Confining Effect and Strength Criterion for Lightweight Aggregate Concrete in Steel Tubes
Scope of the Experimental Program
This paper by Ji Bohai from Hohai University and colleagues presents the results of an experimental study on the confining effect of steel tubes on lightweight aggregate concrete (LWAC). The study involved axial compression tests on concrete-filled steel tube (CFST) specimens with LWAC cores, and the results were used to develop a strength criterion for triaxially compressed LWAC.
For those of us who have worked with lightweight concrete, this is a topic of considerable practical interest. LWAC offers the advantage of reduced self-weight, which is particularly beneficial in long-span structures and in buildings where the dead load is a significant portion of the total load. However, LWAC is generally more brittle and has a lower tensile strength than normal-weight concrete, which raises concerns about its behavior in composite members.
Analysis of Confinement and Strength
The experimental program yielded several important findings, which are summarized in the following table:
| Aspect | Observation | Practical Significance |
|---|---|---|
| Stress-strain behavior | LWAC exhibits improved ductility and strength when confined by the steel tube | The confinement effect is beneficial but less pronounced than for normal concrete |
| Confinement effect | The confining effect of the steel tube on LWAC is smaller than on normal-weight concrete | This is attributed to the lower lateral expansion of LWAC |
| Failure mode | The specimens failed by crushing of the concrete core and local buckling of the steel tube | The failure was more sudden than for normal concrete |
| Strength criterion | A triaxial strength criterion was developed for LWAC | This criterion can be used for design calculations |
The key finding is that the confining effect of the steel tube on LWAC is smaller than on normal-weight concrete. This is because LWAC has a lower modulus of elasticity and a lower lateral expansion coefficient than normal-weight concrete. As a result, the LWAC does not expand laterally as much when subjected to axial compression, and it does not activate the confining stress in the steel tube to the same extent.
Implications for Composite Design and Practice
Design Implications
The reduced confining effect means that the strength enhancement of the concrete core is smaller for LWAC than for normal-weight concrete. This must be accounted for in the design of CFST members with LWAC cores. The design codes typically provide formulas for the strength enhancement factor, but these formulas are based on normal-weight concrete and may not be directly applicable to LWAC.
The strength criterion developed in this paper provides a basis for calculating the strength of LWAC under triaxial compression, which is the stress state in the core of a CFST member. This criterion can be used to verify the adequacy of the design and to ensure that the member has sufficient capacity.
Construction Practicalities
The use of LWAC in CFST members has several practical implications for construction. The lightweight concrete is easier to pump and place, and it reduces the dead load of the structure. However, the lower modulus of elasticity of LWAC means that the composite member will have a lower stiffness than a comparable member with normal-weight concrete. This must be accounted for in the design of the structure, particularly in terms of deflection and stability.
From a fabrication standpoint, the steel tube must be designed to provide the required confinement. The wall thickness of the tube must be sufficient to resist the lateral pressure from the concrete core, and the tube must be able to develop the required confining stress. This is particularly important for LWAC, where the confinement effect is smaller and the tube must work harder to provide the same level of confinement.
Closing Thoughts
This paper provides valuable experimental data on the confining effect of steel tubes on LWAC and proposes a strength criterion for triaxially compressed LWAC. The finding that the confining effect is smaller for LWAC than for normal-weight concrete is an important contribution to the understanding of composite behavior.
For the steel pipe industry, this research underscores the need for a thorough understanding of the material properties of the concrete core. The design of CFST members is not just about the steel tube; it is about the interaction between the tube and the concrete. The properties of the concrete, including its modulus of elasticity, lateral expansion coefficient, and strength, all play a role in determining the behavior of the composite member.
Zhuojin Pipe Fitting Co., Ltd