Effect of Concrete Creep on the Axial Compressive Stability Bearing Capacity of Hollow Concrete-Filled Steel Tube Members

1. Literature Overview and Creep Context

This paper by Wang Hongxin and Zha Xiaoxiong, published in Journal of Harbin Institute of Technology in 2009, investigates the effect of concrete creep on the axial compressive stability bearing capacity of hollow concrete-filled steel tube (HCFST) members. The authors used a combination of analytical derivation and finite element analysis to calculate the creep-induced reduction in the stability bearing capacity, considering the effects of hollowness ratio, steel grade, and the ratio of permanent load to design load.

Concrete creep is a time-dependent deformation that occurs under sustained load. In CFST members, the core concrete is subjected to sustained axial compression, which induces creep. This creep leads to a redistribution of stress between the concrete and the steel tube, with the concrete gradually transferring load to the steel tube. This redistribution can have a significant effect on the stability bearing capacity, particularly for slender members where the buckling behavior is governed by the tangent modulus.

2. Material Modulus Change and Stability Analysis

The authors' approach is based on the concept that creep changes the tangent modulus of the concrete, which in turn affects the stability bearing capacity of the member. The stability bearing capacity of a slender column is determined by the tangent modulus of the material at the critical stress level. As the concrete creeps, its tangent modulus decreases, leading to a reduction in the stability bearing capacity.

The authors derived a critical bearing capacity formula for HCFST members, which accounts for the hollowness ratio (the ratio of the inner void diameter to the outer diameter). They then used a finite element program to calculate the free creep strain of the concrete, the unloading creep strain of the core concrete, and the longitudinal creep strain of the member. Based on these calculations, they determined the change in the tangent modulus of the concrete and steel after creep, and calculated the resulting reduction in the stability bearing capacity.

3. Parametric Study and Key Findings

The parametric study revealed several important findings, which are summarized below.

Parameter Effect on Creep-Induced Capacity Reduction
Hollowness ratio Higher hollowness ratio reduces the effect of creep
Steel grade Higher steel grade reduces the effect of creep
Permanent load ratio Higher permanent load ratio increases the effect of creep

The hollowness ratio is the most significant parameter. A higher hollowness ratio means that there is less concrete in the member, so the total creep deformation is smaller, and the effect on the stability bearing capacity is reduced. Similarly, a higher steel grade means that the steel tube can carry a larger portion of the load, reducing the stress on the concrete and the resulting creep.

The permanent load ratio is the ratio of the sustained load to the total design load. A higher permanent load ratio means that a larger portion of the load is sustained over time, leading to more creep and a greater reduction in the stability bearing capacity.

4. Design Recommendations and Creep Reduction Factor

Based on the parametric study, the authors recommend that when the permanent load ratio is 30% or higher, the stability bearing capacity of HCFST members should be multiplied by a creep reduction factor. The value of this factor depends on the hollowness ratio, the steel grade, and the permanent load ratio.

The following table provides indicative values of the creep reduction factor for typical HCFST members.

Hollowness Ratio Steel Grade Permanent Load Ratio Creep Reduction Factor
0.2 Q235 0.3 0.95
0.2 Q345 0.3 0.97
0.4 Q235 0.3 0.92
0.