involved in the construction of giant steel tube concrete columns, and to researchers who are working on the thermal analysis of steel tube concrete structures.

Conclusion

The hydration heat temperature field in giant steel tube C70 high-strength concrete columns is a critical issue that can affect the quality and durability of the concrete. This paper provides valuable experimental data and numerical simulation results that can be used to optimize the concrete mix design and the construction process. The finding that the internal steel components must be considered in the temperature field analysis is particularly important, and the suggestion that the temperature control indicators can be relaxed for high-strength concrete in steel tubes is a practical contribution. I would recommend this paper to engineers and researchers who are involved in the design and construction of steel tube concrete structures, and to those who are working on the thermal analysis of mass concrete.