ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Development of T23 High-Pressure Boiler Steel Tubes: Lessons from Baosteel's Experience

1. Literature Overview and Core Findings

The paper by Wang Qijiang, Zou Fengming, and Zhang Ke documents Baosteel's development of T23 high-pressure boiler steel tubes, covering the experimental investigation of high-temperature tensile strength, creep rupture strength, and oxidation resistance. The research was supported by the Shanghai Science and Technology Committee and represents a significant milestone in China's ability to produce advanced boiler tube materials domestically.

The key finding is that the T23 tubes produced by Baosteel exhibit stable performance, with all technical indicators meeting the requirements of ASME SA-213. The tubes are deemed suitable for manufacturing large-capacity power station boilers. This is not just a technical achievement; it is a strategic one, as it reduces China's dependence on imported T23 tubes for supercritical and ultra-supercritical boiler applications.

From my perspective, the development of T23 tubes is a classic example of how material development must be closely coupled with manufacturing capability. You cannot simply buy the chemistry and expect to produce a good tube; you must control the entire process chain from melting to final heat treatment.

2. Technical Interpretation: T23 Alloy Design and Properties

2.1 Chemical Composition and Alloy Design

T23 is a 2.25Cr-1.6W-V-Nb steel, developed as a modification of T22 (2.25Cr-1Mo) with the addition of tungsten, vanadium, and niobium, and a reduction in molybdenum content. The alloy design is based on the concept of solid solution strengthening by tungsten and precipitation strengthening by vanadium and niobium carbides.

Element T23 (ASME SA-213) T22 (ASME SA-213) Role
C 0.04–0.10 0.05–0.15 Carbide formation
Mn 0.10–0.60 0.30–0.60 Deoxidizer, mild strengthening
P (max) 0.030 0.030 Impurity control
S (max) 0.010 0.030 Impurity control
Si ≤0.50 ≤0.50 Deoxidizer
Cr 1.90–2.60 1.90–2.60 Corrosion resistance, carbide former
Mo 0.05–0.30 0.87–1.13 Solid solution strengthening
W 1.45–1.75 — Solid solution strengthening, carbide former
V 0.20–0.30 — Precipitation strengthening
Nb 0.02–0.08 — Grain refinement, precipitation strengthening
B 0.0005–0.006 — Hardenability, creep strength

2.2 High-Temperature Tensile Strength

The paper reports the results of high-temperature tensile tests conducted on Baosteel's T23 tubes. The key observation is that the yield strength and tensile strength decrease with increasing temperature, as expected, but the rate of decrease is slower than for T22 due to the tungsten and vanadium additions. This is critical for boiler design, where the allowable stress at elevated temperatures is based on the yield strength and creep rupture strength.

2.3 Creep Rupture Strength

The creep rupture strength is the most important property for boiler tube design, as it determines the allowable stress at the design temperature. The paper reports that Baosteel's T23 tubes achieve creep rupture strength values that meet or exceed the ASME SA-213 requirements. The long-term creep rupture strength is governed by the stability of the carbide precipitates, particularly the W-rich M23C6 and the Nb-rich MX precipitates.

2.4 Oxidation Resistance

The oxidation resistance of T23 is superior to T22 due to the higher chromium content and the presence of tungsten, which promotes the formation of a protective Cr2O3 scale. The paper reports that the oxidation rate of T23 is significantly lower than that of T22 at temperatures up to 600°C, making it suitable for use in the superheater and reheater sections of large-capacity boilers.

3. Integration with Manufacturing and Site Practice

3.1 Manufacturing Process Chain

The production of T23 tubes involves a complex process chain that must be carefully controlled to achieve the required properties. Based on my experience, the following steps are critical:

  1. Melting and refining: The steel must be melted in an EAF or BOF and refined in a ladle furnace to achieve the tight chemistry control required by ASME SA-213. The phosphorus and sulfur contents must be kept low to prevent embrittlement.
  2. Continuous casting or ingot casting: The steel is cast into billets or ingots, which are then hot-rolled into tube rounds. The casting process must be controlled to minimize segregation and ensure a homogeneous structure.
  3. Hot piercing and rolling: The tube rounds are pierced and rolled into seamless tubes using the Mannesmann or similar process. The deformation temperature and reduction ratio must be optimized to ensure a fine-grained structure and to eliminate any internal defects.
  4. Heat treatment: The tubes are normalized and tempered to achieve the required microstructure. The normalization temperature is typically around 1050°C, and the tempering temperature is around 750°C. The heat treatment must be carefully controlled to ensure the formation of the desired carbide precipitates.
  5. Finishing and inspection: The tubes are straightened, cut to length, and subjected to non-destructive testing (UT, ET, or MT) to detect any internal or surface defects.

3.2 Welding Considerations

One of the critical challenges with T23 is its weldability. The tungsten addition increases the hardenability of the steel, which can lead to the formation of martensite in the heat-affected zone (HAZ) during welding. This martensite is hard and brittle, and it can lead to hydrogen-induced cracking if proper preheat and post-weld heat treatment (PWHT) are not applied.

From my experience, the following welding precautions are essential for T23:

3.3 Site Installation and Inspection

When T23 tubes are installed in a boiler, the following points must be checked:

  1. Verify that the tube material is certified to ASME SA-213 T23 and that the heat number and lot number are traceable.
  2. Confirm that the welding procedure qualification (WPS/PQR) covers the specific wall thickness and welding position.
  3. Ensure that the preheat and PWHT are performed as specified in the WPS.
  4. Perform 100% RT or UT on all butt welds, and MT or PT on all fillet welds.
  5. Verify that the tube supports and hangers do not impose excessive bending stresses on the welds.

4. Key Questions and Reflections

The paper raises an important question about the long-term stability of T23 tubes. While the short-term tests show excellent properties, the long-term behavior under creep conditions is not fully characterized. The creep rupture strength at 100,000 hours is extrapolated from shorter-term tests, and this extrapolation can be inaccurate if the precipitate coarsening kinetics change over time.

Another question is the effect of welding on the creep strength of the HAZ. The HAZ of T23 is known to have lower creep strength than the base metal, which can lead to Type IV cracking in service. This is a significant concern for boiler designers, and it is not addressed in the paper.

From my perspective, the most important lesson from the Baosteel experience is that material development is not just about achieving the specified properties; it is about achieving them consistently and reproducibly. The process control and quality assurance systems are just as important as the alloy design.

5. Study Insights and Practical Recommendations

The development of T23 tubes at Baosteel is a success story that demonstrates the importance of coupling material development with manufacturing capability. The paper provides valuable data on the high-temperature properties of T23, but it also highlights the need for long-term creep testing and a better understanding of the HAZ behavior.

My recommendation for the industry is to establish a comprehensive database of T23 creep rupture data from multiple manufacturers, including the HAZ properties, to support the development of more accurate design curves. This will require collaboration between steel producers, boiler manufacturers, and research institutions.

The paper is a valuable reference for engineers involved in the design and manufacture of supercritical and ultra-supercritical boilers. It provides the data needed to specify T23 tubes with confidence, but it also reminds us that the material is only as good as the process that produces it.