ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Thermal Stress and Cracking in SHS-Centrifugal Stainless Steel Lined Composite Pipes

Introduction and Literature Context

The paper by Xi Wenjun, Yin Sheng and Lai Heyi from the University of Science and Technology Beijing addresses a specific manufacturing problem in the production of stainless steel lined composite pipes using the self-propagating high-temperature synthesis (SHS) centrifugal process. The authors investigate the causes of cracking in the stainless steel lining layer and propose measures to eliminate the cracks. The study combines thermal stress calculation with microstructural analysis of the stainless steel layer. The conclusion is that the cracking is caused by the combined effect of inclusions in the steel, which embrittle the material, and thermal stress generated during the cooling process. The proposed countermeasures include accelerating the phase separation process, reducing inclusions in the lining layer, improving the plasticity of the steel, and increasing the austenite content.

The SHS-centrifugal process is a relatively specialised manufacturing route for producing composite pipes with a metallurgical bond between the outer carbon steel tube and the inner stainless steel lining. The process involves placing a mixture of metal powders and a reactive agent inside the outer tube, igniting the mixture to initiate a self-propagating combustion reaction, and simultaneously rotating the tube to centrifugally cast the molten reaction product onto the inner wall. The high temperature generated by the reaction melts the powder mixture, and the centrifugal force drives the molten metal to the inner surface of the outer tube, where it solidifies and bonds to the substrate.

Technical Points and Interpretation

The thermal stress in the lining layer arises from the difference in thermal expansion coefficients between the stainless steel lining and the carbon steel substrate. During cooling from the reaction temperature, the stainless steel contracts at a different rate than the carbon steel, and if the lining is not able to accommodate this differential strain, cracks will form. The stress is further exacerbated by the presence of inclusions, which act as stress concentrators and reduce the ductility of the lining material.

The microstructural analysis revealed that the inclusions in the lining layer were primarily oxides and other non-metallic phases that formed during the SHS reaction. These inclusions reduce the effective cross-section of the lining and create local stress concentrations. The authors found that the cracking was more severe in areas with higher inclusion density, confirming the role of inclusions in the failure mechanism.

Factor Effect on Cracking Countermeasure
Thermal expansion mismatch Generates tensile stress in lining Optimise cooling rate to reduce thermal gradient
Inclusions in lining Act as stress concentrators, reduce ductility Accelerate phase separation, improve powder purity
Low austenite content Reduces plasticity of stainless steel Adjust alloy composition to increase austenite
High cooling rate Increases thermal stress Controlled cooling after SHS reaction

Integration with Engineering Practice

The SHS-centrifugal process is attractive because it can produce a metallurgical bond between the lining and the substrate without the need for welding or explosive bonding. However, the process is sensitive to the quality of the starting powders and the reaction parameters. The authors' recommendation to accelerate the phase separation process is a practical one, because it means ensuring that the reaction products separate into a clean metal phase and a slag phase, with the slag being expelled from the lining layer. This can be achieved by adjusting the composition of the powder mixture, increasing the centrifugal force, or modifying the reaction kinetics.

The recommendation to increase the austenite content of the stainless steel lining is also practical. Austenitic stainless steels have better ductility and toughness than ferritic or martensitic stainless steels, and they are more resistant to thermal cracking. By adjusting the alloy composition, for example by increasing the nickel content, the austenite phase can be stabilised and the ductility of the lining improved.

For the manufacturer, the key process parameters to control are the powder composition, the particle size distribution, the centrifugal speed, the ignition method, and the cooling rate. Each of these parameters affects the quality of the lining layer, and the process must be carefully optimised to produce a crack-free product. The inspection of the lining layer should include ultrasonic testing, eddy current testing, and visual inspection for surface cracks.

Key Questions and Reflections

One question that arises is whether the thermal stress can be reduced by preheating the outer tube before the SHS reaction. Preheating would reduce the temperature gradient between the lining and the substrate, and thus reduce the thermal stress during cooling. However, preheating also affects the reaction kinetics and the quality of the metallurgical bond. The process window must be carefully determined to balance these competing effects.

Another question is whether the inclusions can be eliminated entirely by using higher purity powders. In practice, some level of inclusions is inevitable, but the size and distribution can be controlled. The authors suggest that accelerating the phase separation process is the key, which means that the slag phase should be expelled from the lining before it solidifies. This requires careful control of the centrifugal force and the cooling rate.

Study Insights and Implications

This paper provides a valuable insight into the failure mechanisms of SHS-centrifugal composite pipes. The combination of thermal stress and inclusions is a classic recipe for cracking, and the authors have identified the key factors that need to be controlled. For the industry, the lesson is that the SHS-centrifugal process is not a simple one-step operation; it requires careful optimisation of the powder composition, the reaction parameters, and the cooling regime.

The recommendations to reduce inclusions and increase the austenite content are directly applicable to the manufacturing process. The manufacturer should work with the powder supplier to ensure consistent quality, and should implement a rigorous quality control programme that includes chemical analysis of the powders, microstructural examination of the lining, and non-destructive testing of the finished pipe.

In summary, this study addresses a specific and important manufacturing problem in the production of SHS-centrifugal composite pipes. The cracking of the stainless steel lining is caused by the combined effect of inclusions and thermal stress, and the proposed countermeasures are practical and achievable. The findings have direct relevance to anyone involved in the production or use of composite pipes for corrosive service.